# US 2026/0209996 A1 · Compound phosphorus-nitrogen flame retardant, flame-retardant regenerated cellulose fiber, and preparation method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0209996 A1
- Document ID: US20260209996A1
- Status: Published application
- Kind: A1
- Application number: 19/141,234
- Filed: 2023-04-19
- Published: 2026-07-23
- Earliest claimed: 2022-12-21
- Assignees: China Textile Academy
- Applicants: China Textile Academy
- Inventors: Min GAO; Qingbo ZHAO; Shuli WANG; Zhongkai XU; Chunzu CHENG; Chenxi ZHANG; Ting LI; Jigang XU; Kedong CHI
- Web page: https://patentgrep.com/patent/US20260209996A1

## CPC

- D01F 1/07: for making fire- or flame-proof filaments
- C07F 9/6574: Esters of oxyacids of phosphorus {(C07F9/657163 takes precedence)}
- D01F 1/10: Other agents for modifying properties
- D01F 2/00: Monocomponent artificial filaments or the like of cellulose or cellulose derivatives; Manufacture thereof
- D01F 2/02: from solutions of cellulose in acids, bases or salts
- D01F 2/04: from cuprammonium solutions
- D01F 2/08: Composition of the spinning solution or the bath
- D01F 2/24: from cellulose derivatives
- D01F 11/02: of cellulose, cellulose derivatives, or proteins
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- C07F: ACYCLIC, CARBOCYCLIC OR HETEROCYCLIC COMPOUNDS CONTAINING ELEMENTS OTHER THAN CARBON, HYDROGEN, HALOGEN, OXYGEN, NITROGEN, SULFUR, SELENIUM OR TELLURIUM (metal-containing porphyrins C07D487/22)

## Abstract

The present invention discloses a compounded phosphorus-nitrogen-based flame retardant, flame-retardant regenerated cellulose fiber, and preparation method thereof. The compounded phosphorus-nitrogen-based flame retardant comprises a compounded mixture of a phosphoramide ester compound and an inorganic compound, wherein a mass ratio of the two is (10-35):(0.1-10); components of the flame-retardant regenerated cellulose fibers comprise cellulose and the compounded phosphorus-nitrogen-based flame retardant dispersed within a cellulose fiber matrix. A preparation method of the compounded phosphorus-nitrogen-based flame retardant comprises: adding a dispersing aid to a dispersion medium and mixing uniformly, then adding a phosphoramide ester compound, and uniformly dispersing by means of ultrasonic dispersion or mechanical stirring, followed by grinding; subsequently adding an inorganic compound and a modifying agent, and performing grinding to obtain a slurry of the compounded phosphorus-nitrogen-based flame retardant. In the compounded phosphorus-nitrogen-based flame retardant of the present invention, the components are synergistically compounded to achieve the purpose of high-efficiency flame retardancy and smoke suppression, and the prepared flame-retardant regenerated cellulose fibers are non-toxic and environmentally friendly, have a low smoke concentration upon combustion, and have permanent flame-retardant performance and excellent mechanical properties.

## Claims

### Claim 1

A compounded phosphorus-nitrogen-based flame retardant, characterized in that it comprises a compounded mixture of a phosphoramide ester compound and an inorganic compound, wherein a mass ratio of said phosphoramide ester compound and said inorganic compound is (10-35):(0.1-10);
Preferably, the mass ratio of said phosphoramide ester compound and said inorganic compound is (10-30):(0.1-10);
More preferably, the mass ratio of said phosphoramide ester compound and said inorganic compound is (10-25):(0.1-10).

### Claim 2 (depends on 1)

The compounded phosphorus-nitrogen-based flame retardant according to claim 1, characterized in that a structural formula of said phosphoramide ester compound is as shown in formula (1):
Where:
X is selected from oxygen or sulfur,
Y is selected from a hydrogen atom, an aryl group, or a methoxy group,
R1 and R2 are selected from an independent hydrogen atom, an alkyl group, an aryl group, a substituted alkyl group, or a substituted aryl group,
R3 is selected from an alkylene group, an aryl group, or a substituted aryl group,
Among them, R1, R2, R3, and a nitrogen atom connected thereto can form a nitrogen-containing heterocyclic structure.

### Claim 3 (depends on 1)

The compounded phosphorus-nitrogen-based flame retardant according to claim 1, characterized in that said inorganic compound is selected from a mixture of one or more of carbon compounds, clay minerals, silicon-based compounds, boron-containing compounds, and metal compounds,
Preferably, said carbon compound is selected from one or more of graphene, fullerene, and carbon nanotubes,
Said clay mineral is selected from one or more of montmorillonite, kaolin, bentonite, talc, muscovite, and diatomaceous earth,
Said silicon-based compound is selected from one or more of silicon dioxide, sodium silicate, magnesium silicate, aluminum silicate, and calcium silicate,
Said boron-containing compound is selected from one or more of zinc borate and boron nitride,
Said metal compound is selected from one or more of titanium oxide, zinc oxide, magnesium oxide, aluminum sulfate, aluminum hydroxide, and magnesium hydroxide,
Preferably, said inorganic compound exists in the form of particles, wherein the particles have an initial particle size distribution with X90 of less than 50 μm; preferably, have an initial particle size distribution with X90 of less than 10 μm; more preferably, have an initial particle size distribution with X90 of less than 5 μm.

### Claim 4 (depends on 1)

The compounded phosphorus-nitrogen-based flame retardant according to claim 1, characterized in that it further comprises a dispersing aid and a modifying agent, wherein a mass ratio of said phosphoramide ester compound to said modifying agent is 1:(0.01-10); preferably 1:(0.01-5.0), more preferably 1:(0.01-2.0),
Preferably, said dispersing aid is selected from a mixture of at least two or more of naphthalene sulfonates, sodium dodecylbenzene sulfonate, sodium alpha-olefin sulfonate, sodium lignosulfonate, sodium dodecyl sulfate, water-soluble polyesters, polycarboxylates, sodium polyacrylate, polyoxyethylene ether compounds, polyalkylsiloxane compounds, aliphatic-aromatic block copolymers, styrene-maleic anhydride modified copolymers, styrene-acrylic acid modified copolymers, sodium metaphosphate, sodium tripolyphosphate, and sodium pyrophosphate,
Preferably, said modifying agent is at least one of an alkane compound or an organosilicon compound,
Preferably, said alkane compound is a small molecule alkane compound containing an organic group; preferably, a small molecule alkane compound containing a small amount of carboxyl or mercapto groups,
Preferably, said organosilicon compound is selected from a siloxane solution or a siloxane coupling agent; preferably, said siloxane solution is a polymerized or non-polymerized siloxane compound, preferably an oligosiloxane compound containing hydrogen, methoxy, ethoxy, etc.; said siloxane coupling agent is a siloxane coupling agent containing a methoxy, ethoxy, or acyloxy group, preferably a siloxane coupling agent containing a small amount of vinyl, amino, epoxy, or mercapto groups.

### Claim 5 (depends on 1)

The compounded phosphorus-nitrogen-based flame retardant according to claim 1, characterized in that the preparation method of a compounded phosphorus-nitrogen-based flame retardant comprises: adding a dispersing aid to a dispersion medium and mixing uniformly, then adding a phosphoramide ester compound, uniformly dispersing for 0.5-5 h by means of ultrasonic dispersion or mechanical stirring, followed by performing a first grinding; subsequently adding an inorganic compound and a modifying agent, and performing a second grinding to obtain a slurry of the compounded phosphorus-nitrogen-based flame retardant,
Preferably, the first grinding causes particles to have a particle size distribution with X10 of less than 1 μm and X90 of less than 10 μm; the second grinding is performed until the particles in the compounded flame retardant slurry have a particle size distribution with X10 of less than 0.5 μm and X90 of less than 5.0 μm.

### Claim 6 (depends on 5)

The compounded phosphorus-nitrogen-based flame retardant according to claim 5, characterized in that the phosphoramide ester compound is added directly, or the phosphoramide ester compound is first pretreated and modified before being added,
Preferably, the method for pretreating and modifying said phosphoramide ester compound comprises: uniformly dispersing the phosphoramide ester compound in a mixed solution of water and ethanol, then adding a silicate ester and a modifying agent, and pretreating at 25-70° C. for 0.5-12 h, followed by filtering, washing, and drying to obtain a modified phosphoramide ester compound,
Preferably, in said mixed solution of water and ethanol, a volume ratio of water to ethanol is 1:(0.1-10),
Preferably, said silicate ester is at least one of tetraethyl orthosilicate, tetramethyl orthosilicate, tetrapropyl orthosilicate, or tetrabutyl orthosilicate,
Preferably, a mass ratio of said phosphoramide ester compound to said silicate ester is 1:(0.1-10),
Preferably, a mass ratio of said phosphoramide ester compound to said modifying agent is 1:(0.01-10); preferably, the mass ratio is 1:(0.01-5.0), more preferably; the mass ratio is 1:(0.01-2.0).

### Claim 7 (depends on 5)

The compounded phosphorus-nitrogen-based flame retardant according to claim 5, characterized in that said modifying agent is added in the form of an ethanol solution, wherein in said ethanol solution, a molar concentration of the modifying agent is 0.01-1 mol/L, preferably 0.01-0.1 mol/L.

### Claim 8 (depends on 5)

The compounded phosphorus-nitrogen-based flame retardant according to claim 5, characterized in that in said slurry of the compounded phosphorus-nitrogen-based flame retardant, a total mass of said phosphoramide ester compound, said inorganic substance, and said modifying agent accounts for 10-30% of a total mass of the slurry, a mass of the dispersing aid accounts for 0.5-20% of the total mass of the slurry, and the remainder is a dispersion medium,
Preferably, said dispersion medium is at least one of deionized water, an ethanol solution, or an N-methylmorpholine-N-oxide solution.

### Claim 9 (depends on 1)

A compounded phosphorus-nitrogen-based flame-retardant regenerated cellulose fiber, characterized in that components of the regenerated cellulose fiber comprise cellulose and a flame retardant dispersed within a cellulose fiber matrix, wherein said flame retardant is the compounded phosphorus-nitrogen-based flame retardant as described in claim 1.
Preferably, in said regenerated cellulose fibers, a mass ratio of the flame retardant to the cellulose is (15-50):100; preferably, the mass ratio is (15-35):100; more preferably (15-30):100.
Preferably, said regenerated cellulose fibers have a dry breaking strength of ≥2.0 cN/dtex, a wet breaking strength of ≥1.5 cN/dtex, and a limiting oxygen index value of ≥28%.

### Claim 10 (depends on 5)

A preparation method of compounded phosphorus-nitrogen-based flame-retardant regenerated cellulose fibers, characterized in that it comprises:
(1) Preparing a slurry of a compounded phosphorus-nitrogen-based flame retardant using the preparation method described in claim 5;
(2) Mixing the obtained slurry of the compounded phosphorus-nitrogen-based flame retardant with a suspension of cellulose or a cellulose solution, and dispersing uniformly to prepare a flame-retardant cellulose spinning solution, which is extruded through a spinneret into a coagulation bath for forming, followed by stretching, washing, oiling, and drying to obtain the compounded phosphorus-nitrogen-based flame-retardant regenerated cellulose fibers.
Preferably, in step (2), the cellulose solution comprises a cellulose xanthate solution, a solution of cellulose in N-methylmorpholine-N-oxide, a solution of cellulose in an ammonia solution of copper hydroxide or copper salt, or a solution of cellulose in an ionic liquid.
Preferably, components of said coagulation bath comprise sulfuric acid, sodium sulfate, zinc sulfate; or, said coagulation bath is an NMMO aqueous solution.