# US 2026/0183740 A1 · Porous carbon sorbent for carbon dioxide capture and methods of making and using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0183740 A1
- Document ID: US20260183740A1
- Status: Published application
- Kind: A1
- Application number: 19/008,033
- Filed: 2025-01-02
- Published: 2026-07-02
- Earliest claimed: 2025-01-02
- Assignees: Saudi Arabian Oil Company
- Applicants: Saudi Arabian Oil Company
- Inventors: Wala Algozeeb; Noha Al-Shihri; Emad N. Al-Shafei
- Web page: https://patentgrep.com/patent/US20260183740A1

## CPC

- B01J 20/20: comprising free carbon; comprising carbon obtained by carbonising processes
- B01D 53/0462: {Temperature swing adsorption}
- B01D 53/047: Pressure swing adsorption
- B01J 20/205: {Carbon nanostructures, e.g. nanotubes, nanohorns, nanocones, nanoballs (carbon nanotubes per se C01B32/15)}
- B01J 20/28057: {Surface area, e.g. B.E.T specific surface area}
- B01J 20/28061: {being in the range 100-500 m2/g}
- B01J 20/28064: {being in the range 500-1000 m2/g}
- B01J 20/28066: {being more than 1000 m2/g}
- B01J 20/28069: {Pore volume, e.g. total pore volume, mesopore volume, micropore volume}
- B01J 20/28071: {being less than 0.5 ml/g}
- B01J 20/28073: {being in the range 0.5-1.0 ml/g}
- B01J 20/2808: {being less than 2 nm, i.e. micropores or nanopores}
- B01J 20/28083: {being in the range 2-50 nm, i.e. mesopores}
- B01J 20/3071: {Washing or leaching}
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- C01B 32/05: Preparation or purification of carbon not covered by groups C01B32/15, C01B32/20, C01B32/25, C01B32/30
- B01D 2253/102: Carbon
- B01D 2253/112: Metals or metal compounds not provided for in B01D2253/104 or B01D2253/106
- B01D 2253/306: Surface area, e.g. BET-specific surface
- B01D 2253/308: Pore size
- B01D 2253/311: Porosity, e.g. pore volume
- B01D 2257/504: Carbon dioxide
- B01D 2259/40088: by heating
- C01P 2006/12: Surface area
- C01P 2006/14: Pore volume
- C01P 2006/16: Pore diameter
- Y02C 20/40: of CO2
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02C: CAPTURE, STORAGE, SEQUESTRATION OR DISPOSAL OF GREENHOUSE GASES [GHG]

## Abstract

A method for capturing and releasing carbon dioxide (CO2) includes contacting a nanoporous carbon (NPC) material with a CO2-containing gas stream, thereby at least partially absorbing CO2 in the form of molecules on surfaces and pores of the NPC material to form a sample; releasing the CO2 from the sample by thermally heating the sample or exposing the sample to a pressure swing adsorption (PSA) unit; and collecting the CO2. A method of making the NPC material by heating one or more low fixed carbon feeds in the presence of one or more metal salts is also disclosed.

## Claims

### Claim 1

A method for capturing and releasing carbon dioxide (CO2), comprising:
contacting a nanoporous carbon (NPC) material with a CO2-containing gas stream, thereby at least partially absorbing CO2 in the form of molecules on surfaces and pores of the NPC material to form a sample, wherein the NPC material is prepared from one or more low fixed carbon feeds selected from the group consisting of a pyrolysis oil, a light cycle oil, a heavy cycle oil, an Arab light crude oil, an Arab extra light crude oil, a natural gas fluid, and mixtures thereof;
releasing the CO2 from the sample by thermally heating the sample or exposing the sample to a pressure swing adsorption (PSA) unit; and
collecting the CO2.

### Claim 2 (depends on 1)

The method of claim 1, wherein the NPC material is in contact with the CO2-containing gas stream at a temperature of about 0 to about 25° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the NPC material is in contact with the CO2-containing gas stream at a pressure of about 1 to about 800 atmospheric pressure (Po).

### Claim 4 (depends on 1)

The method of claim 1, wherein the NPC material comprises about 50 to about 90 wt. % of carbon, about 10 to about 50 wt. % of oxygen, and about 0.001 to about 10 wt. % of one or more alkali metals and alkali earth metals, as determined by energy dispersive X-ray spectroscopy (EDX).

### Claim 5 (depends on 4)

The method of claim 4, wherein the one or more alkali metals and alkali earth metals are selected from the group consisting of lithium, sodium, potassium, rubidium, cesium, francium, beryllium, magnesium, calcium, strontium, barium, radium, and mixtures thereof.

### Claim 6 (depends on 4)

The method of claim 4, wherein the NPC material comprises about 64.4 wt. % of carbon, about 30.2 wt. % of oxygen, and about 5.4 wt. % of potassium.

### Claim 7 (depends on 1)

The method of claim 1, wherein the NPC material has a hierarchical pore structure comprising mesopores and nanopores.

### Claim 8 (depends on 1)

The method of claim 1, wherein the NPC material has a Barrett-Joyner-Halenda (BJH) pore size of about 1 nanometers (nm) to about 2 nm.

### Claim 9 (depends on 1)

The method of claim 1, wherein the NPC material has an average pore volume of about 0.2 to about 0.9 milliliters per gram (mL/g).

### Claim 10 (depends on 1)

The method of claim 1, wherein the NPC material has a Brunauer-Emmett-Teller (BET) surface area of about 450 to about 1050 square meters per gram (m2/g).

### Claim 11 (depends on 1)

The method of claim 1, wherein the NPC material has a CO2 uptake capacity of about 0.1 to about 7 millimoles of CO2 per gram of the NPC material (mmol/g) at a temperature of about 25° C.

### Claim 12 (depends on 1)

The method of claim 1, wherein the NPC material has less than about 0.05 wt. % of weight loss at a temperature of up to about 400° C. in an oxygen atmosphere.

### Claim 13 (depends on 1)

The method of claim 1, wherein the thermally heating the sample is carried out at a temperature of about 30 to about 150° C.

### Claim 14 (depends on 1)

The method of claim 1, wherein the exposing the sample to the PSA unit is carried out under a reduced pressure condition, thereby releasing the CO2 from the NPC material.

### Claim 15 (depends on 1)

The method of claim 1, further comprising preparing the NPC material by:
mixing the one or more low fixed carbon feeds and one or more metal salts to form a mixture;
heating the mixture at a temperature of about 400 to about 800° C. in an inert atmosphere to form a crude material; and
washing the crude material with water and drying.

### Claim 16 (depends on 15)

The method of claim 15, wherein the one or more metal salts are compounds having a formula X-Y, wherein X is a metal cation selected from the group consisting of potassium, calcium, and sodium, and wherein Y is an anion selected from the group consisting of fluoride, chloride, bromide, acetate, oxalate, carbonate, and bicarbonate.

### Claim 17 (depends on 16)

The method of claim 16, wherein the one or more metal salts comprise potassium carbonate and potassium chloride.

### Claim 18 (depends on 15)

The method of claim 15, wherein a weight ratio of the one or more low fixed carbon feeds and the one or more metal salts is in a range of about 10:1 to about 1:5.

### Claim 19 (depends on 18)

The method of claim 18, wherein the weight ratio of the one or more low fixed carbon feeds and the one or more metal salts is about 1:2.

### Claim 20 (depends on 15)

The method of claim 15, wherein the mixture is heated at a temperature of about 600 to about 700° C. in the inert atmosphere.