# US 2026/0193443 A1 · Method for decomposing fluorine-containing polymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0193443 A1
- Document ID: US20260193443A1
- Status: Published application
- Kind: A1
- Application number: 19/551,983
- Filed: 2026-02-27
- Published: 2026-07-09
- Earliest claimed: 2023-09-01
- Assignees: Daikin Industries, Ltd.; Kanagawa University
- Applicants: Daikin Industries, Ltd.; Kanagawa University of
- Inventors: Ayane NAKAUE; Hirofumi Mukae; Yosuke Kishikawa; Hisao Hori; Jin Hamaura
- Web page: https://patentgrep.com/patent/US20260193443A1

## CPC

- C08J 11/14: by treatment with steam or water
- C08F 8/26: Removing halogen atoms or halogen-containing groups from the molecule
- C08J 11/16: by treatment with inorganic material (C08J11/14 takes precedence)
- C08F 214/22: Vinylidene fluoride
- C08J 2327/12: containing fluorine atoms
- Y02W 30/62: Plastics recycling; Rubber recycling
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method for decomposing a fluorine-containing polymer that can decompose a fluorine-containing polymer while suppressing generation of impurities after the decomposition reaction. A method for decomposing a fluorine-containing polymer, including a decomposition step including reacting a fluorine-containing polymer in subcritical water that is at a temperature of 180° C. or higher and lower than 250° C. and that contains at least one basic compound selected from the group consisting of alkali metal hydroxides and alkaline earth metal hydroxides at a concentration of 0.5 M or lower.

## Claims

### Claim 1

A method for decomposing a fluorine-containing polymer, comprising
a decomposition step including reacting a fluorine-containing polymer in subcritical water that is at a temperature of 180° C. or higher and lower than 250° C. and that contains at least one basic compound selected from the group consisting of alkali metal hydroxides and alkaline earth metal hydroxides at a concentration of 0.5 M or lower.

### Claim 2 (depends on 1)

The method for decomposing a fluorine-containing polymer according to claim 1,
wherein the temperature of the subcritical water in the decomposition step is 200° C. or higher.

### Claim 3 (depends on 1)

The method for decomposing a fluorine-containing polymer according to claim 1,
wherein the fluorine-containing polymer is a fluororubber.

### Claim 4 (depends on 3)

The method for decomposing a fluorine-containing polymer according to claim 3,
wherein the temperature of the subcritical water in the decomposition step is 200° C. or higher and 235° C. or lower,
the concentration of the at least one basic compound in the subcritical water is 0.10 M or higher and 0.35 M or lower, and
the fluororubber is a copolymer of 50 to 80 mol % vinylidene fluoride and 50 to 20 mol % hexafluoropropylene.

### Claim 5 (depends on 3)

The method for decomposing a fluorine-containing polymer according to claim 3,
wherein the fluorine-containing polymer to be decomposed in the decomposition step is a cross-linked material of a composition containing the fluororubber.

### Claim 6 (depends on 1)

The method for decomposing a fluorine-containing polymer according to claim 1,
wherein the method comprises, before the decomposition step, a pulverization step of pulverizing the fluorine-containing polymer into pulverized particles having a maximum linear length of 3 mm or less.

### Claim 7 (depends on 1)

The method for decomposing a fluorine-containing polymer according to claim 1,
wherein the at least one basic compound is at least one of sodium hydroxide or potassium hydroxide.

### Claim 8 (depends on 1)

The method for decomposing a fluorine-containing polymer according to claim 1,
wherein the method comprises, after the decomposition step, a recovery step of recovering calcium fluoride generated by adding calcium hydroxide to an aqueous solution after the decomposition.