# US 2026/0184582 A1 · Lithium ion conductor and all solid state battery comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0184582 A1
- Document ID: US20260184582A1
- Status: Published application
- Kind: A1
- Application number: 18/729,800
- Filed: 2024-06-14
- Published: 2026-07-02
- Earliest claimed: 2023-06-29
- Assignees: Samsung Electro-Mechanics Co., Ltd.; Bass, Inc.
- Applicants: Samsung Electro-Mechanics Co., Ltd.; Bass Co., Ltd.
- Inventors: Kyongbok Min; Han Kim; Jongmin Kim; Kil Ho Kim; Daehyun Kim; Taeho Park; Shiwoo Lee; Duckhyun Chang; Emmanuel Kwame Ampadu; Poo Reum Choi
- Web page: https://patentgrep.com/patent/US20260184582A1

## CPC

- C01D 15/04: Halides
- C03C 10/16: Halogen containing crystalline phase
- C03C 3/23: containing halogen and at least one oxide, e.g. oxide of boron
- C03C 4/14: for electro-conductive glass
- H01B 1/08: oxides
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/66: Selection of materials
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0562: Solid materials
- H01M 10/058: Construction or manufacture
- C01P 2002/04: Compounds with a limited amount of crystallinty, e.g. as indicated by a crystallinity index
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/88: by thermal analysis data, e.g. TGA, DTA, DSC
- C01P 2004/03: obtained by SEM
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0071: Oxides
- H01M 2300/008: Halides
- Y02E 60/10: Energy storage using batteries
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The lithium ion conductor for an all-solid-state battery according to the present disclosure is represented by Chemical Formula 1. In Chemical Formula 1, 4.2≤x≤6.0, 0.15≤y≤0.45, and z≥1.1, and X is F, Cl, Br, or I.

## Claims

### Claim 1

A lithium ion conductor being represented by Chemical Formula 1:
Lix(B1-yAly)7O12X2 [Chemical Formula 1]
wherein, in Chemical Formula 1,
4.2≤x≤6.0, 0.15≤y≤0.45, and z≥1.1, and
X is F, Cl, Br, or I.

### Claim 2 (depends on 1)

The lithium ion conductor of claim 1, wherein
the lithium ion conductor has a crystallinity of 65% to 100% calculated by Equation 1:
Crystallinity (%)=[Ic/(Ic+Ia)]×100 [Equation 1]
wherein, in Equation 1, Ic is a sum of integrated values of scattering intensities of crystalline peaks in an X-ray diffraction analysis spectrum of the lithium ion conductor, and
Ia is a sum of integral values of the scattering intensities of the amorphous halo in an X-ray diffraction analysis spectrum of the lithium ion conductor.

### Claim 3 (depends on 1)

The lithium ion conductor of claim 1, wherein
the lithium ion conductor includes a crystal, and
the crystal includes a first crystal represented by LiaB7-bAlbO12Xe and a second crystal represented by Li4B7O12X:
in the first crystal, 3.5≤a≤4, 0<b<7, and 0.9≤c≤1, and
in the first crystal and the second crystal, X is F, Cl, Br, or I.

### Claim 4 (depends on 3)

The lithium ion conductor of claim 3, wherein
a crystallization ratio of the first crystal and the second crystal is 2.5:1 to 20:1.

### Claim 5 (depends on 1)

The lithium ion conductor of claim 1, wherein
a lithium ionic conductivity at 25° C. of the lithium ion conductor is greater than or equal to 1.0λ10−5 S/cm.

### Claim 6 (depends on 1)

The lithium ion conductor of claim 1, wherein
a crystallization temperature (Tc) of the lithium ion conductor is 400° C. to 500° C.

### Claim 7

A method of preparing a lithium ion conductor, comprising melting and cooling a precursor mixture including lithium (Li) oxide, boron (B) oxide, aluminum (Al) oxide, and lithium halide (Li—X); and heat-treating the precursor mixture, to prepare lithium ion conductor represented by Chemical Formula 1:
Lix(B1 yAly)7O12X2 [Chemical Formula 1]
wherein, in Chemical Formula 1,
4.2≤x≤6.0, 0.15≤y≤0.45, and z≥1.1, and
X is F, Cl, Br, or I.

### Claim 8 (depends on 7)

The method of claim 7, wherein
the precursor mixture includes 25 mol % to 30 mol % of the lithium (Li) oxide, 35 mol % to 45 mol % of the boron (B) oxide, 10 mol % to 20 mol % of the aluminum (Al) oxide, and 15 mol % to 30 mol % of the lithium halide (LiX), where X is F, Cl, Br, or I, based on a total of 100 mol % of the precursor mixture.

### Claim 9 (depends on 7)

The method of claim 7, wherein
the heat-treating of the precursor mixture is performed at a temperature of 350° C. to 550° C.

### Claim 10

An all-solid-state battery, comprising
a solid electrolyte layer and a positive electrode layer and a negative electrode layer disposed with the solid electrolyte layer therebetween, wherein any one selected from the solid electrolyte layer, the positive electrode layer, the negative electrode layer,
and a combination thereof includes a lithium ion conductor, and the lithium ion conductor is represented by Chemical Formula 1:
Lix(B1-yAly)7O12X2 [Chemical Formula 1]
wherein, in Chemical Formula 1,
4.2≤x≤6.0, 0.15≤y≤0.45, and z≥1.1, and
X is F, Cl, Br, or I.

### Claim 11 (depends on 10)

The all-solid-state battery of claim 10, wherein
a crystallinity of the lithium ion conductor calculated by Equation 1 is 65% to 100%:
Crystallinity (%)=[Ic/(Ic+Ia)]×100 [Equation 1]
wherein, in Equation 1, Ic is a sum of integrated values of scattering intensities of crystalline peaks in an X-ray diffraction analysis spectrum of the lithium ion conductor, and
Ia is a sum of integral values of the scattering intensities of the amorphous halo in an X-ray diffraction analysis spectrum of the lithium ion conductor.

### Claim 12 (depends on 10)

The all-solid-state battery of claim 10, wherein
the lithium ion conductor includes a crystal, and
the crystal includes a first crystal represented by LiaB7-bAlbO12Xe and a second crystal represented by Li4B7O12X:
in the first crystal, 3.5≤a≤4, 0<b<7, and 0.9≤c≤1, and
in the first crystal or second crystal, X is F, Cl, Br, or I.

### Claim 13 (depends on 12)

The all-solid-state battery of claim 12, wherein
a crystallization ratio of the first crystal and the second crystal is 2.5:1 to 20:1.

### Claim 14 (depends on 10)

The all-solid-state battery of claim 10, wherein
a lithium ionic conductivity at 25° C. of the lithium ion conductor is greater than or equal to 1.0λ10−5 S/cm.

### Claim 15 (depends on 10)

The all-solid-state battery of claim 10, wherein
a crystallization temperature (Tc) of the lithium ion conductor is 400° C. to 500° C.

### Claim 16 (depends on 1)

The lithium ion conductor of claim 1, wherein z is less than or equal to 1.4

### Claim 17 (depends on 10)

The all-solid-state battery of claim 10, wherein the positive electrode layer has a thickness greater than that of the negative electrode layer, and the solid electrolyte layer has a thickness greater than both the positive and negative electrode layers.

### Claim 18

A method of manufacturing an all-solid-state battery, comprising:
preparing a solid electrolyte layer green sheet including a fused and cooled precursor mixture;
preparing a positive electrode layer green sheet including a positive electrode active material and a lithium ion conductor;
preparing a negative electrode layer green sheet including a negative electrode active material and the lithium ion conductor;
stacking the positive electrode layer green sheet, the solid electrolyte layer green sheet and the negative electrode green sheet; and
firing the stack with a hot press under pressure,
wherein the precursor mixture comprises Li2O, B2O3, Al2O3 and LiX, X being selected from the group consisting of F, Cl, Br and I, and
wherein the lithium ion conductor is represented by Chemical Formula 1:
Lix(B1-yAly)7O12X2 [Chemical Formula 1]
wherein, in Chemical Formula 1,
4.2≤x≤6.0, 0.15≤y≤0.45, and z≥1.1, and
X is F, Cl, Br, or I.

### Claim 19 (depends on 18)

The method of claim 18, wherein firing is performed at a temperature in a range from 300° C. to 600° C.

### Claim 20 (depends on 18)

The method of claim 18, wherein firing is performed under a pressure in a range from 20 MPa to 60 MPa.

### Claim 21 (depends on 18)

The method of claim 18, wherein preparing the solid electrolyte layer green sheet comprises:
melting and cooling the precursor mixture; and
heat-treating the precursor mixture.

### Claim 22 (depends on 21)

The method of claim 21, wherein the heat-treating of the precursor mixture is performed at a temperature of 350° C. to 550° C.

### Claim 23 (depends on 21)

The method of claim 21, wherein the heat-treating is performed at a pressure in a range from 0.5 MPa to 40 MPa.

### Claim 24 (depends on 18)

The method of claim 18, wherein a content of lithium ion conductor in the positive electrode layer green sheet and/or the negative electrode layer green sheet is in a range from 10% to 80%.

### Claim 25 (depends on 18)

The method of claim 18, wherein the positive electrode active material is selected from the group consisting of lithium cobalt oxide, lithium nickel cobalt manganese oxide, lithium nickel cobalt aluminum oxide, lithium iron phosphate, lithium manganese oxide, and a combination thereof.

### Claim 26 (depends on 18)

The method of claim 18, wherein the negative electrode active material is selected from the group consisting of a carbon-based material, silicon, a silicon oxide, a silicon-based alloy, a silicon-carbon-based material composite, tin, a tin-based alloy, a tin-carbon composite, a metal oxide, a lithium metal, a lithium metal alloy and a combination thereof.

### Claim 27 (depends on 18)

The method of claim 18, wherein the solid electrolyte layer further comprises inorganic solid electrolyte including an oxide-based solid electrolyte, a sulfide-based solid electrolyte, or a combination thereof.