# US 2026/0186416 A1 · Method for manufacturing cured film and use of the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0186416 A1
- Document ID: US20260186416A1
- Status: Published application
- Kind: A1
- Application number: 19/549,434
- Filed: 2026-02-25
- Published: 2026-07-02
- Earliest claimed: 2019-04-26
- Assignees: Merck Patent GmbH
- Applicants: Merck Patent GmbH
- Inventors: Takashi SEKITO; Shigemasa NAKASUGI; Hiroshi YANAGITA; Taku HIRAYAMA
- Web page: https://patentgrep.com/patent/US20260186416A1

## CPC

- G03F 7/091: {characterised by antireflection means or light filtering or absorbing means, e.g. anti-halation, contrast enhancement}
- G03F 7/11: having cover layers or intermediate layers, e.g. subbing layers {(G03F7/091 - G03F7/093, B41N3/03 take precedence)}
- C08G 61/10: only aromatic carbon atoms, e.g. polyphenylenes
- C09D 165/00: Coating compositions based on macromolecular compounds obtained by reactions forming a carbon-to-carbon link in the main chain (C09D107/00 - C09D157/00, C09D161/00 take precedence); Coating compositions based on derivatives of such polymers
- G03F 7/025: Non-macromolecular photopolymerisable compounds having carbon-to-carbon triple bonds, e.g. acetylenic compounds (G03F7/075 takes precedence)
- G03F 7/027: Non-macromolecular photopolymerisable compounds having carbon-to-carbon double bonds, e.g. ethylenic compounds (G03F7/075 takes precedence)
- G03F 7/0388: {with ethylenic or acetylenic bands in the side chains of the photopolymer}
- G03F 7/094: {Multilayer resist systems, e.g. planarising layers}
- C08G 2261/124: alternating
- C08G 2261/1424: containing ether groups, including alkoxy
- C08G 2261/18: conjugated
- C08G 2261/228: Polymers, i.e. more than 10 repeat units
- C08G 2261/312: Non-condensed aromatic systems, e.g. benzene
- C08G 2261/3142: fluorene-based, e.g. fluorene, indenofluorene, or spirobifluorene
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

[Problem] To provide a method for manufacturing a cured film having high film density, high film hardness and high etching resistance. [Means for Solution] A method for manufacturing a cured film comprising (1) applying a composition (i) above a substrate; (2) forming a hydrocarbon-containing film from the composition (i); and (3) irradiating the hydrocarbon-containing film with plasma, electron beam and/or ion to form a cured film. Use of the cured film.

## Claims

### Claim 1

A method for manufacturing a cured film comprising the following processes:
(1) applying a composition (i) above a substrate;
(2) forming a hydrocarbon-containing film from the composition (i); and
(3) irradiating the hydrocarbon-containing film with plasma, electron beam and/or ion to form a cured film,
provided that the composition (i) comprises a hydrocarbon-containing compound (A) and a solvent (B); and
the hydrocarbon-containing compound (A) comprises a structural unit (A1) represented by the following formula (A1):
wherein,
Ar11 is a C6-60 hydrocarbon group substituted with R11 or unsubstituted (provided that Ar11 contains no fused aromatic ring);
R11 is a linear, branched or cyclic C1-20 alkyl, amino or alkylamino;
R12 is I, Br or CN;
p11 is a number of 0 to 5, p12 is a number of 0 to 1, q11 is a number of 0 to 5, q12 is a number of 0 to 1, r11 is 0, s11 is a number of 0 to 5; and
p11, q11 and r11 do not become 0 simultaneously in one structural unit.

### Claim 2 (depends on 1)

The method for manufacturing a cured film according to claim 1, wherein the formula (A1) is the following formulae (A1-1), (A1-2), and/or (A1-3):
wherein,
Ar21 is a C6-50 aromatic hydrocarbon group;
R21, R22 and R23 are each independently a C6-50 aromatic hydrocarbon group, hydrogen, or a single bond bonded to another structural unit;
n21 is an integer of 0 or 1;
where, Ar21, R21, R22 and R23 contain no fused aromatic ring; and
the definitions of R12, p11, p12, q11, q12, r11 and s11 are each independently the same as the above,
wherein,
L31 and L32 are each independently a single bond or phenylene;
n31, n32, m31 and m32 are each independently a number of 0 to 6; and
where, the definitions of R12, p11, p12, q11, q12, r11 and s11 are each independently the same as the above,
wherein,
Ar41 is a C6-50 aromatic hydrocarbon group;
R41 and R42 are each independently a C1-10 alkyl, and R41 and R42 can form a hydrocarbon ring;
the carbon atom at the position of *41 is a quaternary carbon atom;
L41 is a C6-50 arylene or a single bond bonded to another structural unit;
where, the definitions of R12, p11, p12, q11, q12, r11 and s11 are each independently the same as the above; and
preferably, the molecular weight of the hydrocarbon-containing compound (A) is 500 to 6,000.

### Claim 3 (depends on 1)

The method for manufacturing a cured film according to claim 1, wherein the composition (i) further comprises a surfactant (C);
preferably, the composition (i) further comprises an additive (D); and/or
preferably, the additive (D) comprises a crosslinking agent, a high carbon material, an acid generator, a radical generator, a photopolymerization initiator, a substrate adhesion enhancer, or a mixture of any of these.

### Claim 4 (depends on 1)

The method for manufacturing a cured film according to claim 1, wherein the solvent (B) comprises an organic solvent; and
preferably, the organic solvent comprises a hydrocarbon solvent, an ether solvent, an ester solvent, an alcohol solvent, a ketone solvent, or a mixture of any of these.

### Claim 5 (depends on 1)

The method for manufacturing a cured film according to claim 1, wherein
the content of the hydrocarbon-containing compound (A) is 2 to 30 mass % based on the composition (i);
the content of the solvent (B) is 60 to 98 mass % based on the composition (i);
preferably, the content of the surfactant (C) is 0.01 to 10 mass % based on the hydrocarbon-containing compound (A); and/or
preferably, the content of the additive (D) is 0.05 to 100 mass % based on the hydrocarbon-containing compound (A).

### Claim 6 (depends on 1)

The method for manufacturing a cured film according to claim 1, wherein
the hydrocarbon-containing compound (A) is polymer, and an aldehyde derivative used when the polymer is synthesized is 0 to 30 mol % based on the sum of all elements used in the synthesis; and
preferably, the polymer essentially does not contain secondary or tertiary carbon atoms in its main chain.

### Claim 7 (depends on 1)

The method for manufacturing a cured film according to claim 1, wherein the process (3) comprises the following conditions:
in the case of plasma irradiation:
the atmosphere is N2, NF3, H2, fluorocarbon, rare gas, or a mixture of any of these; and/or
the RF discharge power is 1,000 to 10,000 W,
in the case of electron beam irradiation:
the acceleration voltage is 2 to 200 kV, and/or
the irradiation amount is 100 to 5,000 kGy,
in the case of ion irradiation:
the elemental species of the ion to be irradiated is hydrogen, boron, carbon, nitrogen, rare gas, or a mixture of any of these;
the acceleration voltage is 3 to 1000 kV; and/or
the irradiation amount is 1013 to 1018 ion/cm2.

### Claim 8 (depends on 1)

The method for manufacturing a cured film according to claim 1, wherein
in the cured film formed in the process (3), the film density is increased by 5 to 75% and/or the film hardness is increased by 50 to 500%, as compared with the hydrocarbon-containing film formed in the process (2);
preferably, the intensity ratio of G band and D band R=ID/IG in Raman spectroscopy (measured with laser wavelength of 514.5 nm) of the cured film formed in the process (3) is 0.35 to 0.90;
preferably, the hydrocarbon-containing film formed in the process (2) is more easily etched by 5 to 200% than the cured film formed in the process (3); and/or
preferably, the surface resistivity of the cured film formed in the process (3) is 109 to 1016Ω.

### Claim 9 (depends on 1)

The method for manufacturing a cured film according to claim 1, wherein the process (2) for forming a hydrocarbon-containing film from the composition (i) comprises at least either of the following conditions:
heating at 80 to 800° C. for 30 to 180 seconds; and
irradiating ultraviolet light of 10 to 380 nm.

### Claim 10 (depends on 1)

The method for manufacturing a cured film according to claim 1, wherein
the film density of the carbon-containing cured film is 1.3 to 3.2 g/cm3; and/or
the film hardness of the carbon-containing cured film is 1.5 to 20 GPa.

### Claim 11 (depends on 1)

A method for manufacturing a resist layer above the cured film according to claim 1.

### Claim 12 (depends on 11)

A method for manufacturing a resist pattern by exposing and developing the resist layer according to claim 11.

### Claim 13 (depends on 1)

A method for manufacturing a device comprising the method according to claim 1.