# US 2026/0198105 A1 · Short-wave dual-band infrared detector based on indium phosphide substrate and fabrication method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0198105 A1
- Document ID: US20260198105A1
- Status: Published application
- Kind: A1
- Application number: 19/443,703
- Filed: 2026-01-08
- Published: 2026-07-09
- Earliest claimed: 2025-01-09
- Assignees: Institute of Semiconductors, Chinese Academy Science
- Applicants: Institute of Semiconductors, Chinese Academy of Science
- Inventors: Hongyue HAO; Yingqiang XU; Zhichuan NIU; Guowei WANG; Donghai WU; Dongwei JIANG; Xiangbin SU
- Web page: https://patentgrep.com/patent/US20260198105A1

## CPC

- H10F 30/223: the potential barrier being a PIN barrier
- H10F 30/24: the devices having only two potential barriers, e.g. bipolar phototransistors
- H10F 30/21: the devices being sensitive to infrared, visible or ultraviolet radiation
- H10F 30/2215: {the devices comprising active layers made of only Group III-V materials}
- H10F 30/222: the potential barrier being a PN heterojunction
- H10F 30/288: {the devices being sensitive to multiple wavelengths, e.g. multi-spectrum radiation detection devices}
- H10F 71/1272: {comprising at least three elements, e.g. GaAlAs or InGaAsP}
- H10F 71/129: {Passivating}
- H10F 71/139: {using temporary substrates}
- H10F 77/1243: {characterised by the dopants}
- H10F 77/1248: {having three or more elements, e.g. GaAlAs, InGaAs or InGaAsP}
- H10F 77/146: {Superlattices; Multiple quantum well structures}
- H10F 77/147: {Shapes of bodies}
- H10F 77/241: {comprising ring electrodes}
- H10F 77/306: {for devices having potential barriers}
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present application relates to the field of infrared photoelectric materials and devices, and particularly to a short-wave dual-band infrared detector based on an indium phosphide substrate and a fabrication method thereof. An N-type doped indium phosphide substrate is used as a base of a device, and an indium phosphide absorption layer, a first P-type contact layer, a second P-type contact layer, a short-wave infrared superlattice absorption layer, and an N-type contact layer are sequentially grown on the N-type doped indium phosphide substrate. A lower metal electrode is in contact with the N-type doped indium phosphide substrate, and an upper metal electrode is in contact with the N-type contact layer and a light-transmitting hole is formed at a center of the upper metal electrode. In the present application, by using bandgap characteristics of the N-type doped indium phosphide substrate to participate in spectral absorption and converting the spectral absorption into an electrical signal for detection, a back-to-back diode structure is simultaneously employed to realize different responses to short-wave dual-band infrared by adjusting the bias voltage. Because the N-type doped indium phosphide substrate participates in spectral absorption, it is not necessary to remove the substrate in traditional methods, resulting in a simple epitaxial structure, reduced fabrication costs, and a simplified process.

## Claims

### Claim 1

A short-wave dual-band infrared detector based on an indium phosphide substrate, comprising:
an N-type doped indium phosphide substrate; and
an epitaxial structure deposited on the N-type doped indium phosphide substrate,
wherein the epitaxial structure is etched into a cylindrical shape and forms a bench structure with the N-type doped indium phosphide substrate,
wherein an annular lower metal electrode is provided at a location of the bench structure corresponding to the N-type doped indium phosphide substrate, and an annular upper metal electrode is provided at a location of the bench structure corresponding to a top of the epitaxial structure, a light-transmitting hole is formed at a center of the upper metal electrode, and a sulfide layer and a passivation layer are sequentially provided at a corresponding region of the bench structure other than the lower metal electrode, the upper metal electrode, and the light-transmitting hole;
wherein the epitaxial structure comprises:
an indium phosphide absorption layer grown on the indium phosphide substrate;
a first P-type contact layer grown on the indium phosphide absorption layer, the first P-type contact layer being doped with indium phosphide;
a second P-type contact layer grown on the first P-type contact layer, the second P-type contact layer being doped with aluminum gallium arsenide antimony alloy;
a short-wave infrared superlattice absorption layer grown on the second P-type contact layer; and
an N-type contact layer grown on the short-wave infrared superlattice absorption layer, the N-type contact layer being doped with gallium arsenide indium.

### Claim 2 (depends on 1)

The short-wave dual-band infrared detector based on the indium phosphide substrate of claim 1, wherein the N-type doped indium phosphide substrate is a (100)-oriented N-type sulfur-doped indium phosphide substrate.

### Claim 3 (depends on 1)

The short-wave dual-band infrared detector based on the indium phosphide substrate of claim 1, wherein both the lower metal electrode and the upper metal electrode comprise, from bottom to top, a titanium layer, a platinum layer, and a gold layer, the titanium layer having a thickness of 20 nm to 80 nm, the platinum layer having a thickness of 20 nm to 80 nm, and the gold layer having a thickness of 250 nm to 400 nm; the titanium layer of the lower metal electrode is in contact with the N-type doped indium phosphide substrate, and the titanium layer of the upper metal electrode is in contact with the N-type contact layer.

### Claim 4 (depends on 1)

The short-wave dual-band infrared detector based on the indium phosphide substrate of claim 1, wherein the indium phosphide absorption layer has a thickness of 500 nm to 2500 nm and a bandgap width of 1.34 eV to 1.35 eV.

### Claim 5 (depends on 1)

The short-wave dual-band infrared detector based on the indium phosphide substrate of claim 1, wherein the short-wave infrared superlattice absorption layer is at least one of a gallium arsenide indium superlattice or a gallium arsenide antimony superlattice, and the short-wave infrared superlattice absorption layer has a thickness of 500 nm to 2500 nm, and a bandgap width of 1.34 eV to 1.35 eV.

### Claim 6 (depends on 5)

The short-wave dual-band infrared detector based on the indium phosphide substrate of claim 5, wherein the short-wave infrared superlattice absorption layer comprises a plurality of gallium arsenide indium superlattice layers and a plurality of gallium arsenide antimony superlattice layers, the plurality of gallium arsenide indium superlattice layers and the plurality of gallium arsenide antimony superlattice layers being grown in an alternatively stacked manner to form the short-wave infrared superlattice absorption layer.

### Claim 7 (depends on 1)

A method for fabricating a short-wave dual-band infrared detector based on an indium phosphide substrate, used in fabricating the short-wave dual-band infrared detector based on the indium phosphide substrate in claim 1, comprising:
using an N-type doped indium phosphide substrate as a structural substrate of the infrared detector, and performing degassing and deoxidation pretreatment on the N-type doped indium phosphide substrate;
homoepitaxially growing, based on pretreated N-type doped indium phosphide substrate, an indium phosphide absorption layer on the N-type doped indium phosphide substrate;
growing a first P-type contact layer on the indium phosphide absorption layer;
growing a second P-type contact layer on the first P-type contact layer;
growing a short-wave infrared superlattice absorption layer on the second P-type contact layer;
growing an N-type contact layer on the short-wave infrared superlattice absorption layer;
constituting an epitaxial structure deposited on the N-type doped indium phosphide substrate based on the indium phosphide absorption layer, the first P-type contact layer, the second P-type contact layer, the short-wave infrared superlattice absorption layer as well as the N-type contact layer, performing inductively coupled plasma (ICP) etching on sides of the epitaxial structure to make the epitaxial structure cylindrical;
covering the N-type doped indium phosphide substrate and the epitaxial structure with a sulfide layer and a passivation layer;
fabricating a mask by photolithography at a location of the passivation layer corresponding to the N-type doped indium phosphide substrate, forming a first annular opening through reactive ion etching, fabricating a mask by photolithography at a location of the passivation layer corresponding to the N-type contact layer, and forming a second annular opening through reactive ion etching, and
performing evaporative deposition treatment at the first annular opening to form an annular lower metal electrode, and performing evaporative deposition treatment at the second annular opening to form an annular upper metal electrode and a light-transmitting hole.

### Claim 8 (depends on 7)

The method for fabricating the short-wave dual-band infrared detector based on the indium phosphide substrate of claim 7, wherein performing the degassing and deoxidation pretreatment on the N-type doped indium phosphide substrate comprises:
placing the N-type doped indium phosphide substrate in a sample introduction chamber of a molecular beam epitaxy system, maintaining a temperature of the sample introduction chamber at 200° C., and performing low-temperature degassing for 150 min;
transferring the N-type doped indium phosphide substrate subjected to low-temperature degassing into a buffer chamber of the molecular beam epitaxy system, maintaining a temperature of the buffer chamber at 360° C., and performing high-temperature degassing for 60 min to 100 min; and
transferring the N-type doped indium phosphide substrate subjected to high-temperature degassing into a growth chamber of the molecular beam epitaxy system, gradually heating the N-type doped indium phosphide substrate to 500° C. to 700° C., and performing deoxidation treatment for 15 min to 30 min to remove oxides on a surface of the N-type doped indium phosphide substrate.

### Claim 9 (depends on 7)

The method for fabricating the short-wave dual-band infrared detector based on the indium phosphide substrate of claim 7, wherein
the indium phosphide absorption layer has a growth rate of 0.5 monolayer per second, and grown indium phosphide absorption layer has a thickness of 500 nm to 2500 nm;
the first P-type contact layer has a growth rate of 0.5 monolayer per second, and grown first P-type contact layer has a thickness of 200 nm to 400 nm;
the second P-type contact layer has a growth rate of 0.5 monolayer per second, and grown second P-type contact layer has a thickness of 400 nm to 600 nm;
the short-wave infrared superlattice absorption layer has a growth rate of 0.5 monolayer per second, and grown short-wave infrared superlattice absorption layer has a thickness of 500 nm to 2500 nm; and
the N-type contact layer has a growth rate of 0.5 monolayer per second, and grown N-type contact layer has a thickness of 150 nm to 2500 nm.

### Claim 10 (depends on 7)

The method for fabricating the short-wave dual-band infrared detector based on the indium phosphide substrate of claim 7, wherein growing the short-wave infrared superlattice absorption layer on the second P-type contact layer comprises:
growing a gallium arsenide indium superlattice layer on the second P-type contact layer, and growing a gallium arsenide antimony superlattice layer on grown gallium arsenide indium superlattice layer; and
using the grown gallium arsenide indium superlattice layer and grown gallium arsenide antimony superlattice layer as a periodic unit, continuing to grow a plurality of periodic units upwards until a total thickness of all periodic units reaches 500 nm to 2500 nm to form the short-wave infrared superlattice absorption layer.