# US 2026/0198231 A1 · Thin film having single-crystal-level crystal orientation property, and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0198231 A1
- Document ID: US20260198231A1
- Status: Published application
- Kind: A1
- Application number: 19/557,696
- Filed: 2026-03-05
- Published: 2026-07-09
- Earliest claimed: 2018-11-02
- Assignees: Korea Electrotechnology Research Institute
- Applicants: Korea Electrotechnology Research Institute
- Inventors: Ho Sup KIM; Sang Soo OH; Hong Soo HA; Jeong Hyeon JO; Gwan Tae KIM; Hyun Woo NOH
- Web page: https://patentgrep.com/patent/US20260198231A1

## CPC

- H10N 50/85: Materials of the active region
- H10N 60/0576: {characterised by the substrate}
- C21D 6/00: Heat treatment of ferrous alloys
- C22C 38/10: containing cobalt
- C23C 14/02: Pretreatment of the material to be coated (C23C14/04 takes precedence)
- C23C 14/042: {using masks}
- C23C 14/14: Metallic material, boron or silicon
- C30B 30/00: Production of single crystals or homogeneous polycrystalline material with defined structure characterised by the action of electric or magnetic fields, wave energy or other specific physical conditions
- H10N 60/01: Manufacture or treatment
- H10N 60/83: Element shape
- H10N 60/85: Superconducting active materials
- C23C 14/16: on metallic substrates or on substrates of boron or silicon
- C23C 14/24: Vacuum evaporation
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

Proposed are a thin film having single crystallinity and an excellent crystal orientation property, a method of manufacturing the same, and a semiconductor device, a battery device, a superconducting wire, and a superconducting article including the thin film having single crystallinity. The technical gist of the present disclosure includes a thin film having single crystallinity, which is formed by depositing a polycrystalline second material on an upper portion of a substrate including a polycrystalline first material and which has a crystal orientation property satisfying the following Relational Expression 1 at a grain boundary, a method of manufacturing the same, and a semiconductor device, a battery device, a superconducting wire, and a superconducting article including the thin film having single crystallinity. 0°<FWHM2≤3° [Relational Expression 1] (FWHM2 is a full width at half maximum of a distribution curve of a misorientation angle at the grain boundary of the thin film).

## Claims

### Claim 1

A method of manufacturing a thin film, comprising:
preparing a substrate including a polycrystalline first material having first crystal grains of a first average grain size; and
forming the thin film by depositing a polycrystalline second material on an upper portion of the substrate so that second crystal grains of the second material are formed,
wherein the depositing is performed such that:
(i) the second crystal grains have a second average grain size greater than the first average grain size; and
(ii) crystal orientation of the second crystal grains is performed in parallel with an average direction of orientation axes of the first crystal grains of the substrate,
thereby yielding a thin film comprising the substrate and the polycrystalline second material formed on the upper portion of the substrate,
wherein the thin film has a crystal orientation property satisfying the following Relational Expression 1 at a grain boundary of the thin film:
0°<FWHM2≤30,
wherein FWHM2 is a full width at half maximum of a distribution curve of a misorientation angle at the grain boundary of the thin film, and
wherein the second average grain size is at least two times as large as the first average grain size.

### Claim 2 (depends on 1)

The method of claim 1, wherein the second material is Fe, a Fe alloy, or a Fe-based compound.

### Claim 3 (depends on 1)

The method of claim 1, wherein a crystal orientation property of the substrate and the crystal orientation property of the thin film satisfy the following Relational Expression 2:
5°≤(FWHM1-FWHM2)≤20°,
wherein FWHM1 and FWHM2 are full widths at half maximum of distribution curves of misorientation angles at grain boundaries of the substrate and of the thin film, respectively.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first material is a crystalline solid.