# US 2026/0182316 A1 · Method for stressing the box by creep

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0182316 A1
- Document ID: US20260182316A1
- Status: Published application
- Kind: A1
- Application number: 19/426,178
- Filed: 2025-12-19
- Published: 2026-06-25
- Earliest claimed: 2024-12-23
- Assignees: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Applicants: Commissariat A L'energie Atomique Et Aux Energies Alternatives
- Inventors: Sylvie JARJAYES; Claire FENOUILLET-BERANGER
- Web page: https://patentgrep.com/patent/US20260182316A1

## CPC

- H10D 30/796: {having memorised stress for introducing strain in the channel regions, e.g. recrystallised polysilicon gates}
- H10P 95/40: Treatments of semiconductor bodies to modify their internal properties, e.g. to produce internal imperfections
- H10D 30/798: {being provided in or under the channel regions}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/061: {using SOI processes together with lateral isolation, e.g. combinations of SOI and shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Aspects of the present disclosure provide a method for fabricating a device with strained semiconductor regions, including coating a semiconductor layer of a substrate of the semiconductor on insulator type with a stressing layer made of an amorphous material having a tensile intrinsic strain, forming, in the stressing layer, at least one opening facing a first semiconductor region of said semiconductor layer, and carrying out a creep annealing according to a duration and a temperature adapted to allow the creep of the insulating layer of the substrate and tension the first semiconductor region.

## Claims

### Claim at position 1

1-14. (canceled)

### Claim 15

A method for modifying a strain state of at least one semiconductor region of a semiconductor device, the method comprising:
coating a surface semiconductor layer of a semiconductor-on-insulator substrate with a stressing layer, the substrate including a support layer, an insulating layer on the support layer, and the surface semiconductor layer on the insulating layer, the surface semiconductor layer including isolation trenches filled with insulating material and arranged on opposite sides of an active semiconductor zone including a first semiconductor region;
forming, in the stressing layer, at least one opening extending through the stressing layer and facing the first semiconductor region while preserving at least one portion of the stressing layer on and facing a part of the substrate that is disposed against and in contact with the first semiconductor region; and
performing a creep annealing for a duration and at a temperature sufficient to allow creep of the insulating layer and relaxation of the preserved portion of the stressing layer so as to modify the strain state of the first semiconductor region.

### Claim 16 (depends on 15)

The method of claim 15, wherein the opening facing the first semiconductor region is centered between a first isolation trench and a second isolation trench disposed on opposite sides of the first semiconductor region.

### Claim 17 (depends on 15)

The method of claim 15, wherein the part of the substrate facing the preserved portion of the stressing layer is a second semiconductor region disposed against and in contact with the first semiconductor region, and wherein the opening is formed to preserve an additional portion of the stressing layer facing at least a third semiconductor region disposed against and in contact with the first semiconductor region, the preserved portion and the additional portion being arranged on opposite sides of the opening, and the second semiconductor region and the third semiconductor region being disposed on opposite sides of the first semiconductor region.

### Claim 18 (depends on 17)

The method of claim 17, wherein the stressing layer is under tensile strain, and wherein the creep annealing causes compression of the second semiconductor region and the third semiconductor region so as to place the first semiconductor region under tensile strain.

### Claim 19 (depends on 15)

The method of claim 15, wherein the first semiconductor region is part of an active semiconductor zone configured for at least one N-type transistor, and wherein the opening is formed to preserve a portion of the stressing layer facing another active semiconductor zone configured for one or more P-type transistors.

### Claim 20 (depends on 15)

The method of claim 15, further comprising, after forming the opening and before performing the creep annealing, depositing a second stressing layer on the stressing layer and on the first semiconductor region.

### Claim 21 (depends on 15)

The method of claim 15, further comprising forming a second opening through the stressing layer to expose another semiconductor region of the surface semiconductor layer, the opening and the second opening having different respective dimensions.

### Claim 22 (depends on 15)

The method of claim 15, wherein, prior to the creep annealing, a portion of the substrate is coated with a second stressing layer that is different from the stressing layer and/or has a thickness different from that of the stressing layer, and wherein the method further comprises, prior to the creep annealing, forming at least one opening in the second stressing layer to expose another semiconductor region of the surface semiconductor layer.

### Claim 23 (depends on 15)

The method of claim 15, wherein the stressing layer comprises silicon nitride under tensile strain.

### Claim 24 (depends on 15)

The method of claim 15, wherein the stressing layer has a thickness between 20 nm and 100 nm.

### Claim 25 (depends on 15)

The method of claim 15, wherein the creep annealing is performed at a temperature between 900° C. and 1200° C. for a duration between 1 minute and 30 minutes.

### Claim 26 (depends on 15)

The method of claim 15, wherein the first semiconductor region comprises silicon, and wherein at least one other semiconductor region of the substrate coated by the stressing layer comprises SixGe1-x, with 0<x<1.

### Claim 27 (depends on 26)

The method of claim 26, wherein the at least one other semiconductor region is a germanium-enriched region of the surface semiconductor layer, the surface semiconductor layer comprising silicon, and wherein the method further comprises, before coating the surface semiconductor layer with the stressing layer:
forming a silicon-germanium block on the at least one other semiconductor region; and
thermally oxidizing the silicon-germanium block and the surface semiconductor layer to enrich the at least one other semiconductor region with germanium.

### Claim 28 (depends on 15)

A method for manufacturing a semiconductor device including transistors, the method comprising:
performing the method of claim 15;
removing the stressing layer after the creep annealing; and
after removing the stressing layer, forming at least one transistor in the first semiconductor region and at least one additional transistor in another semiconductor region of the surface semiconductor layer.