# US 2026/0184625 A1 · Method of forming lithium-free glass articles having improved compressive stress and reduced warp

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0184625 A1
- Document ID: US20260184625A1
- Status: Published application
- Kind: A1
- Application number: 19/407,518
- Filed: 2025-12-03
- Published: 2026-07-02
- Earliest claimed: 2024-12-30
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Ozgur Gulbiten; Atul Kumar; Qiang Zhang; Zheming Zheng
- Web page: https://patentgrep.com/patent/US20260184625A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03B 32/00: Thermal after-treatment of glass products not provided for in groups {C03B19/00} , C03B25/00 - C03B31/00 {or C03B37/00}, e.g. crystallisation, eliminating gas inclusions or other impurities; {Hot-pressing vitrified, non-porous, shaped glass products}
- C03C 3/091: containing aluminium
- C03C 23/007: {by thermal treatment}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A method of forming a lithium-free glass article includes thermally treating the glass article to impart a fictive temperature and ion exchanging the thermally treated glass article. The thermal treatment includes heating the glass article to a hold temperature from 130° C. below to 20° C. above an annealing point of the glass article; holding the glass article at the hold temperature for a hold period; cooling the glass article at a first cooling rate from the hold temperature to an intermediate temperature; and cooling the glass article at a second cooling rate from the intermediate temperature to room temperature. The ion exchanged glass article includes a compressive stress greater than or equal to 900 MPa, as measured for an article having a thickness of 1.1 mm; and a warp less than or equal to 0.3 mm, as measured for an article having a length less than 200 mm.

## Claims

### Claim 1

A method of forming a lithium-free glass article, the method comprising:
thermally treating the lithium-free glass article to impart a fictive temperature, the thermal treatment comprising:
heating the lithium-free glass article to a hold temperature greater than or equal to 130° C. below and less than or equal to 20° C. above an annealing point of the lithium-free glass article;
holding the lithium-free glass article at the hold temperature for a hold period; and
cooling the lithium-free glass article at a first cooling rate from the hold temperature to an intermediate temperature;
cooling the lithium-free glass article at a second cooling rate from the intermediate temperature to room temperature; and
ion exchanging the thermally treated lithium-free glass article,
wherein the ion exchanged lithium-free glass article comprises:
a compressive stress greater than or equal to 900 MPa, as measured for an article having a thickness of 1.1 mm; and
a warp less than or equal to 0.3 mm, as measured for an article having a length less than 200 mm.

### Claim 2 (depends on 1)

The method of claim 1, wherein the fictive temperature is greater than or equal to 550° C. and less than or equal to 700° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the hold period is greater than or equal to 0.05 minutes and less than or equal to 24 hours.

### Claim 4 (depends on 3)

The method of claim 3, wherein the hold period is greater than or equal to 0.25 minutes and less than or equal to 6 hours.

### Claim 5 (depends on 1)

The method of claim 1, wherein the lithium-free glass article is heated to the hold temperature at a heating rate greater than or equal to 3° C./min and less than or equal to 20° C./min.

### Claim 6 (depends on 1)

The method of claim 1, wherein the hold temperature is greater than or equal to 110° C. below and less than or equal to 5° C. above an annealing point of the lithium-free glass article.

### Claim 7 (depends on 1)

The method of claim 1, wherein the hold temperature is greater than or equal to 500° C. and less than or equal to 650° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first cooling rate is greater than or equal to 0.2° C./min and less than or equal to 4° C./min.

### Claim 9 (depends on 1)

The method of claim 1, wherein the intermediate temperature is greater than or equal to 300° C. and less than or equal to 530° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the second cooling rate is greater than or equal to 20° C./min and less than or equal to 120° C./min.

### Claim 11 (depends on 1)

The method of claim 1, wherein the ion exchanging the thermally treated lithium-free glass article comprises strengthening the thermally treated lithium-free glass article in an ion exchange bath at a temperature greater than or equal to 380° C. and less than or equal to 500° C. for a time period greater than or equal to 1 hour and less than or equal to 20 hours.

### Claim 12 (depends on 11)

The method of claim 11, wherein the ion exchange bath comprises greater than or equal to 90 wt % and less than or equal to 100 wt % KNO3 and greater than or equal to 0 wt % and less than or equal to 10 wt % NaNO3.

### Claim 13 (depends on 1)

The method of claim 1, wherein the ion exchanged lithium-free glass article comprises a compressive stress greater than or equal to 1000 MPa, as measured for an article having a thickness of 1.1 mm.

### Claim 14 (depends on 1)

The method of claim 1, wherein the ion exchanged lithium-free glass article comprises a warp less than or equal to 0.2 mm, as measured for an article having a length less than 200 mm.

### Claim 15 (depends on 1)

The method of claim 1, wherein the ion exchanged lithium-free glass article comprises a depth of layer greater than or equal to 35 μm, as measured for an article having a thickness of 1.1 mm.

### Claim 16 (depends on 1)

The method of claim 1, wherein the ion exchanged lithium-free glass article comprises an automotive interior article.

### Claim 17 (depends on 1)

The method of claim 1, wherein the lithium-free glass article comprises an alkali aluminosilicate glass or an alkali aluminoborosilicate glass.

### Claim 18 (depends on 1)

The method of claim 1, wherein the lithium-free glass article comprises:
greater than or equal to 50 wt % and less than or equal to 70 wt % SiO2;
greater than or equal to 0 wt % and less than or equal to 10 wt % B2O3;
greater than or equal to 10 wt % and less than or equal to 30 wt % Al2O3;
greater than or equal to 2 wt % and less than or equal to 20 wt % Na2O;
greater than or equal to 0 wt % and less than or equal to 1 wt % SnO2; and
greater than or equal to 0 wt % and less than or equal to 5 wt % MgO.

### Claim 19 (depends on 1)

The method of claim 1, wherein the lithium-free glass article comprises a thickness greater than or equal to 0.2 mm and less than or equal to 2 mm.

### Claim 20 (depends on 1)

The method of claim 1, wherein the thermally treating the lithium-free glass article comprises holding the lithium-free glass article in a cassette during thermal treatment.