# US 2026/0183760 A1 · Modified Zeolite Catalyst Compositions and Methods of Use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0183760 A1
- Document ID: US20260183760A1
- Status: Published application
- Kind: A1
- Application number: 19/547,829
- Filed: 2026-02-24
- Published: 2026-07-02
- Earliest claimed: 2019-10-29
- Assignees: W.R. Grace & Co.-Conn.
- Applicants: W.R. Grace & Co.-Conn.
- Inventors: Dorai Ramprasad
- Web page: https://patentgrep.com/patent/US20260183760A1

## CPC

- B01J 29/40: of the pentasil type, e.g. types ZSM-5, ZSM-8 or ZSM-11, as exemplified by patent documents US3702886, GB1334243 and US3709979, respectively
- B01J 37/26: Fluorinating
- B01J 21/04: Alumina
- B01J 21/16: Clays or other mineral silicates
- B01J 23/06: of zinc, cadmium or mercury
- B01J 27/12: Fluorides
- B01J 27/138: with alkaline earth metals, magnesium, beryllium, zinc, cadmium or mercury
- B01J 29/405: {containing rare earth elements, titanium, zirconium, hafnium, zinc, cadmium, mercury, gallium, indium, thallium, tin or lead}
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 37/0205: {in several steps}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C07D 211/02: Preparation by ring-closure or hydrogenation
- C07D 213/10: from acetaldehyde or cyclic polymers thereof
- B01J 27/132: with chromium, molybdenum, tungsten or polonium
- B01J 29/48: containing arsenic, antimony, bismuth, vanadium, niobium tantalum, polonium, chromium, molybdenum, tungsten, manganese, technetium or rhenium
- B01J 2229/16: to increase the Si/Al ratio; Dealumination
- B01J 2229/186: not in framework positions
- B01J 2229/20: to introduce other elements in the catalyst composition comprising the molecular sieve, but not specially in or on the molecular sieve itself
- B01J 2229/42: Addition of matrix or binder particles
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07D: HETEROCYCLIC COMPOUNDS (macromolecular compounds C08)

## Abstract

A modified zeolite catalyst composition is disclosed formed from a zeolite, alumina binder, and matrix. The modified zeolite catalyst composition may contain fluorine. Also disclosed, are methods for the preparation of pyridine and/or its alkylpyridine derivatives in high yield utilizing the modified zeolite catalyst composition.

## Claims

### Claim 1

A modified zeolite catalyst composition, comprising:
one or more particles comprising
a zeolite;
an alumina binder; and
a matrix; wherein at least one of the zeolite, alumina binder, or matrix has been treated with one or more ions of or compounds containing fluorine, wherein the one or more particles have an average particle size of from about 20 μm to about 100 μm.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the zeolite comprises ZSM-5.

### Claim 3 (depends on 1)

The composition of claim 1, wherein the alumina binder is selected from the group consisting of (pseudo)boehmite, gibbsite, heat-treated forms of gibbsite such as flash-calcined gibbsite, poly aluminum chloride, highly crystalline alumina, and combinations thereof.

### Claim 4 (depends on 1)

The composition of claim 1, wherein the modified zeolite catalyst comprises from about 30% to about 40% by weight of zeolite, from about 7% to about 12$ by weight of alumina, and from about 35% to about 48% by weight of matrix.

### Claim 5 (depends on 1)

The composition of claim 1, wherein the matrix comprises kaolin.

### Claim 6 (depends on 1)

The composition of claim 1, wherein the zeolite comprises a zeolite having a silica to alumina ratio of from about 20:1 to about 60:1.

### Claim 7

A method for preparing a modified zeolite catalyst composition, said method comprising the steps of:
combining a zeolite with an alumina binder and matrix to form a catalyst composition;
contacting the catalyst composition with one or more fluorine containing compounds to form a modified zeolite catalyst composition, and
drying the modified zeolite catalyst composition.

### Claim 8 (depends on 7)

The method of claim 7, wherein the zeolite comprises ZSM-5.

### Claim 9 (depends on 7)

The method of claim 7, wherein the alumina binder is selected from the group consisting of (pseudo)boehmite, gibbsite, heat-treated forms of gibbsite such as flash-calcined gibbsite, poly aluminum chloride, highly crystalline alumina, and combinations thereof.

### Claim 10 (depends on 7)

The method of claim 7, wherein the flouring containing compound is selected from ammonium fluorosilicate, ammonium fluoride, zinc hexaflourosilicate, and combinations thereof.

### Claim 11 (depends on 7)

The method of claim 7, wherein contacting the catalyst composition with the fluorine containing compound comprises contacting the catalyst composition via an incipient wetness method with the fluorine containing compound.

### Claim 12 (depends on 7)

The method of claim 7, wherein drying the modified zeolite catalyst composition comprises drying the modified zeolite catalyst composition in a vacuum oven at a temperature of from about 100° C. to about 140° C. for a drying time of from about 5 hours to about 12 hours.

### Claim 13 (depends on 7)

The method of claim 7, further comprising contacting the modified zeolite catalyst composition a second time with a fluorine containing compound after drying.

### Claim 14 (depends on 7)

The method of claim 7, further comprising calcining the modified zeolite catalyst composition.

### Claim 15 (depends on 14)

The method of claim 14, wherein calcining the modified zeolite catalyst composition comprises calcining the modified zeolite catalyst composition at a temperature of about 550° C. for about 5 hours.

### Claim 16 (depends on 14)

The method of claim 14, wherein combining the zeolite with an alumina binder and matrix comprises spray drying the zeolite with alumina binder and kaolin.

### Claim 17 (depends on 14)

The method of claim 14, wherein combining the zeolite with an alumina binder and matrix comprises preparing a slurry comprising the zeolite, alumina binder, and matrix, and spray-drying the slurry to form one or more particles of the modified zeolite catalyst composition.

### Claim 18 (depends on 14)

The method of claim 14, wherein the modified zeolite catalyst composition comprises form about 40% by weight of zeolite, from about 12% by weight alumina, and from about 48% by weight of matrix.

### Claim 19 (depends on 14)

The method of claim 14, wherein the fluorine containing compound is zinc hexafluorosilicate hydrate.

### Claim 20 (depends on 14)

A modified zeolite catalyst composition according to claim 14.