# US 2026/0193822 A1 · Spunbond non-woven fabrics for filters and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0193822 A1
- Document ID: US20260193822A1
- Status: Published application
- Kind: A1
- Application number: 19/132,805
- Filed: 2023-11-07
- Published: 2026-07-09
- Earliest claimed: 2022-12-26
- Assignees: Kolon Industries, Inc.
- Applicants: Kolon Industries, Inc.
- Inventors: Woo-seok CHOI; Min-ho LEE; Hee-jung CHO; Young-shin PARK; Dong-heon KANG; Jung-soon JANG
- Web page: https://patentgrep.com/patent/US20260193822A1

## CPC

- D04H 3/153: Mixed yarns or filaments
- B01D 39/16: of organic material, e.g. synthetic fibres
- D01D 5/08: Melt spinning methods {(D01D5/0023 takes precedence)}
- D01F 6/62: from polyesters
- D01F 8/14: with at least one polyester as constituent
- D04H 3/011: Polyesters
- D04H 3/016: characterised by the fineness
- D04H 3/018: characterised by the shape
- D04H 3/147: Composite yarns or filaments
- D04H 3/16: with bonds between thermoplastic filaments produced in association with filament formation, e.g. immediately following extrusion
- D06M 15/564: Polyureas, polyurethanes or other polymers having ureide or urethane links; Precondensation products forming them
- D10B 2331/04: polyesters, e.g. polyethylene terephthalate [PET]
- D04H: MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARY MATERIAL (weaving D03; knitting D04B; braiding D04C; net-making D04G; sewing D05B; tufting D05C; finishing non-woven fabrics D06); FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS, NON-WOVEN FABRICS; COTTON-WOOL; WADDING {; NON-WOVEN FABRICS FROM STAPLE FIBRES, FILAMENTS OR YARNS, BONDED WITH AT LEAST ONE WEB-LIKE MATERIAL DURING THEIR CONSOLIDATION}(non-woven fabrics having an intermediate or external layer of a different kind, e.g. of woven fabric, B32B)
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

The present disclosure relates to a spunbond nonwoven fabric for filters and a method for manufacturing the same. According to the present disclosure, there is provided a spunbond nonwoven fabric for filters having excellent filtration performance and a long service life, as well as a method for manufacturing the same.

## Claims

### Claim 1

A spunbond nonwoven fabric for filters, comprising a fiber web in which a first polyester filament having a melting point of 250° C. or higher and a second polyester filament having a melting point of 150° C. to 220° C. are mixedly spun,
wherein the first polyester filament has a fineness of 1 to 10 denier and includes hollow cross-section filaments and heteromorphic cross-section filaments,
wherein the hollow cross-section filaments and the heteromorphic cross-section filaments have a fineness difference of 2 denier or more.

### Claim 2 (depends on 1)

The spunbond nonwoven fabric for filters according to claim 1,
wherein the fiber web comprises 70 to 95 wt % of the first polyester filament and 5 to 30 wt % of the second polyester filament.

### Claim 3 (depends on 1)

The spunbond nonwoven fabric for filters according to claim 1,
wherein the first polyester filament comprises 30 to 70 wt % of the hollow cross-section filaments and 30 to 70 wt % of the heteromorphic cross-section filaments.

### Claim 4 (depends on 1)

The spunbond nonwoven fabric for filters according to claim 1,
wherein the hollow cross-section filaments and the heteromorphic cross-section filaments have a fineness difference of 3 to 9 denier.

### Claim 5 (depends on 1)

The spunbond nonwoven fabric for filters according to claim 1,
wherein the hollow cross-section filaments have a hollowness ratio of 10% to 30%,
wherein the hollowness ratio is a percentage of an area of an inscribed circle based on an area of a circumscribed circle of the hollow cross-section.

### Claim 6 (depends on 1)

The spunbond nonwoven fabric for filters according to claim 1,
wherein the heteromorphic cross-section filaments have a cross-section shape of a Y-shaped, W-shaped, triangular, star-shaped, cross-shaped, flat-shaped, or multi-lobed shaped.

### Claim 7 (depends on 1)

The spunbond nonwoven fabric for filters according to claim 1,
wherein the second polyester filament is a circular cross-section filament having a fineness of 1 to 5 denier.

### Claim 8 (depends on 1)

The spunbond nonwoven fabric for filters according to claim 1,
wherein the spunbond nonwoven fabric has a basis weight of 100 g/m2 to 350 g/m2.

### Claim 9 (depends on 1)

The spunbond nonwoven fabric for filters according to claim 1,
wherein the spunbond nonwoven fabric has a thickness of 0.1 mm to 1.0 mm.

### Claim 10 (depends on 1)

A method for manufacturing a spunbond nonwoven fabric for filters according to claim 1, comprising the steps of:
melt-spinning a first polyester having a melting point of 250° C. or higher to form a first polyester filament,
melt-spinning a second polyester having a melting point of 150° C. to 220° C. to form a second polyester filament,
forming a fiber web in which the first polyester filament and the second polyester filament are mixedly spun, and
heat-treating the fiber web under pressure to form a spunbond nonwoven fabric;
wherein the first polyester filament has a fineness of 1 to 10 denier and includes hollow cross-section filaments and heteromorphic cross-section filaments,
wherein the hollow cross-section filaments and the heteromorphic cross-section filaments have a fineness difference of 2 denier or more.

### Claim 11 (depends on 10)

The method for manufacturing a spunbond nonwoven fabric for filters according to claim 10,
wherein the steps of forming the first polyester filament and forming the second polyester filament are performed at a spinning speed of 4000 m/min to 6000 m/min, respectively.