# US 2026/0200793 A1 · Method for hydrophobicizing a glass substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0200793 A1
- Document ID: US20260200793A1
- Status: Published application
- Kind: A1
- Application number: 19/132,181
- Filed: 2023-11-22
- Published: 2026-07-16
- Earliest claimed: 2022-11-25
- Applicants: Saint-Gobain Sekurit France
- Inventors: Barbara BRUDIEU; Vincent PERROT
- Web page: https://patentgrep.com/patent/US20260200793A1

## CPC

- C03C 17/42: at least one coating of an organic material and at least one non-metal coating
- C09D 1/00: Coating compositions, e.g. paints, varnishes or lacquers, based on inorganic substances
- C03C 2217/213: SiO2
- C03C 2217/76: Hydrophobic and oleophobic coatings
- C03C 2218/113: by sol-gel processes
- C03C 2218/32: After-treatment
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

A method for hydrophobicizing a glass substrate, includes forming a primer layer on one of the main surfaces of the glass substrate, grafting a layer of C8-C16 alkyltrialkoxysilane and/or C8-C16 alkyltrichlorosilane onto the primer layer.

## Claims

### Claim 1

A method for hydrophobicizing a glass substrate, the method comprising consecutively:
forming a primer layer on one of the main surfaces of the glass substrate,
grafting a layer of C8-C16 alkyltrialkoxysilane and/or C8-C16 alkyltrichlorosilane onto the primer layer,
optionally, a polishing step using a cloth soaked in a water/alcohol mixture containing from 30% to 90% by weight of water,
wherein the C8-C16 alkyltrialkoxysilane is a linear alkylsilane of formula CH3 (CH2)nSiR3, where n=7-15, each R representing a C1-3 alkoxy group, and the C8-C16 alkyltrichlorosilane is a linear alkyltrichlorosilane of formula CH3 (CH2)nSiR3, where n=7-15, and each R representing a chlorine atom.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the C8-C16 alkyltrialkoxysilane is a linear alkyltrialkoxysilane of formula CH3 (CH2)nSiR3, where n=7-11, and each R represents a C1-3 alkoxy group.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the C8-C16 alkyltrichlorosilane is a linear alkyltrichlorosilane of formula CH3 (CH2)nSiR3, where n=7-11, and each R represents a chlorine atom.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the primer layer is made of silica and that the silica primer layer is formed in a sol-gel step wherein a tetrachlorosilane and/or tetraalkoxysilane is hydrolyzed in an acidic aqueous-alcoholic medium.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the sol-gel step for forming the silica primer layer is carried out with an acidic aqueous-alcoholic solution containing from 0.1% to 1% by weight of tetraalkoxysilane and/or tetrachlorosilane.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the H2O/tetraalkoxysilane or H2O/tetrachlorosilane molar ratio of the acidic aqueous-alcoholic solution is between 400 and 600.

### Claim 7 (depends on 5)

The method according to claim 5, wherein the aqueous-alcoholic solution of tetraalkoxysilane and/or tetrachlorosilane is left at room temperature for a period of about 30 minutes to about 4 hours, before being applied to the glass substrate by immersion, curtain coating, spraying or wiping.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the grafting of C8-C16 alkyltrialkoxysilane and/or C8-C16 alkyltrichlorosilane is carried out by a sol-gel step wherein the C8-C16 alkyltrialkoxysilane and/or the C8-C16 alkyltrichlorosilane is hydrolyzed in an acidic aqueous-alcoholic medium.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the grafting of C8-C16 alkyltrialkoxysilane and/or C8-C16 alkyltrichlorosilane is carried out with an acidic aqueous-alcoholic solution containing from 1% to 4% by weight of C8-C16 alkyltrialkoxysilane and/or C8-C16 alkyltrichlorosilane.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the H2O/alkyltrialkoxysilane or H2O/alkyltrichlorosilane molar ratio of the acidic aqueous-alcoholic solution is between 70 and 200.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the aqueous-alcoholic solution of C8-C16 alkyltrialkoxysilane and/or C8-C16 alkyltrichlorosilane is left at room temperature for a period of about 30 minutes to about 3 hours, before being applied, by spraying or wiping, to the glass substrate covered on one of its main faces with the silica primer layer.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the grafting of C8-C16 alkyltrialkoxysilane and/or C8-C16 alkyltrichlorosilane is carried out after at least 5 minutes of drying of the silica primer layer at room temperature.

### Claim 13 (depends on 1)

A hydrophobic glass substrate obtained by the method according to claim 1, comprising a transparent glass substrate which is covered, on one of its main faces, with a silica primer layer, said silica primer layer being grafted with linear C8-C16 alkylsilyl groups, wherein the linear C8-C16 alkyl has a formula CH3 (CH2) n, where n=7-15.

### Claim 14 (depends on 13)

The hydrophobic glass substrate according to claim 13, wherein n is between 7 and 11, limit values included.

### Claim 15 (depends on 13)

The hydrophobic glass substrate according to claim 13, wherein the silica primer layer has a thickness of between 5 nm and 250 nm.

### Claim 16 (depends on 13)

The hydrophobic glass substrate according to claim 13, wherein the hydrophobic glass substrate is a motor vehicle side window.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the primer layer is made of silica.

### Claim 18 (depends on 1)

The method according to claim 1, wherein the C1-3 alkoxy group is a methoxy or ethoxy group.

### Claim 19 (depends on 2)

The method according to claim 2, wherein the C8-C16 alkyltrialkoxysilane is a linear alkyltrialkoxysilane of formula CH3 (CH2)nSiR3, where n=7-11, and each R represents a methoxy or ethoxy group.

### Claim 20 (depends on 4)

The method according to claim 4, wherein a tetraethoxysilane is hydrolyzed in an acidic aqueous-alcoholic medium.