Abstract
This disclosure methods of reducing circulation loss in a using a sealant composition, including volcanic ash, cement, an epoxy resin, and a crosslinker.
Claims23
A method of reducing circulation loss in a wellbore, comprising:
- applying a sealant composition to the wellbore, the sealant composition comprising:
- volcanic ash, wherein the volcanic ash is in particle form and about 80% of the volcanic ash particles have a diameter of less than about 60 μm;
- cement;
- about 70 wt % to about 92 wt % of epoxy resin;
- a crosslinker.
2 more elements
-6. (canceled)
A method of reducing circulation loss in a wellbore, comprising:
- applying a sealant composition to the wellbore, the sealant composition comprising:
- about 1 wt % to about 10 wt % volcanic ash, wherein the volcanic ash is in particle form and about 80% of the volcanic ash particles have a diameter of less than about 60 μm;
- about 1 wt % to about 10 wt % cement;
- about 70 wt % to about 92 wt % bisphenol-A-epichlorohydrin epoxy resin comprising an oxirane mono [(C12-14)-alkyloxy)methyl] derivative;
- and
- about 1 wt % to about 10 wt % diethylenetriamine (DETA).