# US 2026/0184910 A1 · Polyolefin resin composition with improved interfacial stability for insulation, a method for preparing the same and an article comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0184910 A1
- Document ID: US20260184910A1
- Status: Published application
- Kind: A1
- Application number: 19/405,742
- Filed: 2025-12-02
- Published: 2026-07-02
- Earliest claimed: 2024-12-26
- Assignees: Hanwha Totalenergies Petrochemical Co., Ltd.
- Applicants: Hanwha TotalEnergies Petrochemical Co.,Ltd.
- Inventors: Hyun Tae Jung; Jong Kun Song; Eun Woong Lee
- Web page: https://patentgrep.com/patent/US20260184910A1

## CPC

- C08L 53/00: Compositions of block copolymers containing at least one sequence of a polymer obtained by reactions only involving carbon-to-carbon unsaturated bonds; Compositions of derivatives of such polymers
- H01B 3/441: {from alkenes}
- C08F 2/001: {Multistage polymerisation processes characterised by a change in reactor conditions without deactivating the intermediate polymer (C08F295/00, C08F297/00 take precedence)}
- C08F 287/00: Macromolecular compounds obtained by polymerising monomers on to block polymers
- C08L 2203/202: use in electrical wires or wirecoating
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2205/035: containing four or more polymers in a blend
- C08L 2207/324: Liquid component is low molecular weight polymer
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The present invention relates to a polyolefin resin composition with improved interfacial stability for insulation, a method for preparing the same and an article comprising the same, and more specifically, it relates to a polyolefin resin composition which comprises an ethylene-propylene block copolymer, a propylene-alpha-olefin rubber copolymer with a propylene content in a specific range, and polyethylene glycol with a number average molecular weight in a specific range, and has excellent flexibility, low-temperature impact resistance, heat resistance, etc., good insulation breakdown characteristics, and, in particular, excellent interface stability for long-term life improvement, so that it can be suitably utilized as an eco-friendly material for insulation layer in power cables for low-voltage, high-voltage, or extra-high-voltage direct current (DC) or alternating current (AC) transmission or distribution (especially, insulation layer of a high-voltage or extra-high-voltage power cables), a method for preparing the same and an article (especially, power cable) comprising the same.

## Claims

### Claim 1

A polyolefin resin composition comprising:
(A) an ethylene-propylene block copolymer;
(B) a propylene-alpha-olefin rubber copolymer with a propylene content of more than 60% by weight; and
(C) a polyethylene glycol with a number average molecular weight of less than 20,000 g/mol.

### Claim 2 (depends on 1)

The polyolefin resin composition of claim 1, wherein the ethylene-propylene block copolymer is a polymerization product of a propylene homopolymer or an ethylene-propylene random copolymer and an ethylene-propylene rubber copolymer.

### Claim 3 (depends on 1)

The polyolefin resin composition of claim 1, wherein the amount of rubber component in 100% by weight of the ethylene-propylene block copolymer is 1 to 45% by weight, as extracted with a xylene solvent at 135° C.

### Claim 4 (depends on 1)

The polyolefin resin composition of claim 1, wherein the intrinsic viscosity of rubber component in the ethylene-propylene block copolymer is 1.0 to 4.0 dl/g, as measured in a decalin solvent at 135° C.

### Claim 5 (depends on 1)

The polyolefin resin composition of claim 1, wherein the melting temperature (Tm) of the ethylene-propylene block copolymer is 145 to 165° C.

### Claim 6 (depends on 1)

The polyolefin resin composition of claim 1, wherein the melt index of the ethylene-propylene block copolymer is 0.5 to 20.0 g/10 min, as measured at 230° C. under a load of 2.16 kg according to ASTM D1238.

### Claim 7 (depends on 1)

The polyolefin resin composition of claim 1, wherein the propylene-alpha-olefin rubber copolymer is at least one selected from the group consisting of propylene-ethylene rubber, propylene-1-butene rubber, propylene-butylene rubber, propylene-ethylene-butylene rubber, propylene-1-pentene rubber, propylene-1-hexene rubber, propylene-1-heptene rubber, propylene-1-octene rubber and propylene-4-methyl-1-pentene rubber.

### Claim 8 (depends on 1)

The polyolefin resin composition of claim 1, further comprising at least one additive selected from the group consisting of antioxidant, neutralizer, UV stabilizer, long-term heat stabilizer, slip agent, anti-blocking agent, reinforcing agent, filler, weather stabilizer, antistatic agent, lubricant, nucleating agent, flame retardant, pigment and dye.

### Claim 9 (depends on 1)

The polyolefin resin composition of claim 1, wherein the amount of rubber component in 100% by weight of the polyolefin resin composition is 25 to 45% by weight, as extracted with a xylene solvent at 135° C.

### Claim 10 (depends on 1)

The polyolefin resin composition of claim 1, wherein the glass transition temperature of rubber component in the polyolefin resin composition is-60 to −35° C.

### Claim 11 (depends on 1)

The polyolefin resin composition of claim 1, wherein the melting temperature (Tm) of the polyolefin resin composition is 145 to 165° C.

### Claim 12 (depends on 1)

The polyolefin resin composition of claim 1, wherein the melt index of the polyolefin resin composition is 0.5 to 20.0 g/10 min, as measured at 230° C. under a load of 2.16 kg according to ASTM D1238.

### Claim 13 (depends on 1)

The polyolefin resin composition of claim 1, wherein the flexural modulus of the polyolefin resin composition is less than 450 MPa, as measured by applying a flexural load at a rate of 5 mm/min according to ASTM D790.

### Claim 14 (depends on 1)

The polyolefin resin composition of claim 1, wherein a sheet with 1 mm thickness prepared by molding the polyolefin resin composition at a cooling rate of 1° C./min or less does not exhibit interfacial separation.

### Claim 15 (depends on 1)

The polyolefin resin composition of claim 1, wherein a sheet with 20 mm thickness prepared by molding the polyolefin resin composition at a cooling rate of 1° C./min or less, when aged at 80° C. for 30 days, does not exhibit interfacial separation.

### Claim 16

A method for preparing a polyolefin resin composition, comprising:
(1) a step of copolymerizing propylene and alpha-olefin in the presence of ethylene-propylene block copolymer to produce a propylene-alpha-olefin rubber copolymer with a propylene content of more than 60% by weight, or blending an ethylene-propylene block copolymer with a propylene-alpha-olefin rubber copolymer with a propylene content of more than 60% by weight; and
(2) a step of adding polyethylene glycol with a number average molecular weight of less than 20,000 g/mol to the resulting product of step (1).

### Claim 17 (depends on 1)

An article comprising the polyolefin resin composition of claim 1.

### Claim 18 (depends on 17)

The article of claim 17, wherein the polyolefin resin composition is that molded at a cooling rate of 1° C./min or less.

### Claim 19 (depends on 17)

The article of claim 17, which is a power cable comprising the polyolefin resin composition as insulation layer.