# US 2026/0184913 A1 · Cycloolefin resin composition, resin material, preparation method therefor, and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0184913 A1
- Document ID: US20260184913A1
- Status: Published application
- Kind: A1
- Application number: 19/426,118
- Filed: 2025-12-19
- Published: 2026-07-02
- Earliest claimed: 2024-12-31
- Assignees: Shanghai Sinochem Science & Technology Co., Ltd
- Applicants: Shanghai Sinochem Science & Technology Co., Ltd
- Inventors: Xianfeng YANG; Tao Tong; Jiaxing Fang; Yingying Mi
- Web page: https://patentgrep.com/patent/US20260184913A1

## CPC

- B01J 31/2278: {Complexes comprising two carbene ligands differing from each other, e.g. Grubbs second generation catalysts}
- C08L 65/00: Compositions of macromolecular compounds obtained by reactions forming a carbon-to-carbon link in the main chain (C08L7/00 - C08L57/00, C08L61/00 take precedence); Compositions of derivatives of such polymers
- B01J 31/24: Phosphines {, i.e. phosphorus bonded to only carbon atoms, or to both carbon and hydrogen atoms, including e.g. sp2-hybridised phosphorus compounds such as phosphabenzene, phosphole or anionic phospholide ligands}
- C08F 234/00: Copolymers of cyclic compounds having no unsaturated aliphatic radicals in a side chain and having one or more carbon-to-carbon double bonds in a heterocyclic ring (cyclic esters of polyfunctional acids C08F218/00; cyclic anhydrides or imides C08F222/00)
- C08G 61/08: of carbocyclic compounds containing one or more carbon-to-carbon double bonds in the ring
- C08J 5/244: {using glass fibres}
- C08L 45/00: Compositions of homopolymers or copolymers of compounds having no unsaturated aliphatic radicals in side chain, and having one or more carbon-to-carbon double bonds in a carbocyclic or in a heterocyclic ring system; Compositions of derivatives of such polymers (of cyclic anhydrides or imides C08L35/00; of cyclic esters of polyfunctional acids C08L31/00)
- C09D 165/00: Coating compositions based on macromolecular compounds obtained by reactions forming a carbon-to-carbon link in the main chain (C09D107/00 - C09D157/00, C09D161/00 take precedence); Coating compositions based on derivatives of such polymers
- H05K 1/0366: {reinforced, e.g. by fibres, fabrics (H05K1/036 takes precedence)}
- B01J 2231/543: alkene metathesis
- B01J 2531/821: Ruthenium
- C08G 2261/11: Homopolymers
- C08G 2261/122: statistical
- C08G 2261/332: containing only carbon atoms
- C08G 2261/3325: derived from other polycyclic systems
- C08G 2261/418: Ring opening metathesis polymerisation [ROMP]
- C08J 2365/00: Characterised by the use of macromolecular compounds obtained by reactions forming a carbon-to-carbon link in the main chain (C08J2307/00 - C08J2357/00, C08J2361/00 take precedence); Derivatives of such polymers
- C08L 2203/20: use in electrical or conductive gadgets
- C08L 2205/035: containing four or more polymers in a blend
- C08L 2207/322: Liquid component is processing oil
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

The present disclosure discloses a cycloolefin resin composition, a resin material, a preparation method therefor, and a use thereof. Specifically, the present disclosure discloses a use of a cycloolefin resin composition M1 in the preparation of a substrate material for a high-frequency and high-speed information transmission device, wherein the cycloolefin resin composition M1 comprises component A and component B, wherein the component A is cycloolefin, the component B is a ruthenium alkylidene compound of Formula I and/or Formula II or a salt thereof, and the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:(7500-60000). The resin material prepared using the cycloolefin resin composition of the present disclosure exhibits low dielectric loss and low dielectric constant under high-frequency conditions, along with good heat resistance.

## Claims

### Claim 1

A method for preparing a substrate material for a high-frequency and high-speed information transmission device, comprising the following steps: subjecting a cycloolefin resin composition M1 to a liquid molding process to obtain the substrate material for the high-frequency and high-speed information transmission device, wherein the cycloolefin resin composition M1 comprises component A and component B, wherein the component A is cycloolefin, the component B is a ruthenium alkylidene compound of Formula I and/or Formula II or a salt thereof, and the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:(7500-60000),
wherein
R11 and R12 are each independently C4-C18 alkyl or C4-C18 alkyl substituted by R1-1;
R1-1 is C6-C10 aryl;
R21, R22, and R23 are each independently C6-C18 alkyl.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the method satisfies one or more of the following conditions:
(1) the substrate material for the high-frequency and high-speed information transmission device has a dielectric loss of <0.001 at a frequency of ≥1 GHz;
(2) the substrate material for the high-frequency and high-speed information transmission device has a dielectric constant of <2.5 at a frequency of ≥1 GHz;
(3) the substrate material for the high-frequency and high-speed information transmission device has a glass transition temperature of ≥135° C.;
(4) the substrate material for the high-frequency and high-speed information transmission device has a heat deflection temperature of ≥110° C.;
(5) in the cycloolefin resin composition M1, the mass percentage of the component A is 80% or more, but less than 100%;
(6) the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:(7500-50000);
(7) the component A is a single type of cycloolefin or a mixture of multiple cycloolefins; the cycloolefin contains only C and H elements and may be substituted by one or more RA, wherein each RA is independently F, C1-C18 alkyl, C2-C18 alkenyl, C6-C10 aryl, alkoxy with a carbon chain length of C2-C18, —C(═O)OC2-C18, or —OC(═O)C2-C18;
(8) in the ruthenium alkylidene compound of Formula I, in R11 and R12, the C4-C18 alkyl and the C4-C18 alkyl in the C4-C18 alkyl substituted by R1-1 are each independently C4-C18 linear alkyl;
(9) in the ruthenium alkylidene compound of Formula I, in R1-1, the C6-C10 aryl is phenyl or naphthyl;
(10) in the ruthenium alkylidene compound of Formula II, in R21, R22, and R23, each C6-C18 alkyl is independently C6-C10 alkyl;
(11) the liquid molding process is a reaction injection molding process, a resin transfer molding process, or a vacuum-assisted resin infusion process;
(12) in the liquid molding process, the temperature for curing and molding is 40-145° C.;
(13) in the liquid molding process, the time for curing and molding may be 1-120 min.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the method satisfies any one of the following conditions:
(1) the component A is a single type of cycloolefin or a mixture of multiple cycloolefins, the component A at least comprises cycloolefin S1, the cycloolefin S1 contains only C and H elements and comprises the following structural moieties:
wherein the structural moieties are connected to other parts of the molecule via a carbon atom marked with “*”; the cycloolefin S1 may be substituted by one or more RA, wherein each RA is independently F, C1-C18 alkyl, C2-C18 alkenyl, C6-C10 aryl, C2-C18 alkoxy, —C(═O)OC2-C18, or —OC(═O)C2-C18;
(2) the component A is one or more selected from tetracyclododecene, cyclopentadiene polymer, 5-ethylidene-2-norbornene, cyclohexene, cycloheptene, cyclooctene, and cycloolefin having a structure of Formula A-1
wherein in Formula A-1, m is 0, 1, or 2, and RA1, RA2, RA3, and RA4 are each independently H, F, C1-C18 alkyl, C2-C18 alkenyl, C6-C10 aryl, C2-C18 alkoxy, —C(═O)OC2-C18, or —OC(═O)C2-C18;
(3) the ruthenium alkylidene compound of Formula II is one or more selected from the following compounds:
(4) the ruthenium alkylidene compound of Formula II is

### Claim 4 (depends on 1)

The method according to claim 1, wherein the method satisfies any one of the following conditions:
(1) the component A is tetracyclododecene;
(2) the component A is dihydrodicyclopentadiene;
(3) in the component A, the mass percentage of dicyclopentadiene is 70% to 100%;
(4) in the component A, the mass percentage of tricyclopentadiene is 0% to 30%;
(5) in the ruthenium alkylidene compound of Formula I, R11 and R12 are each independently C4-C18 alkyl or C4-C18 alkyl substituted by one phenyl group;
(6) the ruthenium alkylidene compound of Formula I is one or more selected from the following compounds:
(7) the ruthenium alkylidene compound of Formula I is

### Claim 5 (depends on 1)

The method according to claim 1, wherein the method satisfies any one of the following conditions:
(1) the component A comprises 70% to 100% by mass of dicyclopentadiene and 0% to 30% by mass of tricyclopentadiene;
(2) the component A consists of the following components: 85% to 95% by mass of dicyclopentadiene and 5% to 15% by mass of tricyclopentadiene;
(3) the component A consists of the following components: 90% to 100% by mass of dicyclopentadiene and 0% to 10% by mass of 5-ethylidene-2-norbornene;
(4) the component A consists of the following components: 70% to 90% by mass of dicyclopentadiene, 10% to 30% by mass of tricyclopentadiene, and 0% to 5% by mass of tetracyclopentadiene;
(5) the component A consists of the following components: 70% to 90% by mass of dicyclopentadiene, 10% to 20% by mass of tricyclopentadiene, 0% to 10% by mass of dihydrodicyclopentadiene, and 0% to 5% by mass of cyclohexene;
(6) the component A consists of 90% by mass of dicyclopentadiene and 10% by mass of tricyclopentadiene;
(7) the component A consists of 98% by mass of dicyclopentadiene and 2% by mass of 5-ethylidene-2-norbornene;
(8) the component A consists of 79% by mass of dicyclopentadiene, 20% by mass of tricyclopentadiene, and 1% by mass of tetracyclopentadiene;
(9) the component A consists of 80% by mass of dicyclopentadiene, 15% by mass of tricyclopentadiene, 4.5% by mass of dihydrodicyclopentadiene, and 0.5% by mass of cyclohexene;
(10) the substrate material for the high-frequency and high-speed information transmission device is a copper-clad laminate;
(11) the component B is a ruthenium alkylidene compound of Formula I;
(12) the component B is a ruthenium alkylidene compound of Formula II;
(13) the component B consists of a ruthenium alkylidene compound of Formula I and a ruthenium alkylidene compound of Formula II;
(14) the component B consists of a ruthenium alkylidene compound of Formula I and a ruthenium alkylidene compound of Formula II, wherein the molar ratio of the ruthenium alkylidene compound of Formula I to the ruthenium alkylidene compound of Formula II is 1:(1.5-5).

### Claim 6 (depends on 1)

The method according to claim 1, wherein the cycloolefin resin composition M1 further comprises component C and/or component D, wherein,
the component C is one or more selected from solid paraffin, liquid paraffin, and chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %;
the component D is one or more selected from thermoplastic resin, linear or branched chain olefin with a carbon chain length of C12 or more, linear or branched chain alkane with a carbon chain length of C12 or more, solid paraffin, and mineral oil; and the thermoplastic resin, chain olefin, and chain alkane contain only C and H elements.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the method satisfies any one of the following conditions:
(1) the component C is liquid paraffin, chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %, or a mixture of liquid paraffin and chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %;
(2) the component C is a mixture of liquid paraffin and chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %, wherein in the mixture, the mass ratio of the liquid paraffin to the chlorinated paraffin with a chlorine content of 5 wt % to 65 wt % is (10-20): 1;
(3) when the cycloolefin resin composition MI comprises component C, the ratio of the total mass of the component C and the component B to the mass of the component A is 1:(15-200);
(4) the component C is liquid paraffin and/or chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %, and the mass ratio of the component C to the component B is (15-70): 1;
(5) the component C is liquid paraffin, and the mass ratio of the component C to the component B is (60-70): 1;
(6) the component C is chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %, and the mass ratio of the component C to the component B is (15-35): 1;
(7) the chlorinated paraffin with a chlorine content of 5 wt % to 65 wt % is chlorinated paraffin with a chlorine content of 5 wt % to 52 wt %;
(8) the thermoplastic resin is one or more selected from ethylene-propylene rubber (EP), ethylene-propylene-diene monomer rubber (EPDM), polyolefin elastomer (POE), liquid butyl rubber (LBR), styrene-butadiene rubber (SBR), hydrogenated styrene-butadiene rubber (SEBS), and styrene-butadiene-styrene block copolymer (SBS);
(9) the thermoplastic resin is added with an additive, wherein the additive is an organic phosphorus compound and/or an antioxidant;
(10) the thermoplastic resin is added with an additive, wherein the additive is an organic phosphorus compound and/or an antioxidant, and based on the total mass of component A and component D, the mass percentage of the additive is 0-0.5 wt %;
(11) the linear or branched chain alkane with a carbon chain length of C12 or more is n-pentadecane;
(12) when the cycloolefin resin composition MI comprises component D, based on the total mass of component A and component D, the mass percentage of the component D is 0-20 wt %.

### Claim 8 (depends on 1)

The method according to claim 1, wherein
the cycloolefin resin composition M1 is any one of the following schemes:
scheme (1) the cycloolefin resin composition M1 consists of the component A and the component B;
scheme (2) the cycloolefin resin composition M1 consists of the component A, the component B and component C, wherein the component C is one or more selected from solid paraffin, liquid paraffin, and chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %;
scheme (3) the cycloolefin resin composition M1 consists of the component A, the component B and component D, wherein the component D is one or more selected from thermoplastic resin, linear or branched chain olefin with a carbon chain length of C12 or more, linear or branched chain alkane with a carbon chain length of C12 or more, solid paraffin, and mineral oil; and the thermoplastic resin, chain olefin, and chain alkane contain only C and H elements;
scheme (4) the cycloolefin resin composition M1 consists of the component A, the component B, component C and component D, wherein the component C is one or more selected from solid paraffin, liquid paraffin, and chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %, and the component D is one or more selected from thermoplastic resin, linear or branched chain olefin with a carbon chain length of C12 or more, linear or branched chain alkane with a carbon chain length of C12 or more, solid paraffin, and mineral oil; and the thermoplastic resin, chain olefin, and chain alkane contain only C and H elements;
scheme (5) the cycloolefin resin composition M1 consists of component A and component B,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
scheme (6) the cycloolefin resin composition M1 consists of component A and component B,
the component A is tetracyclododecene;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:15000;
scheme (7) the cycloolefin resin composition M1 consists of component A and component B,
the component A is dihydrodicyclopentadiene;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:15000;
scheme (8) the cycloolefin resin composition M1 consists of component A, component B, and component C,
the component A consists of dicyclopentadiene and 5-ethylidene-2-norbornene, wherein the mass percentage of dicyclopentadiene in the component A is 98%, and the mass percentage of 5-ethylidene-2-norbornene in the component A is 2%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
the component C is liquid paraffin;
the ratio of the total mass of the component C and the component B to the mass of the component A is 1:20;
scheme (9) the cycloolefin resin composition M1 consists of component A, component B, and component C,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
the component C is chlorinated paraffin with a chlorine content of 5%;
the ratio of the total mass of the component C and the component B to the mass of the component A is 1:50;
scheme (10) the cycloolefin resin composition M1 consists of component A, component B, and component C,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
the component C is chlorinated paraffin with a chlorine content of 5%;
the ratio of the total mass of the component C and the component B to the mass of the component A is 1:50;
scheme (11) the cycloolefin resin composition M1 consists of component A and component B,
the component A consists of dicyclopentadiene, tricyclopentadiene, and tetracyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 79%, the mass percentage of tricyclopentadiene in the component A is 20%, and the mass percentage of tetracyclopentadiene in the component A is 1%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
scheme (12) the cycloolefin resin composition M1 consists of component A, component B, and component C,
the component A consists of dicyclopentadiene, tricyclopentadiene, and tetracyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 79%, the mass percentage of tricyclopentadiene in the component A is 20%, and the mass percentage of tetracyclopentadiene in the component A is 1%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
the component C is liquid paraffin;
the ratio of the total mass of the component C and the component B to the mass of the component A is 1:200;
scheme (13) the cycloolefin resin composition M1 consists of component A and component B,
the component A consists of dicyclopentadiene, tricyclopentadiene, and tetracyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 79%, the mass percentage of tricyclopentadiene in the component A is 20%, and the mass percentage of tetracyclopentadiene in the component A is 1%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
scheme (14) the cycloolefin resin composition M1 consists of component A and component B,
the component A consists of dicyclopentadiene, tricyclopentadiene, and tetracyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 79%, the mass percentage of tricyclopentadiene in the component A is 20%, and the mass percentage of tetracyclopentadiene in the component A is 1%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:50000;
scheme (15) the cycloolefin resin composition M1 consists of component A, component B, and component C,
the component A consists of dicyclopentadiene, tricyclopentadiene, dihydrodicyclopentadiene, and cyclohexene, wherein the mass percentage of dicyclopentadiene in the component A is 80%, the mass percentage of tricyclopentadiene in the component A is 15%, the mass percentage of dihydrodicyclopentadiene in the component A is 4.5%, and the mass percentage of cyclohexene in the component A is 0.5%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:9500;
the component C consists of liquid paraffin and chlorinated paraffin with a chlorine content of 52 wt %, wherein the mass ratio of liquid paraffin to chlorinated paraffin with a chlorine content of 52 wt % is 11:1;
the ratio of the total mass of the component C and the component B to the mass of the component A is 1:20;
scheme (16) the cycloolefin resin composition M1 consists of component A and component B,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B consists of
wherein the molar ratio of
is 1:2;
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
scheme (17) the cycloolefin resin composition M1 consists of component A and component B,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:7500;
scheme (18) the cycloolefin resin composition M1 consists of component A, component B, and component D,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
the component D is a mixture of n-pentadecane, EPDM, SBS, and mineral oil;
based on the total mass of the component A and the component D, in the component D, the mass percentage of n-pentadecane is 4-5%, and the mass percentages of EPDM, SBS, and mineral oil are independently 2-3%;
scheme (19) the cycloolefin resin composition M1 consists of component A, component B, and component D,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
the component D is a mixture of n-pentadecane, cetene, EPDM, SEBS, POE, and mineral oil;
based on the total mass of the component A and the component D, the mass percentage of n-pentadecane is 2-4%, the mass percentage of cetene is 0.3-1%, the mass percentage of EPDM is 2-3%, the mass percentage of SEBS is 0.3-1%, the mass percentage of POE is 0.5-1.2%, and the mass percentage of mineral oil is independently 2-3%;
scheme (20) the cycloolefin resin composition M1 consists of component A, component B, and component D,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the component D is a mixture of an antioxidant 264, triphenylphosphine, n-pentadecane, EPDM, SEBS, and POE;
based on the total mass of the component A and the component D, the mass percentage of the antioxidant 264 is 0.1-0.2%, the mass percentage of triphenylphosphine is 0.02-0.1%, the mass percentage of n-pentadecane is 4-5%, the mass percentage of EPDM is 1-2%, the mass percentage of SEBS is 1-2%, and the mass percentage of POE is 1-2%.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the method satisfies any one of the following conditions:
(1) the liquid molding process is a resin transfer molding process, comprising the following steps: adding a mixture of each component in the cycloolefin resin composition into a mold, curing and molding;
(2) the liquid molding process is a reaction injection molding process, comprising the following steps: adding a mixture of each component in the cycloolefin resin composition into a mold, curing and molding, wherein the cycloolefin resin composition consists of the component A, the component B and component C, wherein the component C is one or more selected from solid paraffin, liquid paraffin, and chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %;
(3) the liquid molding process is a reaction injection molding process, comprising the following steps: adding a mixture of each component in the cycloolefin resin composition into a mold, curing and molding, wherein the mixture of each component in the cycloolefin resin composition is obtained by mixing each component of the cycloolefin resin composition at 1-3 MPa, wherein the cycloolefin resin composition consists of the component A, the component B and component C, wherein the component C is one or more selected from solid paraffin, liquid paraffin, and chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %;
(4) the liquid molding process is a reaction injection molding process, comprising the following steps: adding a mixture of each component in the cycloolefin resin composition into a mold, curing and molding, wherein the mixture of each component in the cycloolefin resin composition is added into the mold within 4-6 s, wherein the cycloolefin resin composition consists of the component A, the component B and component C, wherein the component C is one or more selected from solid paraffin, liquid paraffin, and chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %;
(5) the liquid molding process is a vacuum-assisted resin infusion process, comprising the following steps: adding a mixture of each component in the cycloolefin resin composition into a mold, curing and molding.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the method satisfies any one of the following conditions:
(1) in the reaction injection molding process, the resin transfer molding process, or the vacuum-assisted resin infusion process, the mixture is a mixture of component A in each resin composition and other components in each resin composition;
(2) in the reaction injection molding process, the resin transfer molding process, or the vacuum-assisted resin infusion process, the mixture is a mixture of component A in each resin composition and other components in each resin composition, wherein the component A is treated as follows: stirring at 60° C.-125° C. for 4-12 hours, and cooling to room temperature for later use;
(3) in the reaction injection molding process, the resin transfer molding process, or the vacuum-assisted resin infusion process, the temperature of the mold is 40-145° C.;
(4) in the reaction injection molding process or the resin transfer molding process, the temperature on one side of the mold is 60-140° C.; the temperature on the other side of the mold is 40-140° C.;
(5) the reaction injection molding process, the resin transfer molding process, or the vacuum-assisted resin infusion process further comprises a post-curing stage, wherein the temperature during the post-curing is 60-145° C., and the time for the post-curing is 0-60 min.

### Claim 11

A cycloolefin resin composition, wherein the cycloolefin resin composition is a cycloolefin resin composition M1, a cycloolefin resin composition M2, a cycloolefin resin composition M3, a cycloolefin resin composition M4, or a cycloolefin resin composition M5 as follows:
cycloolefin resin composition M1: comprising component A and component B, and the mass percentage of the component A is 80% or more, but less than 100%;
cycloolefin resin composition M2: consisting of component A and component B;
cycloolefin resin composition M3: consisting of component A, component B and component C, wherein the component C is one or more selected from solid paraffin, liquid paraffin, and chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %;
cycloolefin resin composition M4: consisting of component A, component B and component D, wherein the component D is one or more selected from thermoplastic resin, linear or branched chain olefin with a carbon chain length of C12 or more, linear or branched chain alkane with a carbon chain length of C12 or more, solid paraffin, and mineral oil; and the thermoplastic resin, chain olefin, and chain alkane contain only C and H elements;
cycloolefin resin composition M5: consisting of component A, component B, component C and component D, wherein the component C is one or more selected from solid paraffin, liquid paraffin, and chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %, and the component D is one or more selected from thermoplastic resin, linear or branched chain olefin with a carbon chain length of C12 or more, linear or branched chain alkane with a carbon chain length of C12 or more, solid paraffin, and mineral oil; and the thermoplastic resin, chain olefin, and chain alkane contain only C and H elements;
and in cycloolefin resin composition M1-M5, the component A is cycloolefin, the component B is a ruthenium alkylidene compound of Formula I and/or Formula II or a salt thereof, and the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:(7500-60000),
wherein
R11 and R12 are each independently C4-C18 alkyl or C4-C18 alkyl substituted by R1-1;
R1-1 is C6-C10 aryl;
R21, R22, and R23 are each independently C6-C18 alkyl.

### Claim 12 (depends on 11)

The cycloolefin resin composition according to claim 11, wherein the cycloolefin resin composition satisfies any one of the following conditions:
(1) the component C is liquid paraffin, chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %, or a mixture of liquid paraffin and chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %;
(2) the component C is a mixture of liquid paraffin and chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %, wherein in the mixture, the mass ratio of the liquid paraffin to the chlorinated paraffin with a chlorine content of 5 wt % to 65 wt % is (10-20): 1;
(3) when the cycloolefin resin composition comprises component C, the ratio of the total mass of the component C and the component B to the mass of the component A is 1:(15-200);
(4) the component C is liquid paraffin and/or chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %, and the mass ratio of the component C to the component B is (15-70): 1;
(5) the component C is liquid paraffin, and the mass ratio of the component C to the component B is (60-70): 1;
(6) the component C is chlorinated paraffin with a chlorine content of 5 wt % to 65 wt %, and the mass ratio of the component C to the component B is (15-35): 1;
(7) the chlorinated paraffin with a chlorine content of 5 wt % to 65 wt % is chlorinated paraffin with a chlorine content of 5 wt % to 52 wt %;
(8) the thermoplastic resin is one or more selected from ethylene-propylene rubber (EP), ethylene-propylene-diene monomer rubber (EPDM), polyolefin elastomer (POE), liquid butyl rubber (LBR), styrene-butadiene rubber (SBR), hydrogenated styrene-butadiene rubber (SEBS), and styrene-butadiene-styrene block copolymer (SBS);
(9) the thermoplastic resin is added with an additive, wherein the additive is an organic phosphorus compound and/or an antioxidant;
(10) the thermoplastic resin is added with an additive, wherein the additive is an organic phosphorus compound and/or an antioxidant, and based on the total mass of component A and component D, the mass percentage of the additive is 0-0.5 wt %;
(11) the linear or branched chain alkane with a carbon chain length of C12 or more is n-pentadecane;
(12) when the cycloolefin resin composition comprises component D, based on the total mass of component A and component D, the mass percentage of the component D is 0-20 wt %.

### Claim 13 (depends on 11)

The cycloolefin resin composition according to claim 11, wherein the cycloolefin resin composition satisfies any one of the following conditions:
(1) the cycloolefin resin composition consists of component A and component B,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
(2) the cycloolefin resin composition consists of component A and component B,
the component A is tetracyclododecene;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:15000;
(3) the cycloolefin resin composition consists of component A and component B,
the component A is dihydrodicyclopentadiene;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:15000;
(4) the cycloolefin resin composition consists of component A, component B, and component C,
the component A consists of dicyclopentadiene and 5-ethylidene-2-norbornene, wherein the mass percentage of dicyclopentadiene in the component A is 98%, and the mass percentage of 5-ethylidene-2-norbornene in the component A is 2%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
the component C is liquid paraffin;
the ratio of the total mass of the component C and the component B to the mass of the component A is 1:20;
(5) the cycloolefin resin composition consists of component A, component B, and component C,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
the component C is chlorinated paraffin with a chlorine content of 5%;
the ratio of the total mass of the component C and the component B to the mass of the component A is 1:50;
(6) the cycloolefin resin composition consists of component A, component B, and component C,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
the component C is chlorinated paraffin with a chlorine content of 5%;
the ratio of the total mass of the component C and the component B to the mass of the component A is 1:50;
(7) the cycloolefin resin composition consists of component A and component B,
the component A consists of dicyclopentadiene, tricyclopentadiene, and tetracyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 79%, the mass percentage of tricyclopentadiene in the component A is 20%, and the mass percentage of tetracyclopentadiene in the component A is 1%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
(8) the cycloolefin resin composition consists of component A, component B, and component C,
the component A consists of dicyclopentadiene, tricyclopentadiene, and tetracyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 79%, the mass percentage of tricyclopentadiene in the component A is 20%, and the mass percentage of tetracyclopentadiene in the component A is 1%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
the component C is liquid paraffin;
the ratio of the total mass of the component C and the component B to the mass of the component A is 1:200;
(9) the cycloolefin resin composition consists of component A and component B,
the component A consists of dicyclopentadiene, tricyclopentadiene, and tetracyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 79%, the mass percentage of tricyclopentadiene in the component A is 20%, and the mass percentage of tetracyclopentadiene in the component A is 1%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
(10) the cycloolefin resin composition consists of component A and component B,
the component A consists of dicyclopentadiene, tricyclopentadiene, and tetracyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 79%, the mass percentage of tricyclopentadiene in the component A is 20%, and the mass percentage of tetracyclopentadiene in the component A is 1%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:50000;
(11) the cycloolefin resin composition consists of component A, component B, and component C,
the component A consists of dicyclopentadiene, tricyclopentadiene, dihydrodicyclopentadiene, and cyclohexene, wherein the mass percentage of dicyclopentadiene in the component A is 80%, the mass percentage of tricyclopentadiene in the component A is 15%, the mass percentage of dihydrodicyclopentadiene in the component A is 4.5%, and the mass percentage of cyclohexene in the component A is 0.5%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:9500;
the component C consists of liquid paraffin and chlorinated paraffin with a chlorine content of 52 wt %, wherein the mass ratio of liquid paraffin to chlorinated paraffin with a chlorine content of 52 wt % is 11:1;
the ratio of the total mass of the component C and the component B to the mass of the component A is 1:20;
(12) the cycloolefin resin composition consists of component A and component B,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B consists of
wherein the molar ratio of
is 1:2;
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
(13) the cycloolefin resin composition consists of component A and component B,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:7500;
(14) the cycloolefin resin composition consists of component A, component B, and component D,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
the component D is a mixture of n-pentadecane, EPDM, SBS, and mineral oil;
based on the total mass of the component A and the component D, in the component D, the mass percentage of n-pentadecane is 4-5%, and the mass percentages of EPDM, SBS, and mineral oil are independently 2-3%;
(15) the cycloolefin resin composition consists of component A, component B, and component D,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:10000;
the component D is a mixture of n-pentadecane, cetene, EPDM, SEBS, POE, and mineral oil;
based on the total mass of the component A and the component D, the mass percentage of n-pentadecane is 2-4%, the mass percentage of cetene is 0.3-1%, the mass percentage of EPDM is 2-3%, the mass percentage of SEBS is 0.3-1%, the mass percentage of POE is 0.5-1.2%, and the mass percentage of mineral oil is independently 2-3%;
(16) the cycloolefin resin composition consists of component A, component B, and component D,
the component A consists of dicyclopentadiene and tricyclopentadiene, wherein the mass percentage of dicyclopentadiene in the component A is 90%, and the mass percentage of tricyclopentadiene in the component A is 10%;
the component B is
the component D is a mixture of an antioxidant 264, triphenylphosphine, n-pentadecane, EPDM, SEBS, and POE;
based on the total mass of the component A and the component D, the mass percentage of the antioxidant 264 is 0.1-0.2%, the mass percentage of triphenylphosphine is 0.02-0.1%, the mass percentage of n-pentadecane is 4-5%, the mass percentage of EPDM is 1-2%, the mass percentage of SEBS is 1-2%, and the mass percentage of POE is 1-2%.

### Claim 14 (depends on 11)

A cycloolefin resin material, wherein the cycloolefin resin material is prepared using the cycloolefin resin composition M1, the cycloolefin resin composition M2, the cycloolefin resin composition M3, the cycloolefin resin composition M4, or the cycloolefin resin composition M5 according to claim 11 as a raw material.

### Claim 15 (depends on 14)

The cycloolefin resin material according to claim 14, wherein the cycloolefin resin material satisfies one or more of the following conditions:
(1) the cycloolefin resin material has a dielectric loss of <0.001 at a frequency of ≥1 GHz;
(2) the cycloolefin resin material has a dielectric constant of <2.5 at a frequency of ≥1 GHz;
(3) the cycloolefin resin material has a glass transition temperature of ≥135° C.;
(4) the cycloolefin resin material has a heat deflection temperature of ≥110° C.;
(5) the cycloolefin resin material is prepared using a liquid molding process.

### Claim 16

A method for reducing a dielectric constant and/or dielectric loss of a cycloolefin resin material, comprising: introducing component B into component A when preparing the cycloolefin resin material, wherein the component A is cycloolefin, the component B is a ruthenium alkylidene compound of Formula I and/or Formula II or a salt thereof, and the molar ratio of Ru in the component B to the monomer of cycloolefin in the component A is 1:(7500-60000),
wherein
R11 and R12 are each independently C4-C18 alkyl or C4-C18 alkyl substituted by R1-1;
R1-1 is C6-C10 aryl;
R21, R22, and R23 are each independently C6-C18 alkyl.

### Claim 17 (depends on 14)

A prepreg comprising the cycloolefin resin material according to claim 14.

### Claim 18 (depends on 17)

A copper-clad laminate comprising the prepreg according to claim 17.

### Claim 19 (depends on 18)

A printed circuit board comprising the copper-clad laminate according to claim 18.