# US 2026/0209034 A1 · Method of manufacturing a microporous polymer structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0209034 A1
- Document ID: US20260209034A1
- Status: Published application
- Kind: A1
- Application number: 19/145,087
- Filed: 2024-01-04
- Published: 2026-07-23
- Earliest claimed: 2023-01-04
- Assignees: Novamem AG
- Applicants: Novamem AG
- Inventors: Michael LOEPFE; Christoph Ruedi KELLENBERGER
- Web page: https://patentgrep.com/patent/US20260209034A1

## CPC

- B81C 1/00047: {Cavities}
- B01D 63/081: {Manufacturing thereof}
- B01D 63/087: {Single membrane modules}
- B01D 69/1071: {Woven, non-woven or net mesh}
- B81C 1/00206: {Processes for functionalising a surface, e.g. provide the surface with specific mechanical, chemical or biological properties}
- B01D 61/14: Ultrafiltration; Microfiltration
- B01D 2313/025: Specific membrane holders
- B01D 2313/04: Specific sealing means
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)

## Abstract

A method of manufacturing a microporous polymer structure with a non-porous structure which supports a porous region. The method including: i) providing a substrate; ii) providing a first composition comprising a first polymer, a solvent for the first polymer, and one or both of nanoparticles and microparticles; iii) providing a second composition comprising a second polymer; iv) applying the first composition to the substrate to form a first coating layer; v) phase separating the first coating layer to obtain a phase separated coating layer; vi) applying the second composition to the surface of the substrate and/or onto the phase separated first coating layer; vii) hardening the second composition to obtain the non-porous support structure; viii) dissolving the nanoparticles and/or microparticles to obtain the porous region; arranging the non-porous support structure and porous regions on the substrate to form common interfaces, and effecting phase separation in the first coating layer.

## Claims

### Claim 1

A method of manufacturing a microporous polymer structure with at least one porous region and a substantially non-porous support structure configured to support said at least one porous region, the method comprising the steps of:
a) providing a substrate;
b) providing a first composition comprising a first polymer, at least one solvent for said first polymer, and one or both of nanoparticles and microparticles dispersed within said first composition;
c) providing a second composition comprising a second polymer or precursors of a second polymer;
d) applying the first composition to a surface of said substrate to form a first coating layer;
f) effecting a phase separation in the first coating layer to obtain a phase-separated coating layer;
g) applying, in a patterned manner, the second composition to at least one of the same surface of said substrate and onto the phase-separated first coating layer;
h) physically hardening or curing the second composition applied in step g) to obtain the non-porous support structure; and
i) dissolving said one or both of nanoparticles and microparticles with a washing solvent to obtain the porous region;
wherein said non-porous support structure and said porous regions are arranged on the substrate such that they form common interfaces, and wherein the phase separation in the first coating layer in step f) is effected from one side of the first coating layer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the second composition provided in step c) further comprises at least one solvent for said second polymer.

### Claim 3 (depends on 1)

The method according to claim 1, further comprising the step of
e) subjecting the first coating layer to an atmosphere promoting the evaporation of at least one of said solvents for said first polymer;
wherein step e) is performed after step d) and prior to step f).

### Claim 4 (depends on 1)

The method according to claim 1, wherein the washing solvent is an acidic aqueous solution.

### Claim 5 (depends on 1)

The method according to claim 1, further comprising the step of
j) drying the microporous polymer structure obtained after step i).

### Claim 6 (depends on 1)

The method according to claim 1, wherein the separation in the first coating layer in step f) is effected from the side of the substrate.

### Claim 7 (depends on 1)

The method according to claim 1, further comprising the step of
k) removing the microporous polymer structure from the substrate to obtain a free-standing microporous polymer structure;
wherein step k) is performed after any one of steps g) to j).

### Claim 8 (depends on 1)

The method according to claim 1, wherein step d) and step g) are performed simultaneously, followed by step f).

### Claim 9 (depends on 1)

The method according to claim 1, wherein phase separation in step f) is effected by applying heat of more than 40° C. to one side of the first coating layer.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the precursors of said second polymer are at least one of radiation-curable monomers and radiation-curable oligomers, and wherein curing of said second composition in step h) is performed by radiation curing using ultraviolet light or high-energy electrons from an electron-beam source.

### Claim 11 (depends on 1)

The method according to claim 1, wherein said one or both of nano-particles and microparticles are selected from the group consisting of oxides, carbonates, sulphates, halogenides, nitrates and phosphates.

### Claim 12

(canceled)

### Claim 13 (depends on 1)

The method according to claim 1, wherein said second composition consists of said at least one second polymer.

### Claim 14 (depends on 1)

A microporous polymer structure obtained by a method according to claim 1, comprising:
a top surface and a bottom surface;
a thickness between said top surface and said bottom surface;
at least one porous region formed from a first composition; and
a substantially non-porous support structure formed from a second composition;
wherein said porous region comprises an anisotropic distribution of pore diameters from the top surface to the bottom surface along the direction of thickness between the top surface and the bottom surface, and wherein the substantially non-porous support structure extends over at least part of the thickness between the top surface and the bottom surface.

### Claim 15 (depends on 14)

The microporous polymer structure according to claim 14, wherein the pore diameter at the top surface is in a comparatively smaller pore diameter range of 5 nm to 5000 nm, wherein the pore diameter at the bottom surface is in a comparatively larger pore diameter range of 500 nm to 50000 nm, and wherein the pore diameter in the thickness between the top surface and the bottom surface is in a pore diameter range of 5 nm to 5000 nm, wherein the pore diameters are determined by fluorescence read out of fluorescently labelled polystyrene or silica microspheres, or by dextran rejection test.

### Claim 16 (depends on 14)

The microporous polymer structure according to claim 14, wherein at least one of:
the porous region constitutes at least 40% and the non-porous support structure constitutes at most 60%, each based on the total volume of the microporous polymer structure; and
the porous region extends over at least 40% and the non-porous support structure extends over at most 60%, each based on the total coated substrate area.

### Claim 17 (depends on 14)

The microporous polymer structure according to claim 14, wherein said substantially non-porous support structure is an integral part of the microporous polymer structure.

### Claim 18 (depends on 14)

The microporous polymer structure according to claim 14, wherein the substantially non-porous support structure comprises a plurality of webs, wherein a first set of webs is arranged substantially parallel to each other.

### Claim 19 (depends on 18)

The microporous polymer structure according to claim 18, wherein at least two of said webs are boundary webs which bound the microporous polymer structure on at least two opposite sides and extend over the entire thickness of the porous regions, wherein at least some of the webs arranged between the boundary webs extend over part of the thickness of the porous regions, and wherein substantially all the webs are interconnected.

### Claim 20 (depends on 14)

A filtration device comprising at least one microporous polymer structure according to claim 14, wherein said at least one microporous polymer structure is attached to said filtration device via the non-porous support structure of said microporous polymer structure.

### Claim 21 (depends on 1)

The method according to claim 1, wherein said one or both of nanoparticles and microparticles have a particle size of 1 to 5000 nm, determined by laser diffraction spectrometer in combination with polarization intensity differential scattering technology.