# US 2026/0208412 A1 · Solvent-protected plastic packaging fused with a multi-layer inner coating, its production process and the use of the inner coating as a solvent protection agent

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0208412 A1
- Document ID: US20260208412A1
- Status: Published application
- Kind: A1
- Application number: 19/424,587
- Filed: 2025-12-18
- Published: 2026-07-23
- Earliest claimed: 2024-12-18
- Assignees: Rog Technologies
- Applicants: Rog Technologies
- Inventors: Agustin Enrique GONZÁLEZ LEAL; Julio Cesar RODRIGUEZ VILLA
- Web page: https://patentgrep.com/patent/US20260208412A1

## CPC

- B29C 45/14598: {Coating tubular articles}
- B29C 45/0001: {characterised by the choice of material}
- B29C 45/0055: {Shaping}
- B29C 45/14065: {Positioning or centering articles in the mould}
- B29C 2045/0079: {applying a coating or covering}
- B29C 2045/14319: {bonding by a fusion bond}
- B29K 2623/086: {EVOH, i.e. ethylene vinyl alcohol copolymer}
- B29K 2677/00: Use of {PA, i.e.} polyamides, e.g. polyesteramides {or derivatives thereof,} for preformed parts, e.g. for inserts
- B29K 2995/0058: Inert to chemical degradation
- B29K 2995/0097: Thickness
- B29L 2031/565: {for containers}
- B29L 2031/712: {Containers; Packaging elements or accessories, Packages (closures therefor B29L2031/56; ink or toner cartridges B29L2031/7678; squeeze tubes B29L2023/20; suitcases B29L2031/7418)}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A plastic container coated (fused) on its inner surface with an extruded film; this film provides the resistance for this container to handle, store, contain, and maintain solvent-based liquids or semi-liquids without affecting or altering their chemical composition, replacing the metal container that is normally used for these products. The plastic container with adequate resistance to prevent said plastic container from deforming, softening, or suffering any effect due to the type of solvent-based liquid it contains. The process for obtaining said container and the use of the inner coating as a solvent protection agent. The plastic container is fused with the protective film or inner multilayer coating resistant to solvent-based products, both parts being fused without being able to be detached from one another.

## Claims

### Claim 1

A process for obtaining a container with an extruded solvent-protection coating comprising the steps of:
a) extruding a multilayer film for chemical protection;
b) forming preforms from the multilayer film extruded in step a) to obtain preforms with protective coating;
c) injecting and thermally fusing at a temperature of 180° C. to 240° C. the container and the preforms with protective coating obtained in step b) to obtain a container;
d) cooling and stabilizing at a temperature of 10° C. to 40° C. the container obtained in step c) to obtain a solvent-protection container, which are detailed below.

### Claim 2 (depends on 1)

The process for obtaining a container with an extruded solvent-protection coating, according to claim 1, wherein in the step a) a multilayer film (1) is produced with a thickness of 100 microns, a total gauge of 400 gauge and a tolerance range of ±10% over the nominal thickness of 101.6 microns, said multilayer film comprising 14% of a first layer of Polyethylene (7), 15% of a second layer of polyethylene (8), 8% of a first adhesive layer (9), 9% of a first Nylon layer (10), 8% of EVOH (11), 9% of a second Nylon layer (12), 8% of a second adhesive layer (13), 15% of a third Polyethylene layer (14) and 14% of a fourth Polyethylene layer (15), wherein the % range of each layer is −2%/+4%.

### Claim 3 (depends on 1)

The process for obtaining a container with an extruded solvent-protection coating, according to claim 1, wherein in step b) the multilayer film (1) obtained in step a) is cut into preforms according to the required dimensions according to the container to be formed, and is positioned inside a mold for a plastic container, said mold being previously temperature-conditioned at a controlled temperature of 10° C. to 40° C., ensuring the adequate fit of the film in the inner contour of the mold.

### Claim 4 (depends on 1)

The process for obtaining a container with an extruded solvent-protection coating, according to claim 1, wherein in that in step c) a formulation of molten base plastic (2) is introduced into the mold that contains the preforms with protective coating (1); the temperature of the molten plastic is kept between 180° C. and 240° C., while the mold is hermetically closed to ensure uniform contact between the preforms with protective coating and the molten plastic material; the preforms with protective coating (1) are at a controlled temperature of 10° C. to 40° C. to obtain a container with a thickness of 1 to 4 mm, wherein 0.08 to 0.15 mm correspond to the protective multilayer film.

### Claim 5 (depends on 1)

The process for obtaining a container with an extruded solvent-protection coating, according to claim 1, wherein in step d) it is carried out in an environment with a controlled temperature of 10° C. to 40° C., once the molten material has cooled and solidified, a plastic container with solvent protection fused with a multilayer inner coating is obtained.

### Claim 6 (depends on 3)

The process for obtaining a container with an extruded solvent-protection coating according to claim 3, wherein the container includes a vessel (16) provided with a cap on an upper part (17).

### Claim 7 (depends on 3)

The process for obtaining a container with an extruded solvent-protection coating, according to claim 3, wherein said preforms must cover from 95 to 100% of the interior of the container that will be formed by the mold.

### Claim 8 (depends on 1)

A plastic container with an extruded solvent-protection coating according to claim 1, wherein said extruded solvent-protection coating comprises 14% of a first layer of Polyethylene (7), 15% of a second layer of polyethylene (8), 8% of a first adhesive layer (9), 9% of a first Nylon layer (10), 8% of EVOH (11), 9% of a second Nylon layer (12), 8% of a second adhesive layer (13), 15% of a third Polyethylene layer (14) and 14% of a fourth Polyethylene layer (15), wherein the % range of each layer is −2%/+4%.

### Claim 9 (depends on 8)

The container with an extruded solvent-protection coating, according to claim 8, wherein the container has a thickness of 1 to 4 mm, wherein 0.08 to 0.15 mm correspond to the fused film.

### Claim 10

An inner coating for plastic containers comprising 14% of a first layer of Polyethylene (7), 15% of a second layer of polyethylene (8), 8% of a first adhesive layer (9), 9% of a first Nylon layer (10), 8% of EVOH (11), 9% of a second Nylon layer (12), 8% of a second adhesive layer (13), 15% of a third Polyethylene layer (14) and 14% of a fourth Polyethylene layer (15) to be used as a solvent protection agent.