# US 2026/0193125 A1 · Method for producing glass, mixture, dried product, and glass

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0193125 A1
- Document ID: US20260193125A1
- Status: Published application
- Kind: A1
- Application number: 19/559,441
- Filed: 2026-03-06
- Published: 2026-07-09
- Earliest claimed: 2023-09-08
- Assignees: AGC Inc.
- Applicants: AGC Inc.
- Inventors: Naoya WADA
- Web page: https://patentgrep.com/patent/US20260193125A1

## CPC

- C03C 1/024: {Chemical treatment of cullet or glass fibres}
- B09B 3/40: involving thermal treatment, e.g. evaporation (processes using mineral binders involving a melting or softening step B09B3/29; involving radiation B09B3/50)
- C03B 1/00: Preparing the batches (chemical compositions C03C)
- C03B 3/02: combined with preheating, premelting or pretreating the glass-making ingredients, pellets or cullet
- C03B 5/005: {of glass-forming waste materials (disposal or transformation of solid waste in general B09B; treatment of radioactive waste G21F9/00)}
- C03B 5/16: Special features of the melting process; Auxiliary means specially adapted for glass-melting furnaces
- C03C 1/004: {Refining agents (refining C03B5/225)}
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/105: containing aluminium
- C03C 3/11: containing halogen or nitrogen
- B09B 3/35: Shredding, crushing or cutting
- B09B 2101/50: Glass
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- B09B: DISPOSAL OF SOLID WASTE NOT OTHERWISE PROVIDED FOR
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A method for producing a glass, the method including: obtaining a mixture; and heating the mixture at a temperature of 700° C. or higher, in which the mixture contains a glass powder containing at least one heavy metal oxide selected from the group consisting of Sb2O3, PbO, and As2O3, a reducing agent, and a liquid medium, and the reducing agent is dissolved in the liquid medium.

## Claims

### Claim 1

A method for producing a glass, the method comprising:
obtaining a mixture; and
heating the mixture at a temperature of 700° C. or higher, wherein
the mixture comprises a glass powder comprising at least one heavy metal oxide selected from the group consisting of Sb2O3, PbO, and As2O3, a reducing agent, and a liquid medium, and
the reducing agent is dissolved in the liquid medium.

### Claim 2

A method for producing a glass, the method comprising:
obtaining a mixture;
drying the mixture to obtain a dried product; and
heating the dried product at a temperature of 700° C. or higher, wherein
the mixture comprises a glass powder comprising at least one heavy metal oxide selected from the group consisting of Sb2O3, PbO, and As2O3, a reducing agent, and a liquid medium,
the reducing agent is dissolved in the liquid medium, and
the dried product comprises the reducing agent and the glass powder comprising the heavy metal oxide.

### Claim 3 (depends on 1)

The method for producing a glass according to claim 1, wherein
the mixture comprises a halogenating agent.

### Claim 4 (depends on 2)

The method for producing a glass according to claim 2, wherein
the mixture comprises a halogenating agent.

### Claim 5 (depends on 3)

The method for producing a glass according to claim 3, wherein
the temperature for the heating is 1,000° C. or higher.

### Claim 6 (depends on 4)

The method for producing a glass according to claim 4, wherein
the temperature for the heating is 1,000° C. or higher.

### Claim 7 (depends on 1)

The method for producing a glass according to claim 1, wherein
the heating is carried out in an atmosphere that comprises water vapor and has a dew point temperature of 0° C. or higher.

### Claim 8 (depends on 2)

The method for producing a glass according to claim 2, wherein
the heating is carried out in an atmosphere that comprises water vapor and has a dew point temperature of 0° C. or higher.

### Claim 9 (depends on 1)

The method for producing a glass according to claim 1, wherein
the heating is carried out in an atmosphere that has a content ratio of oxygen of 30 mass % or less with respect to components other than water vapor.

### Claim 10 (depends on 2)

The method for producing a glass according to claim 2, wherein
the heating is carried out in an atmosphere that has a content ratio of oxygen of 30 mass % or less with respect to components other than water vapor.

### Claim 11 (depends on 1)

The method for producing a glass according to claim 1, wherein
the glass powder comprises Sb2O3 as the heavy metal oxide.

### Claim 12 (depends on 2)

The method for producing a glass according to claim 2, wherein
the glass powder comprises Sb2O3 as the heavy metal oxide.

### Claim 13 (depends on 1)

The method for producing a glass according to claim 1, wherein
the reducing agent is a water-soluble organic compound.

### Claim 14 (depends on 2)

The method for producing a glass according to claim 2, wherein
the reducing agent is a water-soluble organic compound.

### Claim 15 (depends on 1)

The method for producing a glass according to claim 1, wherein
the liquid medium is water.

### Claim 16 (depends on 2)

The method for producing a glass according to claim 2, wherein
the liquid medium is water.

### Claim 17 (depends on 1)

The method for producing a glass according to claim 1, wherein
the reducing agent is a saccharide.

### Claim 18 (depends on 2)

The method for producing a glass according to claim 2, wherein
the reducing agent is a saccharide.

### Claim 19 (depends on 1)

The method for producing a glass according to claim 1, wherein
the glass powder has a median diameter d50 of 100 μm or less.

### Claim 20 (depends on 2)

The method for producing a glass according to claim 2, wherein
the glass powder has a median diameter d50 of 100 μm or less.

### Claim 21 (depends on 1)

The method for producing a glass according to claim 1, wherein
at least one of the mixture or a dried product further comprises a glass raw material.

### Claim 22 (depends on 2)

The method for producing a glass according to claim 2, wherein
at least one of the mixture or the dried product further comprises a glass raw material.

### Claim 23 (depends on 1)

The method for producing a glass according to claim 1, wherein
the glass powder comprises, in terms of mass % based on an oxide;
SiO2: 60% to 80%;
Na2O: 5% to 20%;
MgO: 0% to 15%;
CaO: 5% to 20%;
Al2O3: 0% to 10%; and
the heavy metal oxide: 0.005% to 1%, and
the content of the heavy metal oxide means a total amount of Sb2O3, PbO, and As2O3.

### Claim 24 (depends on 2)

The method for producing a glass according to claim 2, wherein
the glass powder comprises, in terms of mass % based on an oxide;
SiO2: 60% to 80%;
Na2O: 5% to 20%;
MgO: 0% to 15%;
CaO: 5% to 20%;
Al2O3: 0% to 10%; and
the heavy metal oxide: 0.005% to 1%, and
the content of the heavy metal oxide means a total amount of Sb2O3, PbO, and As2O3.

### Claim 25

A mixture comprising:
a glass powder comprising at least one heavy metal oxide selected from the group consisting of Sb2O3, PbO, and As2O3;
a reducing agent; and
a liquid medium, wherein
the reducing agent is dissolved in the liquid medium.