# US 2026/0188642 A1 · Thick-electrode cathode sheet, preparation method therefor, and primary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0188642 A1
- Document ID: US20260188642A1
- Status: Published application
- Kind: A1
- Application number: 19/338,704
- Filed: 2025-09-24
- Published: 2026-07-02
- Earliest claimed: 2024-12-31
- Assignees: Eve Energy Co., Ltd.
- Applicants: Eve Energy Co., Ltd.
- Inventors: Lida QIU; Huihui DENG; Bingmiao ZHANG; Yinyin FANG; Lang CAO; Yuan ZHU
- Web page: https://patentgrep.com/patent/US20260188642A1

## CPC

- H01M 4/04: Processes of manufacture in general
- H01M 4/0435: {Rolling or calendering}
- C08J 5/18: Manufacture of films or sheets
- C08K 3/04: Carbon
- C08K 3/22: of metals
- H01M 4/08: Processes of manufacture
- H01M 4/50: of manganese
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- C08J 2327/18: Homopolymers or copolymers of tetrafluoroethylene
- C08K 2003/2262: {of manganese}
- C08K 2201/001: Conductive additives
- C08K 2201/014: Additives containing two or more different additives of the same subgroup in C08K
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provides are a thick-electrode cathode sheet, a preparation method therefor and a primary battery. The method includes: first, mixing a cathode active material, a conductive agent, and a binder resin to obtain a mixed material; and subjecting the mixed material to fibrillation treatment to obtain a fibrillized mixed material; then subjecting the fibrillized mixed material and a granulating agent to granulation treatment to obtain a precursor material; and finally, subjecting the precursor material to rolling and film-formation treatment to obtain the thick-electrode cathode sheet.

## Claims

### Claim 1

A preparation method for a thick-electrode cathode sheet, comprises the following steps:
S1: mixing a cathode active material, a conductive agent, and a binder resin to obtain a mixed material;
S2: subjecting the mixed material to fibrillation treatment to obtain a fibrillized mixed material;
S3: subjecting the fibrillized mixed material and a granulating agent to granulation treatment to obtain a precursor material; wherein the granulating agent is a liquid with a vapor pressure of more than or equal to 0.2 mmHg; and
S4: subjecting the precursor material to rolling and film-formation treatment to obtain the thick-electrode cathode sheet.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the cathode active material in step S1 comprises any one or a combination of two of manganese dioxide and acetylene black.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the binder resin in step S1 comprises polytetrafluoroethylene.

### Claim 4 (depends on 1)

The method according to claim 1, wherein, in a case where the cathode active material in step S1 is manganese dioxide, based on a total mass of the mixed material as 100%, a mass percentage content of the binder resin in step S1 is 1 wt. %-5 wt. %, and optionally 1.5 wt. %-2.5 wt. %.

### Claim 5 (depends on 1)

The method according to claim 1, wherein, in a case where the cathode active material in step S1 is acetylene black, based on the total mass of the mixed material as 100%, a mass percentage content of the binder resin in step S1 is 5 wt. %-15 wt. %, and optionally 6 wt. %-8 wt. %.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the mixing in step S1 is performed in a manner of gravity-free mixing;
optionally, the mixing in step S1 is performed at a temperature lower than 19° C.

### Claim 7 (depends on 1)

The method according to claim 1, wherein equipment for the fibrillation treatment in step S2 comprises any one or a combination of two of a high-speed mixer and a jet mill;
optionally, a linear velocity of the high-speed mixer is 50-150 m/s;
optionally, an air pressure of the jet mill is 0.75-0.85 MPa.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the granulating agent in step S3 comprises any one or a combination of at least two of N-methylpyrrolidone, dimethyl silicone oil, polyethylene glycol, propylene glycol, isoparaffin, mineral oil, or pure water;
optionally, in a case where the cathode active material is manganese dioxide, based on a total mass of the material for the granulation treatment as 100%, a mass percentage content of the granulating agent in step S3 is 10 wt. %-30 wt. %, and optionally 15 wt. %-25 wt. %;
optionally, in a case where the cathode active material is acetylene black, based on the total mass of the material for the granulation treatment as 100%, a mass percentage content of the granulating agent in step S3 is 30 wt. %-70 wt. %, and optionally 50 wt. %-60 wt. %.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the rolling and film-formation in step S4 is performed in a manner comprising any one or a combination of two of differential-temperature film formation and differential-speed film formation, and optionally differential-temperature film formation.

### Claim 10 (depends on 9)

The method according to claim 9, wherein equipment for differential-temperature film formation comprises a differential-temperature film formation roller system.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the differential-temperature film formation roller system comprises a first pressing roller, a second pressing roller, a third pressing roller, and a fourth pressing roller arranged in sequence; wherein a first feeding inlet is formed above the position between the first pressing roller and the second pressing roller, a second feeding inlet is formed above the position between the third pressing roller and the fourth pressing roller, and the second pressing roller and the third pressing roller can press powder placed in the first feeding inlet and the second feeding inlet into a continuous film;
optionally, a rolling direction of the first pressing roller and the third pressing roller is opposite to a rolling direction of the second pressing roller and the fourth pressing roller;
optionally, a temperature of the first pressing roller and the fourth pressing roller is higher than a temperature of the second pressing roller and the third pressing roller;
optionally, a temperature of both the first pressing roller and the fourth pressing roller is 50° C.-105° C.;
optionally, a temperature of both the second pressing roller and the third pressing roller is 20° C.-60° C.;
optionally, a temperature difference between the first pressing roller and the second pressing roller is 10° C.-90° C., and optionally 30° C.-50° C.;
optionally, a temperature difference between the fourth pressing roller and the third pressing roller is 10° C.-90° C., and optionally 30° C.-50° C.

### Claim 12 (depends on 9)

The method according to claim 9, wherein the differential-speed film formation is performed at a rolling temperature of 40° C.-110° C.;
optionally, equipment for the differential-speed film formation comprises a differential-speed film formation roller system;
optionally, the differential-speed film formation roller system comprises a I-pressing roller, a II-pressing roller, a III-pressing roller, and a IV-pressing roller arranged in sequence; a first feeding inlet is formed above the position between the I-pressing roller and the II-pressing roller, a second feeding inlet is formed above the position between the III-pressing roller and the IV-pressing roller, and the II-pressing roller and the III-pressing roller can press powder placed in the first feeding inlet and the second feeding inlet into a continuous film;
optionally, a gap between adjacent rollers in the differential-speed film formation roller system is 0.10-0.60 mm.

### Claim 13 (depends on 12)

The method according to claim 12, wherein a rolling direction of the I-pressing roller and the III-pressing roller is opposite to a rolling direction of the II-pressing roller and the IV-pressing roller;
optionally, a linear velocity of the I-pressing roller and the IV-pressing roller is smaller than a linear velocity of the II-pressing roller and the III-pressing roller;
optionally, a linear velocity of the I-pressing roller is the same as a linear velocity of the IV-pressing roller;
optionally, a linear velocity of the II-pressing roller is the same as a linear velocity of the III-pressing roller;
optionally, a ratio of the linear velocity of any one or a combination of two of the I-pressing roller and the IV-pressing roller to the linear velocity of any one or a combination of two of the II-pressing roller and the III-pressing roller is 1:(1.1-2).

### Claim 14 (depends on 1)

A thick-electrode cathode sheet, wherein the thick-electrode cathode sheet is prepared by the preparation method for a thick-electrode cathode sheet according to claim 1.

### Claim 15 (depends on 14)

A primary battery, comprising a cathode sheet, an anode sheet, an electrolyte, and a separator, and the cathode sheet comprises the thick-electrode cathode sheet according to claim 14.
