# US 2026/0193424 A1 · Bio based natural rubber solutions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0193424 A1
- Document ID: US20260193424A1
- Status: Published application
- Kind: A1
- Application number: 19/133,311
- Filed: 2023-11-30
- Published: 2026-07-09
- Earliest claimed: 2022-12-02
- Assignees: Fraunhofer-Gesellschaft zur Förderung der angewandten Forschung e. V.
- Applicants: Fraunhofer-Gesellschaft zur Förderung der angewandten Forschung e. V.
- Inventors: Christian Schulze Gronover; Lowis-Gerrit-Boje Müller
- Web page: https://patentgrep.com/patent/US20260193424A1

## CPC

- C08J 3/09: in organic liquids
- C09J 107/00: Adhesives based on natural rubber
- C08J 3/092: {Hydrocarbons}
- C08K 5/01: Hydrocarbons {(C08K5/0091 takes precedence)}
- C08K 5/13: Phenols; Phenolates
- C09D 107/00: Coating compositions based on natural rubber
- C08J 2307/00: Characterised by the use of natural rubber
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

The present invention relates to a natural rubber solution that is obtained by dissolving natural rubber in a terpene, the process to obtain the natural rubber solution and uses thereof.

## Claims

### Claim 1

A natural rubber solution, comprising:
i) a natural rubber, and
ii) at least one terpene.

### Claim 2 (depends on 1)

The natural rubber solution according to claim 1, wherein the natural rubber is selected from the group consisting of Standard Malaysian rubber, Standard African rubber and Standard Thai rubber, Standard Indonesian Rubber, Standard Nigerian Rubber, Standard Vietnamese Rubber, Standard Chinese Rubber, dandelion rubber, guayule rubber and combinations thereof, preferably Standard Malaysian rubber, Standard African rubber and Standard Thai rubber and combinations thereof.

### Claim 3 (depends on 1)

The natural rubber solution according to claim 1, wherein the at least one terpene is selected from the group consisting of polylimonene, limonene, carvone, α-pinene, citral, 1,8-cineole, eucalyptol, citronellol, geraniol, geranylgeraniol, citronellen, terpinen-4-ol, borneol, camphor, guayule resin, farnesene, and combinations thereof, preferably is selected from the group consisting of limonene, carvone, α-pinene, citral, 1,8 cineole, eucalyptol, citronellol, geraniol, geranylgeraniol, citronellen, terpinen-4-ol and farnesene, more preferably, is limonene.

### Claim 4 (depends on 1)

The natural rubber solution according to claim 1, wherein the solution comprises natural rubber in an amount of 0.01 to 99 parts by weight per hundred parts by weight of terpene.

### Claim 5 (depends on 1)

The natural rubber solution according to claim 1, wherein the solution further comprises at least one anti-aging agent.

### Claim 6 (depends on 5)

The natural rubber solution according to claim 5, wherein the anti-aging agent is selected from the group consisting of butylated hydroxytoluene (BHT); vitamin E in at least one stereoisomeric form such as tocopherol and tocotrienol, or a derivative thereof, N—C1-12 alkyl-N′-phenyl-p-phenylenediamines such as N-isopropyl-N′-phenyl-p-phenylenediamine, N-1,3-dimethylbutyl-N′-phenyl-p-phenylenediamine (6PPD), N-1,4-dimethylpentyl-N′-phenyl-p-phenylenediamine (7PPD), N,N′-bis-1,4-(1,4-dimethylpentyl)-p-phenylenediamine (77PD), diaryl-p-phenylenediamine (DTPD), 4,4′-bis(C1-12-alkylamino)triphenylamine; 7,8-dimethylisoalloxazine or a derivative thereof such as riboflavin; p-phenylenediamine; p-di(nitroso)arene such as poly-p-di(nitroso)benzene, oligomerized 2,2,4-trimethyl-1,2-dihydro-quinoline (TMQ), styrenated diphenylamine (DDA), cumylated diphenylamine, Zinc salt of 4- and 5-methylmercaptobenzimidazol, Zinc salt of di-n-butyldithiocarbamic acid, 2,6-di-tert-butylphenol, 2,6-di-tert-butyl-4-ethylphenol, 2,2′-methylen-bis(6-tert-butyl)-p-cresol, poly(dicyclopentadien-co-p-cresol), n-octadecyl-β-(4-hydroxy-3,5-di-tert-butyl-phenyl)-propionate, 2,2′-methylen-bis-(4-methyl-6-tert-butylphenol) (BPH), 2-methyl-4,6-bis(octylsulfanylmethyl)phenol, thiobisphenole, 4,4′-bis-(1,1-dimethylbenzyl)-diphenylamine (CDPA), octylated diphenylamine (ODPA), phenyl-a-naphthylamine (PAN), phenyl-β-naphthylamine (PBN), tris(nonylphenyl)phosphite, sodium hypophosphite, 2,2,4-trimethyl-1,2-dihydroquinoline (TMQ), 2-mercaptobenzimidazol (MBI), methyl-2-mercaptobenzimidazol (MMBI), and a mixture of reaction products between p-cresol and dicyclopentadiene corresponding to formula (I)
wherein n is any integer from 1 to 9,
or combinations thereof, preferably the anti-aging agent is a bio-based anti-aging agent, more preferably the anti-aging agent is butylated hydroxytoluene (BHT).

### Claim 7 (depends on 5)

The natural rubber solution according to claim 5, wherein the total content of the anti-aging agent is at least 0.01 phr (w/w) based on the amount of natural rubber.

### Claim 8 (depends on 1)

The natural rubber solution according to claim 1, wherein the dissolved natural rubber has one or more, or all of the following parameters:
a weight average molecular weight Mw of from 1.0 to 10.0×107 g/mol determined by thermal field-flow fractionation (ThFFF) measurement, and/or
a polydispersity index PD, being the ratio of Mw/Mn, of from 5.0 to 20.0 determined by ThFFF measurement, and/or
a Z average molecular weight Mz of from 5.0 to 35×107 g/mol determined by ThFFF measurement, and/or
a weight average gyration radius Rw of from 10 to 110 nm determined by ThFFF measurement, and/or
wherein the natural rubber solution has a dynamic shear viscosity at a constant shear rate of 50 s−1 of from 2300 to 2700 mPas when measured in dynamic shear measurements at a temperature of from 20 to 40° C.

### Claim 9 (depends on 1)

A process for obtaining the natural rubber solution according to claim 1, wherein the process comprises:
a. Providing a natural rubber;
b. Adding the natural rubber to a liquid terpene to obtain a mixture of solid natural rubber in liquid terpene; and
c. Incubating the mixture obtained in step b at a temperature in the range of 25° C. to 60° C. until the natural rubber is dissolved.

### Claim 10 (depends on 9)

The process according to claim 9, wherein the natural rubber is shredded into pieces before adding to the liquid terpene in step b and/or at least one anti-aging agent is added to the mixture of solid natural rubber in liquid terpene obtained in step b.

### Claim 11 (depends on 9)

A process for obtaining a cross-linked natural rubber, wherein the process according to claim 9 further comprises:
d. Adding a cross-linking agent; and
e. Drying the natural rubber solution containing a cross-linking agent; and
f. Heating the dried natural rubber containing a cross-linking agent obtained in step e.

### Claim 12 (depends on 11)

The process for obtaining a cross-linked natural rubber according to claim 11, wherein the cross-linking agent is added in step d in an amount of 0.01 to 3 phr (w/w) based on the amount of natural rubber and/or characterized in that the cross-linking agent is dicumyl peroxide.

### Claim 13 (depends on 11)

The process for obtaining a cross-linked natural rubber according to claim 11, wherein the heating in step f is performed at a temperature in the range of 50° C. to 250° C.

### Claim 14 (depends on 11)

A cross-linked natural rubber obtainable by the process according to claim 11 having a glass transition temperature of from −70° C. to −43° C., measured as tan δ in a dynamic mechanical analysis.

### Claim 15 (depends on 1)

The natural rubber solution according to claim 1, being a thickener, opacifier, lubricant, paint, a basis for solid natural rubber and in elastic coatings, elastic joints, elastic moldings, elastic sealings and elastic films.