# US 2026/0194706 A1 · Method and device for preparing semiconductor three-dimensional micro/nanostructures with tunable bandgap and semiconductor three-dimensional micro/nanostructure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0194706 A1
- Document ID: US20260194706A1
- Status: Published application
- Kind: A1
- Application number: 19/096,737
- Filed: 2025-04-01
- Published: 2026-07-09
- Earliest claimed: 2025-01-09
- Assignees: China University of Geosciences (Wuhan)
- Applicants: China University of Geosciences, Wuhan
- Inventors: Jing Zhang; Yao Wang; Ziyi Ding; Tianye Huang; Xiangyun Hu
- Web page: https://patentgrep.com/patent/US20260194706A1

## CPC

- G02B 6/0239: {Comprising means for varying the guiding properties, e.g. tuning means}
- C03B 37/0146: {Furnaces therefor, e.g. muffle tubes, furnace linings}
- G02B 1/005: {made of photonic crystals or photonic band gap materials (photonic band-gap structures or photonic lattices in integrated optics G02B6/1225; photonic band-gap structures or photonic lattices in optical fibres G02B6/02295)}
- G02B 6/02309: {Structures extending perpendicularly or at a large angle to the longitudinal axis of the fibre, e.g. photonic band gap along fibre axis}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

The present disclosure belongs to the field of semiconductor device manufacturing technology, specifically disclosing a method for preparing semiconductor three-dimensional micro/nanostructures with tunable bandgap, including: heating a semiconductor-core optical fiber, and controlling the cooling rate, wherein the heating process and cooling rate have a corresponding relationship with the stress applied to the semiconductor three-dimensional micro/nanostructure, and this stress can tune the bandgap. In the situation where the target heating temperature is higher than the melting point of the fiber core, heating the optical fiber partially to apply controllable compressive stress to form a semiconductor three-dimensional micro/nanostructure and tune its bandgap. In the situation where the target heating temperature is lower than the melting point of the fiber core, heating the whole optical fiber to recrystallize the semiconductor three-dimensional micro/nanostructure, and using the volume mismatch to apply tensile stress to the semiconductor three-dimensional micro/nanostructure and tune its bandgap.

## Claims

### Claim 1

A method for preparing a semiconductor three-dimensional micro/nanostructure with tunable bandgap, comprising:
heating a semiconductor optical fiber according to a target heating temperature, and controlling a cooling rate of the optical fiber during cooling, wherein a heating process and the cooling rate have a corresponding relationship with a stress applied to a fiber core and the semiconductor three-dimensional micro/nanostructure in the optical fiber, the stress is able to tune the bandgap of the semiconductor three-dimensional micro/nanostructure;
wherein in a situation where the target heating temperature is higher than a melting point of the fiber core, the optical fiber is partially heated to apply a compressive stress to the fiber core and form the semiconductor three-dimensional micro/nanostructure; in a situation where the target heating temperature is lower than the melting point of the fiber core, the whole optical fiber is heated to recrystallize the semiconductor three-dimensional micro/nanostructure, and a volume difference between a recrystallized structure and an original structure is utilized to apply a tensile stress to the semiconductor three-dimensional micro/nanostructure, and a bandgap structure is tuned.

### Claim 2 (depends on 1)

The method for preparing the semiconductor three-dimensional micro/nanostructure with tunable bandgap according to claim 1, wherein the heating of the semiconductor optical fiber according to the target heating temperature, and controlling the cooling rate when cooling the optical fiber comprises:
heating a target area by a first heating source, wherein during the heating process, the optical fiber enter and leave the target area according to a target moving speed, so as to make the fiber core to form into the semiconductor three-dimensional micro/nanostructure, the target area and the optical fiber are located in a same horizontal plane, the target heating temperature specifically refers to a temperature at a center of the target area, which is higher than the melting point of the fiber core of the optical fiber, the optical fiber has a first cooling rate in a process of leaving the target area.

### Claim 3 (depends on 2)

The method for preparing the semiconductor three-dimensional micro/nanostructure with tunable bandgap according to claim 2, wherein in a situation where the first heating source conducts uniform heating to the target area, a shape of the semiconductor three-dimensional micro/nanostructure is spherical;
in a situation where the first heating source conducts non-uniform heating to the target area, the shape of the semiconductor three-dimensional micro/nanostructure is non-spherical.

### Claim 4 (depends on 2)

The method for preparing the semiconductor three-dimensional micro/nanostructure with tunable bandgap according to claim 2, wherein the first heating source is a laser, and before heating the target area through the first heating source, the method further comprises:
adjusting a height of the laser to determine a spot size formed by a laser emitted from the laser in the target area, wherein the spot size affects the cooling rate, where the smaller spot size results in the faster first cooling rate.

### Claim 5 (depends on 4)

The method for preparing the semiconductor three-dimensional micro/nanostructure with tunable bandgap according to claim 4, further comprising:
acquiring an image of the optical fiber in the target area;
displaying the image and receiving a target input, wherein the image is used to calculate and quantify a numerical value of the cooling rate utilizing a blackbody radiation principle, and the target input is used to indicate an adjustment amount of a moving speed and an adjustment amount of an laser power;
in response to the target input, based on the adjustment amount of the moving speed and the adjustment amount of the laser power, a target moving speed of the optical fiber and the laser power are controlled.

### Claim 6 (depends on 2)

The method for preparing the semiconductor three-dimensional micro/nanostructure with tunable bandgap according to claim 2, further comprising: through a moving stage carrying the optical fiber, the moving stage is used to carry the optical fiber and move the optical fiber at a target speed during the process of heating the target area by the first heating source.

### Claim 7 (depends on 1)

The method for preparing the semiconductor three-dimensional micro/nanostructure with tunable bandgap according to claim 1, wherein the heating of the semiconductor optical fiber according to the target heating temperature and controlling the cooling rate when cooling the optical fiber comprises:
through a second heating source, the optical fiber processed by the first heating source is heated overall to recrystallize the semiconductor three-dimensional micro/nanostructure in the optical fiber, a target heating temperature provided by the second heating source for the optical fiber is lower than the melting point of the fiber core, the overall heating process comprises a temperature rising stage from a preset temperature to the target heating temperature, a temperature maintaining stage, and a temperature decreasing stage from the target heating temperature to the preset temperature, the temperature decreasing stage has a second cooling rate.

### Claim 8 (depends on 7)

The method for preparing the semiconductor three-dimensional micro/nanostructure with tunable bandgap according to claim 7, wherein the second heating source is a tubular furnace;
the tubular furnace is utilized to hold the optical fiber containing the semiconductor three-dimensional micro/nanostructure after being processed by the first heating source, and in a vacuum environment, a temperature inside the furnace is adjusted according to a target furnace temperature, a heating rate, a cooling rate, and a holding time, where the target furnace temperature is the target heating temperature, and the cooling rate is the second cooling rate.

### Claim 9

A device for preparing a semiconductor three-dimensional micro/nanostructure with tunable bandgap, comprising: a carrier and a heating module;
wherein the carrier is configured for placing an optical fiber;
the heating module is provided to performing heating according to a target heating temperature, and control a cooling rate when the optical fiber is cooled, a heating process and the cooling rate have a corresponding relationship with a stress applied to a fiber core and the semiconductor three-dimensional micro/nanostructure in the optical fiber, the stress is able to tune the bandgap of the semiconductor three-dimensional micro/nanostructure;
wherein in a situation where the target heating temperature is higher than a melting point of the fiber core, the optical fiber is partially heated to apply a compressive stress to the fiber core and form the semiconductor three-dimensional micro/nanostructure; in a situation where the target heating temperature is lower than the melting point of the fiber core, the whole optical fiber is heated to recrystallize the semiconductor three-dimensional micro/nanostructure, and a volume difference between a recrystallized structure and an original structure is utilized to apply a tensile stress to the semiconductor three-dimensional micro/nanostructure, and the bandgap structure is tuned.

### Claim 10 (depends on 1)

A semiconductor three-dimensional micro/nanostructure, wherein the semiconductor three-dimensional micro/nanostructure is obtained by applying the method of preparing the semiconductor three-dimensional micro/nanostructure with tunable bandgap according to claim 1.