# US 2026/0193446 A1 · Thermoplastic resin composition, and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0193446 A1
- Document ID: US20260193446A1
- Status: Published application
- Kind: A1
- Application number: 18/863,896
- Filed: 2023-11-08
- Published: 2026-07-09
- Earliest claimed: 2022-11-10
- Assignees: Lotte Fine Chemical Co., Ltd.
- Applicants: Lotte Fine Chemical Co., Ltd.
- Inventors: Dooho Kim; Gyujong Jeon; Gyungdon Kang
- Web page: https://patentgrep.com/patent/US20260193446A1

## CPC

- C08K 5/053: Polyhydroxylic alcohols
- C08L 1/284: {with hydroxylated hydrocarbon radicals}
- C08K 3/013: Fillers, pigments or reinforcing additives
- C08K 5/0025: {Crosslinking or vulcanising agents; including accelerators}
- C08K 5/0033: {Additives activating the degradation of the macromolecular compound}
- C08K 5/005: {Stabilisers against oxidation, heat, light, ozone}
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present invention relates to a thermoplastic resin composition and a preparation method therefor and, more specifically, to: an environmentally friendly thermoplastic resin composition which is biodegradable, has excellent molding processability, and has improved mechanical properties such as tensile strength and elongation, and which can be applied as an environmentally friendly material in various fields; and a preparation method therefor.

## Claims

### Claim 1

A thermoplastic resin composition comprising:
65 wt % to 80 wt % of hydroxyethyl cellulose having a viscosity in a range of 4,000 cps to 250,000 cps, the viscosity obtained when measuring an aqueous solution in which 2 wt % of hydroxyethyl cellulose is dissolved in water at a temperature of 20° C. using a Brookfield viscometer; and
20 wt % to 35 wt % of glycerin.

### Claim 2 (depends on 1)

The thermoplastic resin composition of claim 1, further comprising one or more additives selected from the group consisting of an antioxidant, a lubricant, a biodegradation accelerator, and a strength reinforcing agent.

### Claim 3 (depends on 2)

The thermoplastic resin composition of claim 2, wherein the lubricant is one or more selected from the group consisting of sorbitol, magnesium stearate, calcium stearate, ethylene glycol, glycerol monostearate, and lecithin.

### Claim 4

A method of preparing a thermoplastic resin composition, the method comprising:
(a) adding 20 wt % to 35 wt % of glycerin to 65 wt % to 80 wt % of hydroxyethyl cellulose having a viscosity in a range of 4,000 cps to 250,000 cps, the viscosity obtained when measuring an aqueous solution in which 2 wt % of hydroxyethyl cellulose is dissolved in water at a temperature of 20° C. using a Brookfield viscometer; and
(b) kneading the resulting mixture for plasticization.

### Claim 5 (depends on 4)

The method of claim 4, wherein the (b) kneading is performed in a temperature range of 50° C. to 90° C. at a speed of 300 rpm or higher.

### Claim 6 (depends on 1)

A molded article formed from the thermoplastic resin composition of claim 1.

### Claim 7 (depends on 6)

The molded article of claim 6, wherein the molded article has a tensile strength in a range of 4.5 MPa to 6.5 MPa measured according to ASTM D638.

### Claim 8 (depends on 6)