MXene MEMBRANE WITH GRADIENT PORES, PREPARATION METHOD AND APPLICATION THEREOF
AssigneeSouth China University of Technology
InventorsYanying WEI, Yufei WANG, Libo LI, Mide LUO, Zong LU
Life of this patent
Estimating the term…
Loading patent…
AssigneeSouth China University of Technology
InventorsYanying WEI, Yufei WANG, Libo LI, Mide LUO, Zong LU
Estimating the term…
A MXene membrane with gradient pores, its preparation method and application are provided. The MXene membrane with gradient pores, excluding the substrate, includes the following layers in sequence from bottom to top: an ultra large pore MXene membrane layer with a thickness of 0-30 nanometers (nm) and a pore size of 2-5 nm; a large pore MXene membrane layer with a thickness of 0-30 nm and a pore size of 0.9-1.2 nm; a medium pore MXene membrane layer with a thickness of 20-50 nm and a pore size of 0.6-0.8 nm; and a small pore MXene membrane layer with a thickness of 40-60 nm and a pore size of 0.3-0.5 nm. The present disclosure prepares the MXene membrane with gradient pores by repeating spin-coating and plasma irradiation while limiting the irradiation time.
A MXene membrane with gradient pores, wherein excluding a substrate, the MXene membrane with gradient pores comprises following layers in sequence from bottom to top:
Dependencies are inferred from the claim text.