# US 2026/0183875 A1 · Method for manufacturing joined body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0183875 A1
- Document ID: US20260183875A1
- Status: Published application
- Kind: A1
- Application number: 19/428,750
- Filed: 2025-12-22
- Published: 2026-07-02
- Earliest claimed: 2024-12-27
- Assignees: Futaba Industrial Co., Ltd.
- Applicants: Futaba Industrial Co., Ltd.
- Inventors: Tomohiro Katsura; Shoichi Kawano; Yusuke Kito
- Web page: https://patentgrep.com/patent/US20260183875A1

## CPC

- B23K 31/125: {Weld quality monitoring}
- B23K 11/11: Spot welding
- B23K 11/115: {by means of two electrodes placed opposite one another on both sides of the welded parts}
- B23K 11/25: Monitoring devices
- B23K 11/256: {the measured parameter being the inter-electrode electrical resistance}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

One aspect of the present disclosure provides a method including: clamping a first combination of metal workpieces between a first pair of electrodes; applying a welding current between the first pair of electrodes to weld the first combination of metal workpieces, wherein a magnitude of the welding current is set such that a resistance value between the first pair of electrodes falls within a specified range; measuring the resistance value between the first pair of electrodes, during welding of the first combination of metal workpieces, based on (i) the magnitude of the welding current and (ii) a magnitude of a voltage between the first pair of electrodes; and determining, based on the resistance value measured deviating from a specified permissible range, that a welding defect has occurred in the first combination of metal workpieces.

## Claims

### Claim 1

A method for manufacturing a joined body, the method comprising:
clamping a first combination of metal workpieces between a first pair of electrodes;
applying a welding current between the first pair of electrodes to weld the first combination of metal workpieces, wherein a magnitude of the welding current is set such that a resistance value between the first pair of electrodes falls within a specified range;
measuring the resistance value between the first pair of electrodes, during welding of the first combination of metal workpieces, based on (i) the magnitude of the welding current and (ii) a magnitude of a voltage between the first pair of electrodes; and
determining, based on the resistance value measured deviating from a specified permissible range, that a welding defect has occurred in the first combination of metal workpieces.

### Claim 2 (depends on 1)

The method according to claim 1, wherein:
the magnitude of the welding current is set in accordance with a preset current profile over time;
the preset current profile is set to correspond to a resistance profile over time;
the resistance profile is measured by (i) clamping a second combination of metal workpieces between a second pair of electrodes and (ii) applying a constant measurement current between the second pair of electrodes; and
the second combination of metal workpieces is equivalent to the first combination of metal workpieces.

### Claim 3 (depends on 2)

The method according to claim 2, wherein
the constant measurement current is set to a value such that no welding spatter is generated on the second combination of metal workpieces.

### Claim 4 (depends on 1)

The method according to claim 1, wherein
applying a welding current between the first pair of electrodes to weld the first combination of metal workpieces comprises using a welding apparatus capable of controlling the magnitude of the welding current with a time resolution on the order of milliseconds.