# US 2026/0183832 A1 · Joining Method And Self-Piercing Joining Element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0183832 A1
- Document ID: US20260183832A1
- Status: Published application
- Kind: A1
- Application number: 19/545,617
- Filed: 2026-02-20
- Published: 2026-07-02
- Earliest claimed: 2023-08-22
- Assignees: Newfrey LLC
- Applicants: Newfrey LLC
- Inventors: Vadim SARTISSON; Christian Reis; Orhan Demircioglu; Maximilian Stock
- Web page: https://patentgrep.com/patent/US20260183832A1

## CPC

- B21J 15/025: {Setting self-piercing rivets}
- B21J 15/08: Riveting by applying heat {, e.g.} to the end parts of the rivets to enable heads to be formed {(B21J15/027 takes precedence)}
- F16B 5/04: by means of riveting (rivets F16B19/04)
- F16B 19/086: {Self-piercing rivets}
- F16B 2019/045: {Coated rivets}
- B21J: FORGING; HAMMERING; PRESSING METAL; RIVETING; FORGE FURNACES (rolling of metal B21B; making particular products by forging or pressing B21K; cladding or plating B23K; finishing surfaces by hammering B23P9/04; compacting surfaces by blasting with particulate material B24C1/10; general features of presses, presses for consolidating scrap B30B; furnaces in general F27)
- F16B: DEVICES FOR FASTENING OR SECURING CONSTRUCTIONAL ELEMENTS OR MACHINE PARTS TOGETHER, e.g. NAILS, BOLTS, CIRCLIPS, CLAMPS, CLIPS OR WEDGES; JOINTS OR JOINTING (couplings for transmitting rotation F16D)

## Abstract

A method for joining components, particularly metal components, via a joining element which is deformed during the joining process, comprising the following steps: coating a joining element with a temperature-stable coating; preheating at least one of at least two components in an area of a joining location to a preheating temperature in the range from 90° C. to 1,400 ° C., preferably by plasma-heating, laser-heating, electric arc heating and/or induction heating, wherein the components are stacked on top of each other; and driving the coated joining element into the stacked components.

## Claims

### Claim 1

A method for joining components via a self-piercing joining element which is deformed during a joining process, the method comprising:
coating a self-piercing joining element with a coating which has a melting temperature;
preheating at least one of at least two components in an area of a joining location to a preheating temperature in a range from 90 degrees Celsius (° C.) to 1,400° C., wherein the components are stacked on top of each other; and
driving the coated self-piercing joining element into the stacked components,
wherein the coating is configured to be temperature-stable during the step of driving the coated self-piercing joining element into the stacked components,
wherein the preheating temperature is lower than the melting temperature of the coating,
wherein the coating comprises a base coating having a high thermal stability and a friction control coating applied on the base coating, the friction control coating being a top coat with integrated lubricants so as to provide for an optimized coefficient of friction, and
wherein the base coating, before applying the friction control coating, is passivated to provide a passivation layer on top of the base coating, the passivation layer having a thickness in a range from 50 nanometers (nm) to 400 nm.

### Claim 2 (depends on 1)

The method of claim 1, wherein the base coating is made of one of a zinc-based coating, a nickel-based coating, or a copper-based coating.

### Claim 3 (depends on 2)

The method of claim 2, wherein the base coating is made of at least one material selected from the group consisting of: zinc (Zn), a Zn alloy, zinc nickel (ZnNi), nickel (Ni), a Ni alloy, nickel phosphide (NiP), nickel tungsten (NiW), copper (Cu), a Cu alloy, copper nickel (CuNi), and zinc flake.

### Claim 4 (depends on 2)

The method of claim 2, wherein the base coating is a zinc-based coating which includes 8% to 20% nickel.

### Claim 5 (depends on 2)

The method of claim 2, wherein the base coating is a nickel-based coating which includes one of 1% to 15% phosphorous or 30% to 35% tungsten.

### Claim 6 (depends on 1)

The method of claim 1, wherein the friction control coating has a friction coefficient in a range from 0.07 to 0.19.

### Claim 7 (depends on 1)

The method of claim 1, wherein the base coating has a thickness in a range from 3 micrometer (μm) to 15 μm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the base coating, before applying the friction control coating, is baked.

### Claim 9 (depends on 1)

The method of claim 1, wherein the friction control coating has a thickness in a range from 1 μm to 6 μm.

### Claim 10 (depends on 1)

The method of claim 1, wherein the joining element is a punch rivet.

### Claim 11 (depends on 1)

The method of claim 1, wherein the joining element has a Vickers hardness in a range from 220±30 Vickers Pyramid Number (HV) 10 to 590±30 HV10.

### Claim 12 (depends on 1)

The method of claim 1, wherein the at least two components include a first component which is made of steel having a strength in the range from 1000 megapascal (MPa) to 2100 MPa.

### Claim 13 (depends on 12)

The method of claim 12, wherein the at least two components include a second component which is made of an aluminum alloy.

### Claim 14 (depends on 1)

The method of claim 1, wherein the preheating step includes heating the joining location area up to a maximum preheating temperature, and stopping or ramping down the heating thereafter.

### Claim 15 (depends on 14)

The method of claim 14, wherein the step of driving the coated joining element into the stacked components starts at a temperature of the joining location area, which is less than the maximum preheating temperature and higher than 30% of the maximum preheating temperature.

### Claim 16 (depends on 15)

The method of claim 15, wherein the step of driving the coated joining element into the stacked components ends at a temperature of the joining location area, which is higher than a temperature of the environment and less than 85% of the maximum preheating temperature.

### Claim 17

A method of using a joining element in a heat-superimposed mechanical joining process, the method comprising:
providing a joining element having a coating, the coating providing a high thermal stability and an optimized friction coefficient; and
driving the joining element into at least two stacked components after at least one of the components has been preheated at a joining location.

### Claim 18

A self-piercing joining element for use in a joining method, wherein at least one of at least two components to be joined is preheated, the self-piercing joining element comprising:
a body configured to be deformed during a joining process, the body being at least partially coated with a thermally-stable coating.

### Claim 19 (depends on 18)

The self-piercing joining element of claim 18, wherein the coating includes a base coating which has a high thermal stability, and a friction control coating which is applied on the base coating.