- Applicants: Bilkent Universitesi Ulusal Nanoteknoloji Arastirma Merkezi
- Inventors: Evren MUTLUGUN; Yusuf KELESTEMUR; Hilmi Volkan DEMIR
- Web page: https://patentgrep.com/patent/US20260209450A1

## CPC

- C08J 5/18: Manufacture of films or sheets
- C09K 11/881: {Chalcogenides}
- B29C 48/022: {characterised by the choice of material}
- C08J 3/201: {Pre-melted polymers}
- C09K 11/565: {with zinc cadmium}
- C09K 11/661: {Chalcogenides}
- C09K 11/663: {with alkaline earth metals}
- C09K 11/74: containing arsenic, antimony or bismuth
- C09K 11/7492: {Arsenides; Nitrides; Phosphides}
- B29C 48/0018: {combined with shaping by orienting, stretching or shrinking, e.g. film blowing (B29C48/0017 takes precedence)}
- B29C 48/08: flexible, e.g. films
- B29K 2995/0041: Crystalline
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

The present invention relates to a method (100) for producing polymeric nanocrystal films in a wide area.

## Claims

### Claim 1

A method (100) for producing polymeric nanocrystal films in a wide area; characterized in that it comprises steps of
obtaining a homogeneous mixture by mixing a nanocrystalline in a liquid-state form, that is desired to be included in a polymeric film, with poly meric granules in a molten state (101); and
obtaining a polymeric nanocrystal with a desired width by loading the homogeneous mixture into a blow extrusion device (102).

### Claim 2 (depends on 1)

A method (100) according to claim 1; characterized in that at the step of obtaining a homogeneous mixture by mixing a nanocrystalline in a liquid-state form, that is desired to be included in a polymeric film, with polymeric granules in a molten state (101), a quantum dot is combined with at least one nanocrystal in a liquid-state form—that is any of compounds being in a different type such as nanosheet and comprising Cd, In, Zn, Se, S, P—and at least one polymeric granule—that is an extrudable polymer such as low and high-volume polyethylene—in a container and the mixing process is carried out until a homogeneous mixture is obtained.

### Claim 3 (depends on 1)

A method (100) according to claim 1; characterized in that at the step of obtaining a homogeneous mixture by mixing a nanocrystalline in a liquid-state form, that is desired to be included in a polymeric film, with polymeric granules in a molten state (101), the nanocrystal included in the homogeneous mixture is 1 mg-1000 g in scale, the polymeric granule is 1 kg-100 kg in scale, and the mixture ratios are 1:1000-1:1 by mass.

### Claim 4 (depends on 1)

A method (100) according to claim 1; characterized in that at the step of obtaining a homogeneous mixture by mixing a nanocrystalline in a liquid-state form, that is desired to be included in a polymeric film, with polymeric granules in a molten state (101), the resulting homogeneous mixture is dried by being placed in a vacuum oven and kept here at a temperature of 20-200 ° C. for 1 minute-48 hours before being loaded into a blow extrusion device.

### Claim 5 (depends on 4)

A method (100) according to claim 4; characterized in that at the step of obtaining a homogeneous mixture by mixing a nanocrystalline in a liquid-state form, that is desired to be included in a polymeric film, with polymeric granules in a molten state (101), the dried homogeneous mixture is converted into a powder granule form by being ground.

### Claim 6 (depends on 1)

A method (100) according to claim 1; characterized in that at the step of obtaining a polymeric nanocrystal with a desired width by loading the homogeneous mixture into a blow extrusion device (102); the homogeneous mixture converted into a powder granule is loaded into a blow extrusion device with one or more channels and a polymeric film in desired diameters is obtained upon being blown up, by proceeding along a line at a temperature of 100-250° C. and varying the diameter of the output module of the extrusion device.

### Claim 7 (depends on 6)

A method (100) according to claim 6; characterized in that at the step of obtaining a polymeric nanocrystal with a desired width by loading the homogeneous mixture into a blow extrusion device (102); the drawing speed of polymeric film in the extrusion device is greater than 1m2/hour.