# US 2026/0188757 A1 · Zinc-graphite battery based on bromine chemistry enabled by water-in-salt electrolyte

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0188757 A1
- Document ID: US20260188757A1
- Status: Published application
- Kind: A1
- Application number: 19/437,973
- Filed: 2025-12-31
- Published: 2026-07-02
- Earliest claimed: 2024-12-31
- Assignees: University of Sharjah
- Applicants: University of Sharjah
- Inventors: Sirugaloor Thangavel SENTHILKUMAR; Maryam Mohd Haitham MOUSELLY; Javad Basil Marutheri PARAMBATH; Anis ALLAGUI; Hussain ALAWADHI
- Web page: https://patentgrep.com/patent/US20260188757A1

## CPC

- H01M 10/26: Selection of materials as electrolytes
- H01M 4/38: of elements or alloys
- H01M 4/42: Alloys based on zinc
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 4/663: {containing carbon or carbonaceous materials as conductive part, e.g. graphite, carbon fibres}
- H01M 10/36: Accumulators not provided for in groups H01M10/05-H01M10/34
- H01M 10/365: {Zinc-halogen accumulators}
- H01M 2004/029: {Bipolar electrodes}
- H01M 2300/0011: Sulfuric acid-based
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present disclosure discloses a zinc-graphite battery based on bromine chemistry enabled by water-in-salt electrolyte is disclosed. The battery comprises a foil selected to serve as a cathode host for the electrochemical reactions involving bromide ions, an anode selected from zinc foil or graphite foil that serves as a current collector for zinc deposition and dissolution, and water-in-salt electrolyte (WiSE) comprising lithium chloride (LiCl), zinc chloride (ZnCl2), and potassium bromide (KBr). The WiSE provides bromide ions for cathodic reactions and zinc ions for anodic reactions. During charging, bromide ions are oxidized to bromine at the cathode and converted into tribromide, with subsequent bromine intercalation between graphene layers of the graphite foil, while zinc ions are deposited as metallic zinc at the anode. The battery achieves high discharge capacity, coulombic efficiency of not less than 91%, high-power density up to 199.5 mW/cm2, and extended cycle life of at least 800 cycles with a zinc foil anode or at least 1100 cycles with a graphite foil anode.

## Claims

### Claim 1

A zinc-graphite battery based on bromine chemistry enabled by water-in-salt electrolyte, comprising:
a graphite foil selected to serve as a cathode host for the electrochemical reactions involving bromide ions;
an anode selected from zinc foil or graphite foil that serves as a current collector for zinc deposition and dissolution; and
a water-in-salt electrolyte (WiSE) comprising lithium chloride (LiCl), zinc chloride (ZnCl2), and potassium bromide (KBr), wherein the WiSE provides bromide ions for cathodic reactions and zinc ions for anodic reactions.

### Claim 2 (depends on 1)

The zinc-graphite battery according to claim 1, wherein the graphite foil is directly used as a cathode host material without comprising a binder or a carrier.

### Claim 3 (depends on 1)

The zinc-graphite battery according to claim 1, comprising a floating-type cell configuration without a separator or membrane, wherein a safe distance is maintained between the cathode and the anode.

### Claim 4 (depends on 1)

The zinc-graphite battery according to claim 1, wherein no bromine complexing agents are employed, and the generated bromine and/or polybromide are stably stored in the graphite electrode.

### Claim 5 (depends on 1)

The zinc-graphite battery according to claim 1, wherein the water-in-salt electrolyte has a concentration of 16 mol/L for LiCl, 5 mol/L for ZnCl2, and 1 mol/L for KBr.

### Claim 6 (depends on 1)

The zinc-graphite battery according to claim 1, wherein the graphite foil of the cathode is subjected to a surface cleaning process comprising: immersing the graphite foil in a sulfuric acid aqueous solution at 80° C. for 2 hours, subsequently soaking it in distilled water overnight, washing it repeatedly with distilled water and ethanol, and finally drying it in an oven at 70° C. for 8 hours.

### Claim 7 (depends on 3)

The zinc-graphite battery according to claim 3, wherein the floating-type cell configuration uses acrylic plates as the cell case, silicon rubber as the gasket to maintain a safe distance, and titanium foil to establish electrical contact with the cathode and anode electrodes.

### Claim 8 (depends on 1)

The zinc-graphite battery according to claim 1, wherein the battery has a coulombic efficiency of not less than 91%, can achieve at least 800 cycles when the anode is zinc foil, and at least 1100 cycles when the anode host electrode is graphite foil.

### Claim 9

A method for preparing a bipolar-type zinc-graphite battery based on bromine chemistry enabled by water-in-salt electrolyte, comprising the following steps:
a) preparing a cathode host comprising graphite foil, which undergoes electrochemical reactions involving bromide ions;
b) preparing an anode selected from zinc foil or graphite foil that serves as a current collector for zinc deposition and dissolution;
c) preparing a water-in-salt electrolyte (WiSE) comprising lithium chloride (LiCl), zinc chloride (ZnCl2), and potassium bromide (KBr), wherein the WiSE provides bromide ions for cathodic reactions and zinc ions for anodic reactions;
d) assembling the cathode, the anode, and the water-in-salt electrolyte to obtain the bipolar-type zinc-graphite battery.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the graphite foil is directly used as a cathode host material without comprising a binder or a carrier.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the assembled bipolar-type zinc-graphite battery has a configuration without a separator or membrane, and a safe distance is maintained between the cathode and anode during assembly.

### Claim 12 (depends on 9)

The method according to claim 9, wherein no bromine complexing agents are employed in the preparation process, and the generated bromine and/or polybromide in the assembled battery are stably stored in the graphite electrode.

### Claim 13 (depends on 9)

The method according to claim 9, wherein the cathode and the anode, together with a titanium foil, are assembled to form a bipolar electrode structure, with one side for bromide redox reactions and the other for zinc redox reactions, when the anode prepared in step b) is graphite foil.

### Claim 14 (depends on 9)

The method according to claim 9, wherein the water-in-salt electrolyte prepared in step c) has a concentration of 16 mol/L for LiCl, 5 mol/L for ZnCl2, and 1 mol/L for KBr.

### Claim 15 (depends on 9)

The method according to claim 9, wherein the graphite foil of the cathode in step a) is subjected to a surface cleaning process comprising: immersing the graphite foil in a sulfuric acid aqueous solution at 80° C. for 2 hours, subsequently soaking it in distilled water overnight, washing it repeatedly with distilled water and ethanol, and finally drying it in an oven at 70° C. for 8 hours.

### Claim 16 (depends on 11)

The method according to claim 11, wherein when assembling the bipolar-type battery configuration, acrylic plates are used as the cell case, silicon rubber is used as the gasket to maintain a safe distance, and titanium foil is used to establish electrical contact with the cathode and anode.

### Claim 17 (depends on 9)

The method according to claim 9, wherein the bipolar-type zinc-graphite battery obtained by assembly delivers the capacity of 10.60 mAh, and the cell voltage of 6.64 V.