# US 2026/0191255 A1 · Method for producing hollow filter rod of pla fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0191255 A1
- Document ID: US20260191255A1
- Status: Published application
- Kind: A1
- Application number: 18/838,571
- Filed: 2024-02-22
- Published: 2026-07-09
- Earliest claimed: 2023-02-24
- Assignees: China Tobacco Yunnan Industrial Co., Ltd
- Applicants: China Tobacco Yunnan Industrial Co., Ltd.
- Inventors: Baoshan YUE; Tao WANG; Han ZHENG; Jiao XIE; Jing ZHANG; Yanfei SHEN; Hao WANG; Jiang YU; Haiyan DING; Yongfa GUI
- Web page: https://patentgrep.com/patent/US20260191255A1

## CPC

- A24D 3/0229: {Filter rod forming processes (A24D3/0275 takes precedence)}
- A24D 3/064: {having non-circular cross-section}
- A24D 3/08: of organic materials as carrier or major constituent (of ion exchange materials A24D3/12)
- Y02W 90/10: Bio-packaging, e.g. packing containers made from renewable resources or bio-plastics
- A24D: CIGARS; CIGARETTES; TOBACCO SMOKE FILTERS; MOUTHPIECES OF CIGARS OR CIGARETTES; MANUFACTURE OF TOBACCO SMOKE FILTERS OR MOUTHPIECES
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present invention provides a method for producing a hollow filter rod of PLA fiber, relating to the technical field of hollow filter rods of PLA fiber, and comprising the following steps: loosening PLA fiber tows, then feeding the PLA fiber tows into a molding cavity, and heating and curing-molding the PLA fiber tows with heated air to obtain the hollow filter rods of PLA fiber. The present invention heats the PLA fiber tows by means of hot air heating to obtain the hollow filter rod PLA fiber after curing and molding, with good molding effect, good regularity, and low pollution.

## Claims

### Claim 1

A method for producing a hollow filter rod of PLA fiber, characterized in that, comprising the following steps:
loosening PLA fiber tows, then feeding the PLA fiber tows into a molding cavity, and heating and curing-molding the PLA fiber tows with heated air to obtain the hollow filter rod of PLA fiber.

### Claim 2 (depends on 1)

The method for producing the hollow filter rod of PLA fiber according to claim 1, characterized in that,
the temperature of the heated air is in a range of from 65° C. to 85° C.

### Claim 3 (depends on 2)

The method for producing the hollow filter rod of PLA fiber according to claim 2, characterized in that,
when the heated air is fed into the molding cavity, the heated air is pressurized by an air pump, and the air pump is electrically connected to a temperature sensing member in the molding cavity to adjust the output power of the air pump by obtaining real-time temperature in the molding cavity, such that the temperature in the molding cavity is between 65° C. and 85° C.

### Claim 4 (depends on 1)

The method for producing the hollow filter rod of PLA fiber according to claim 1, characterized in that,
a molding inner core is provided in the molding cavity, and the shape of the cross-section of the molding inner core comprises the shapes of a peach heart, a pentagram, a circle and a plum flower, such that the molded hollow filter rod of PLA fiber has a middle hole with a corresponding shape.

### Claim 5 (depends on 1)

The method for producing the hollow filter rod of PLA fiber according to claim 1, characterized in that,
the air is filtered before the air is heated.

### Claim 6 (depends on 1)

The method for producing the hollow filter rod of PLA fiber according to claim 1, characterized in that,
the total denier of the PLA tows ranges from 60000 d to 66000 d.

### Claim 7 (depends on 6)

The method for producing the hollow filter rod of PLA fiber according to claim 6, characterized in that,
the loosening is performed simultaneously with two strands of PLA tows, and the total denier of each strand of the PLA tows is in the range of 30000 d to 33000 d.

### Claim 8 (depends on 1)

The method for producing the hollow filter rod of PLA fiber according to claim 1, characterized in that,