# US 2026/0199890 A1 · Hydrogenation catalyst and preparation method therefor and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0199890 A1
- Document ID: US20260199890A1
- Status: Published application
- Kind: A1
- Application number: 19/136,853
- Filed: 2023-12-05
- Published: 2026-07-16
- Earliest claimed: 2022-12-08
- Assignees: China Petroleum & Chemical Corporation; Sinopec Dalian Research Institute of Petroleum and Petrochemicals Co., Ltd.
- Applicants: China Petroleum & Chemical Corporation; Sinopec Dalian Research Institute of Petroleum and Petrochemicals Co., Ltd.
- Inventors: Jin SUN; Rong GUO; Yang LI; Shikun NIU; Weiyu DUAN
- Web page: https://patentgrep.com/patent/US20260199890A1

## CPC

- B01J 37/0205: {in several steps}
- B01J 21/04: Alumina
- B01J 23/755: Nickel
- B01J 23/882: and cobalt
- B01J 23/883: and nickel
- B01J 23/885: and copper
- B01J 23/8885: {containing also molybdenum}
- B01J 27/0515: {with iron group metals or platinum group metals}
- B01J 35/394: {Metal dispersion value, e.g. percentage or fraction}
- B01J 35/613: {10-100 m2/g}
- B01J 35/615: {100-500 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 35/638: {more than 1.0 ml/g}
- B01J 35/647: {2-50 nm}
- B01J 37/0009: {Use of binding agents; Moulding; Pressing; Powdering; Granulating; Addition of materials ameliorating the mechanical properties of the product catalyst}
- B01J 37/0018: {Addition of a binding agent or of material, later completely removed among others as result of heat treatment, leaching or washing,(e.g. forming of pores; protective layer, desintegrating by heat)}
- B01J 37/0207: {Pretreatment of the support}
- B01J 37/0213: {Preparation of the impregnating solution}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/14: with gases containing free oxygen
- B01J 37/18: with gases containing free hydrogen
- B01J 37/20: Sulfiding
- C07C 5/02: by hydrogenation (simultaneous hydrogenation and dehydrogenation C07C5/52)
- C07C 2523/882: and cobalt
- C07C 2523/883: and nickel
- C07C 2523/885: and copper
- C10G 45/00: Refining of hydrocarbon oils using hydrogen or hydrogen-generating compounds
- Y02P 20/52: using catalysts, e.g. selective catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A dry gas hydrogenation catalyst and a preparation method therefor are provided. The dry gas hydrogenation catalyst have a carrier component containing aluminium oxide and an active hydrogenation component in the form of a sulfide on the catalyst. An average number of lamella layers of the sulfide is less than 1.5, and the proportion of a single layer is 65%-80%. The catalyst is prepared by (I) taking aluminum oxide powder A and roasting same at high temperature in an oxygen-containing atmosphere to obtain aluminum oxide dry gel powder B; II) impregnating the aluminum oxide dry gel powder B using the active hydrogenation component impregnating solution C, drying, roasting at high temperature in the oxygen-containing atmosphere, and sulfidizing same to obtain powder E; and III) molding, drying, and roasting the powder E prepared in step (II). The catalyst is effective in removing impurities such as oxygen, CO, and CO2.

## Claims

### Claim at position 1

1-16. (canceled)

### Claim 17

A hydrogenation catalyst, is characterized in that the hydrogenation catalyst comprises a carrier component and an active hydrogenation component; the carrier component comprises aluminum oxide; and the active hydrogenation component is present in the form of a sulfide on the catalyst, the average number of lamella layers of the sulfide is less than 1.5, and the proportion of a single layer is within the range of 65%-80%.

### Claim 18 (depends on 17)

The catalyst according to claim 17, wherein the average number of lamella layers of the sulfide is within the range of 1.2-1.3; and/or
the hydrogenation catalyst comprises a coagent including one or more of Cu, Ag, Ni, Co, W, and Mo.

### Claim 19 (depends on 18)

The catalyst according to claim 18,
the coagent is present in the form of a metallic state on the catalyst;
the coagent content in the catalyst is from 0.1 wt % to 4 wt %.

### Claim 20 (depends on 17)

The catalyst according to claim 17, wherein the content of active hydrogenation component calculated in terms of sulfide in the total mass of the catalyst is from 1.5 wt % to 30 wt %, based on the weight of said catalyst.

### Claim 21 (depends on 20)

The catalyst according to claim 20, wherein the content of active hydrogenation component calculated in terms of sulfide in the total mass of the catalyst is from 10 wt % to 20 wt %, based on the weight of said catalyst.

### Claim 22 (depends on 17)

The catalyst according to claim 17, wherein the active hydrogenation component comprises Group VIB metals and Group VIII metals.

### Claim 23 (depends on 22)

The catalyst according to claim 22,
Group VIB metals comprise Mo and/or W; Group VIII metals comprise Co and/or Ni;
the content of Group VIB metal sulfide in the total mass of the catalyst is from 1 wt % to 20 wt %,
the content of Group VIII metal sulfide in the total mass of the catalyst is from 0.5 wt % to 10 wt %, based on the weight of the catalyst.

### Claim 24 (depends on 23)

The catalyst according to claim 23,
the content of Group VIB metal sulfide in the total mass of the catalyst is from 8 wt % to 16 wt %,
the content of Group VIII metal sulfide in the total mass of the catalyst is from 2 wt % to 4 wt %, based on the weight of the catalyst.

### Claim 25 (depends on 17)

The catalyst according to claim 17, wherein the total acid amount of the catalyst is within the range of 0.1-0.4 mmol/g, wherein the content of strong acid amount at 400-500° C. is within the range of 5-15%, the content of moderate strength acid amount at 250-400° C. is within the range of 10-20%, and the balance is weak acid at 150-250° C.

### Claim 26

A preparation method of a hydrogenation catalyst, is characterized in that the preparation method comprises the following steps:
(I) taking aluminum oxide powder A and roasting same at high temperature in an oxygen-containing atmosphere to obtain aluminum oxide dry gel powder B;
(II) impregnating the aluminum oxide dry gel powder B by using the active hydrogenation component impregnating solution C, drying, roasting at high temperature in the oxygen-containing atmosphere, and sulfidizing same to obtain powder E;
(III) molding, drying, and roasting the powder E prepared in step (II);
wherein the respective temperature of high-temperature roasting in step (I) and step (II) are 800° C. or above.

### Claim 27 (depends on 26)

The preparation method according to claim 26, wherein the method further comprises the following steps: impregnating the aluminum oxide powder A with a coagent impregnating solution D, drying the impregnated aluminum oxide powder A and reducing to obtain powder F;
step (III) comprises: mixing powder E with powder F, and then molding, drying, and roasting the mixture;
the reduction treatment includes roasting in a reducing atmosphere;
the roasting conditions in the reduction treatment comprise a roasting temperature within the range of 300-700° C. and a roasting time within the range of 2-5 hours;
the drying conditions before reduction comprise a drying time within the range of 1-5 hours and a drying temperature within the range of 80-120° C.;
the impregnation method of the coagent impregnation is saturated impregnation or supersaturated impregnation.

### Claim 28 (depends on 26)

The method according to claim 26, wherein physicochemical parameters of the aluminum oxide powder A comprise: a specific surface area within the range of 100-480 m2/g, a pore volume within the range of 0.4-1.2 cm3/g, and a pore diameter within the range of 4.0-35.0 nm.

### Claim 29 (depends on 26)

The method according to claim 26, wherein in step (I),
the oxygen-containing atmosphere has an oxygen content from 10 v % to 30 v %; and/or
the roasting conditions at high temperatures comprise a roasting temperature within the range of 800-1,100° C. and a roasting time within the range of 0.5-5 hours.

### Claim 30 (depends on 26)

The method according to claim 26, wherein in step (II),
the oxygen-containing atmosphere has an oxygen content from 10 v % to 30 v %; and/or
the roasting conditions at high temperatures comprise a roasting temperature within the range of 800-1,100° C. and a roasting time within the range of 0.5-5 hours.

### Claim 31 (depends on 26)

The method according to claim 26, wherein the sulfidizing in step (II) comprises:
roasting in a mixed atmosphere of H2S and H2, the content of H2S in the mixed atmosphere of H2S and H2 is within the range of 0.1 v %-2 v %;
the roasting conditions comprise a roasting temperature within the range of 250-550° C. and a roasting time within the range of 3-8 hours.

### Claim 32 (depends on 26)

The method according to claim 26, wherein the impregnation method of step (II) is saturated impregnation or supersaturated impregnation.

### Claim 33 (depends on 26)

The method according to claim 26, wherein the catalyst molding process in step (III) comprises: adding an extrusion aid, a peptizing agent, and water into the composite powder and blending to form a plastic body, then kneading and molding the plastic body.

### Claim 34 (depends on 33)

The method according to claim 33,
the extrusion aid is one or more selected from the group consisting of methylcellulose, sesbania powder, starch, and polyvinyl alcohol;
the peptizing agent is one or more selected from the group consisting of dilute nitric acid, dilute phosphoric acid, and silicic acid.

### Claim 35 (depends on 26)

The method according to claim 26, wherein the drying conditions in steps (II) and (III) respectively comprise a drying time within the range of 1-5 hours and a drying temperature within the range of 80-120° C.

### Claim 36 (depends on 26)

The method according to claim 26, wherein the roasting condition in step (III) comprises a roasting temperature within the range of 200-350° C. and a roasting time within the range of 1-4 hours;
the roasting atmosphere is an inert atmosphere, which is one or more gases selected from N2, He, or Ar.