# US 2026/0198361 A1 · Copper bumps on copper pads in semiconductor interconnect structures and methods for forming the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0198361 A1
- Document ID: US20260198361A1
- Status: Published application
- Kind: A1
- Application number: 19/008,934
- Filed: 2025-01-03
- Published: 2026-07-09
- Earliest claimed: 2025-01-03
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company Limited
- Inventors: Wei-Ren Huang; Chiang-Jui Chu; Kuan-Sheng Huang; Ching-Ho Cheng; Ching-Wen Hsiao
- Web page: https://patentgrep.com/patent/US20260198361A1

## CPC

- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/29: Bond pads specially adapted therefor
- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/01238: {in gaseous form, e.g. by CVD or PVD}
- H10W 72/01255: {by using masks}
- H10W 72/01257: {by reflowing}
- H10W 72/019: {of bond pads}
- H10W 72/01935: {by plating, e.g. electroless plating or electroplating}
- H10W 72/01938: {in gaseous form, e.g. by CVD or PVD}
- H10W 72/232: {Plan-view shape, i.e. in top view}
- H10W 72/241: {Dispositions, e.g. layouts}
- H10W 72/242: {relative to the surface, e.g. recessed, protruding}
- H10W 72/90: Bond pads, in general
- H10W 72/921: {Structures or relative sizes of bond pads}
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/934: {Cross-sectional shape, i.e. in side view}
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 72/942: {relative to underlying supporting features, e.g. bond pads, RDLs or vias}
- H10W 70/05: of insulating or insulated package substrates, or of interposers, or of redistribution layers (manufacture or treatment of leadframes H10W70/04)
- H10W 70/65: Shapes or dispositions of interconnections
- H10W 70/66: Conductive materials thereof
- H10W 72/01235: {by plating, e.g. electroless plating or electroplating}
- H10W 72/01951: {Changing the shapes of bond pads}
- H10W 72/01953: {by etching}
- H10W 72/221: {Structures or relative sizes}
- H10W 72/222: {Multilayered bumps, e.g. a coating on top and side surfaces of a bump core}
- H10W 72/223: {characterised by the structure of the outermost layers, e.g. multilayered coatings}
- H10W 72/234: {Cross-sectional shape, i.e. in side view}
- H10W 72/235: {of outermost layers of multilayered bumps, e.g. bump coating not being conformal on a bump core}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/255: {of outermost layers of multilayered bumps, e.g. material of a coating}
- H10W 72/932: {Plan-view shape, i.e. in top view}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Interconnect bump structures with copper bumps on copper pads. An embodiment interconnect bump structure comprises a first passivation layer; a copper pad on the first passivation layer; a copper bump on the copper pad; a tin-silver bump over the copper bump; and a second passivation layer over the first passivation layer, wherein the copper bump passes through an opening in the second passivation layer.

## Claims

### Claim 1

An interconnect bump structure comprising:
a first passivation layer;
a copper pad formed over the first passivation layer;
a copper bump formed over the copper pad;
solder material formed over the copper bump; and
a second passivation layer formed over the first passivation layer, wherein the copper bump is formed through an opening in the second passivation layer.

### Claim 2 (depends on 1)

The interconnect bump structure of claim 1, wherein a ratio RW between a width of the copper bump and a width of the opening in the second passivation layer is between 0.4 and 2, inclusive.

### Claim 3 (depends on 1)

The interconnect bump structure of claim 1, wherein the second passivation layer comprises a substantially flat top surface.

### Claim 4 (depends on 1)

The interconnect bump structure of claim 1, wherein the first passivation layer comprises a layer of SiN formed over a layer of SiCN.

### Claim 5 (depends on 1)

The interconnect bump structure of claim 1, wherein the second passivation layer comprises layer of SiN formed over a layer of SiO2 which is formed over a layer of SiO.

### Claim 6 (depends on 1)

The interconnect bump structure of claim 1, comprising an auxiliary layer on the copper bump, wherein the solder material is on the auxiliary layer, and wherein the auxiliary layer comprises at least one of nickel, palladium-gold, or cobalt.

### Claim 7 (depends on 1)

The interconnect bump structure of claim 1, wherein the second passivation layer comprises a sloped sidewall that slopes from a top surface of the second passivation layer to a top surface of the first passivation layer, and wherein the sloped sidewall creates an angle A between the sidewall and the top surface of the first passivation layer, and wherein the angle A is between 60° and 90°, inclusive.

### Claim 8 (depends on 1)

The interconnect bump structure of claim 1, wherein the copper bump and the solder material form a conductive terminal providing an electrical connection for a ground or power supply voltage between the interconnect bump structure and an external component, the conductive terminal including a solder region and an intermetallic compound (IMC) region.

### Claim 9 (depends on 1)

The interconnect bump structure of claim 1, comprising a polyimide layer over the second passivation layer.

### Claim 10

An interconnect bump structure comprising:
a copper pad;
a dummy structure adjacent to the copper pad;
a copper bump formed over the copper pad;
a tin-silver bump formed over the copper bump; and
a passivation layer supported by the dummy structure such that the passivation layer comprises a substantially flat top surface,
wherein the copper bump passes through an opening in the passivation layer, and
wherein a top surface of the dummy structure is covered by the passivation layer.

### Claim 11 (depends on 10)

The interconnect bump structure of claim 10, wherein the copper pad has a circular shape.

### Claim 12 (depends on 11)

The interconnect bump structure of claim 11, wherein the dummy structure comprises copper dummy pads on opposite sides of the copper pad.

### Claim 13 (depends on 10)

The interconnect bump structure of claim 10, wherein the copper bump has a width between 21 μm and 35 μm, inclusive, and wherein the opening in the passivation layer has a width between 32 μm and 43 μm, inclusive.

### Claim 14 (depends on 11)

The interconnect bump structure of claim 11, wherein a ratio RW between a width of the copper bump and a width of the opening in the passivation layer is between 0.4 and 2, inclusive.

### Claim 15

A method of forming an interconnect bump structure, the method comprising:
depositing a first passivation layer;
forming a copper pad over the first passivation layer;
depositing a second passivation layer over the first passivation layer;
forming a copper bump on the copper pad such that the copper bump passes through an opening in the second passivation layer; and
forming a tin-silver bump over the copper bump.

### Claim 16 (depends on 15)

The method of claim 15, comprising depositing a polyimide layer over the second passivation layer.

### Claim 17 (depends on 15)

The method of claim 15, wherein forming the copper pad further comprises forming a copper dummy structure adjacent to the copper pad.

### Claim 18 (depends on 15)

The method of claim 15, wherein forming the copper pad comprises forming the copper pad in a circular shape, and wherein forming the copper dummy structure comprises forming copper dummy pads on opposite sides of the copper pad.

### Claim 19 (depends on 15)

The method of claim 15, wherein depositing the second passivation layer comprises depositing the second passivation layer to form a substantially flat top surface and patterning and etching the second passivation layer such that the opening in the second passivation layer has a width between 32 μm and 43 μm, inclusive.

### Claim 20 (depends on 15)

The method of claim 15, comprising forming a nickel layer on the copper bump, wherein depositing the tin-silver bump comprises depositing the tin-silver bump on the nickel layer.