# US 2026/0209911 A1 · Ferritic stainless steel with improved formability and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0209911 A1
- Document ID: US20260209911A1
- Status: Published application
- Kind: A1
- Application number: 19/132,268
- Filed: 2023-11-08
- Published: 2026-07-23
- Earliest claimed: 2022-12-12
- Assignees: Posco
- Applicants: Posco Co., Ltd
- Inventors: Jieon Park; Jongsu Paek
- Web page: https://patentgrep.com/patent/US20260209911A1

## CPC

- C22C 38/28: with titanium or zirconium
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C21D 8/0268: {between cold rolling steps}
- C21D 8/0273: {Final recrystallisation annealing}
- C21D 9/46: for sheet metals
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/26: with niobium or tantalum
- H01M 8/021: Alloys based on iron
- C21D 2211/005: Ferrite
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY

## Abstract

The disclosed specification relates to a ferritic stainless steel with improved formability by controlling the average grain diameter through alloy components and manufacturing processes and to a method for manufacturing same. A ferritic stainless steel having improved formability, according to an embodiment, may comprise, in percentage by weight: C: 0.0005-0.02%; N: 0.005-0.02%; Si: 0.01-1.0%; Mn: 0.01-1.0%; P: 0.001-0.05%; Cr: 10.0-30.0%; Nb: 0.05-0.5%; Ti: 0.05-0.5%; and the remainder being Fe and inevitable impurities, wherein an Erichsen height may be 6-50 mm.

## Claims

### Claim 1

A ferritic stainless steel with improved formability, comprising, in percent by weight (wt %), 0.0005 to 0.02% of carbon (C), 0.005 to 0.02% of nitrogen (N), 0.01 to 1.0% of silicon (Si), 0.01 to 1.0% of manganese (Mn), 0.001 to 0.05% of phosphorus (P), 10.0 to 30.0% of chromium (Cr), 0.05 to 0.5% of niobium (Nb), 0.05 to 0.5% of titanium (Ti), the remainder of Iron (Fe), and inevitable impurities, and having an Erichsen height of 6 to 50 mm.

### Claim 2 (depends on 1)

The ferritic stainless steel of claim 1, having an average grain diameter of 5 to 20 μm.

### Claim 3 (depends on 1)

The ferritic stainless steel of claim 1, having a thickness of 200 μm or less.

### Claim 4 (depends on 1)

The ferritic stainless steel of claim 1, having a (thickness)/(average grain diameter) value of 5 to 10.

### Claim 5

A method for manufacturing a ferritic stainless steel with improved formability, the method comprising:
preparing a slab comprising, in percent by weight (wt %), 0.0005 to 0.02% of carbon (C), 0.005 to 0.02% of nitrogen (N), 0.01 to 1.0% of silicon (Si), 0.01 to 1.0% of manganese (Mn), 0.001 to 0.05% of phosphorus (P), 10.0 to 30.0% of chromium (Cr), 0.05 to 0.5% of niobium (Nb), 0.05 to 0.5% of titanium (Ti), the remainder of Iron (Fe), and inevitable impurities, and having an Erichsen height of 6 to 50 mm;
reheating the slab to 1100 to 1300° C. and then performing hot-rolling and hot-annealing on the reheated slab to produce a hot-rolled material; and
performing cold-rolling and cold-annealing on the hot-rolled material, which has been subjected to the hot-annealing, two to five times to produce a steel plate,
wherein the cold-annealing is performed at 850 to 1000° C.

### Claim 6 (depends on 5)

The ferritic stainless steel of claim 5, wherein the hot-annealing is performed at 900 to 1100° C.

### Claim 7 (depends on 5)

The ferritic stainless steel of claim 5, wherein in the producing of the steel plate, a final cold-rolling reduction ratio is 50% or more.