# US 2026/0182265 A1 · Large-area semiconductor device realized through a single domain and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0182265 A1
- Document ID: US20260182265A1
- Status: Published application
- Kind: A1
- Application number: 19/181,289
- Filed: 2025-04-16
- Published: 2026-06-25
- Earliest claimed: 2024-12-19
- Assignees: Myongji University Industry and Academia Cooperation Foundation
- Applicants: Myongji University Industry and Academia Cooperation Foundation
- Inventors: Min Woo KIM; Nu Ri KIM; Se Won YOON
- Web page: https://patentgrep.com/patent/US20260182265A1

## CPC

- H10P 14/3436: {being chalcogenide semiconductor materials not being oxides, e.g. ternary compounds}
- H10D 62/883: {Transition metal dichalcogenides, e.g. MoSe2}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/271: {characterised by the preparation of substrate for selective deposition}
- H10P 14/272: {using mask materials other than SiO2 or SiN}
- H10P 14/276: {Lateral overgrowth}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3238: {being insulating materials}
- H10P 14/3402: {characterised by the chemical composition}
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A large-area semiconductor device through a single domain and a method of manufacturing the same are disclosed. The method comprises forming an absorption layer on a substrate, forming first sub semiconductor characteristic material layers on the absorption layer in spaces among first sub masks by using a first mask including the first sub masks, forming a second mask including second sub masks on the first sub semiconductor characteristic material layers and forming second sub semiconductor characteristic material layers in spaces among the second sub masks. Here, a large-area semiconductor characteristic material layer is formed on the absorption layer by the first sub semiconductor characteristic material layers and the second sub semiconductor characteristic material layers.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, the method comprising:
forming an absorption layer on a substrate;
forming first sub semiconductor characteristic material layers on the absorption layer in spaces among first sub masks by using a first mask including the first sub masks;
forming a second mask including second sub masks on the first sub semiconductor characteristic material layers; and
forming second sub semiconductor characteristic material layers in spaces among the second sub masks,
wherein a large-area semiconductor characteristic material layer is formed on the absorption layer by the first sub semiconductor characteristic material layers and the second sub semiconductor characteristic material layers.

### Claim 2 (depends on 1)

The method of claim 1, wherein the absorption layer is formed of single crystal aluminum oxide Al2O3 or amorphous Hafnium Dioxide HfO2, each of the sub masks is formed of Silicon Dioxide SiO2, and each of the sub semiconductor characteristic material layers is formed of Molybdenum disulfide MoS2 or Tungsten Diselenide WSe2.

### Claim 3 (depends on 1)

The method of claim 1, wherein bond energy between semiconductor characteristic material of the sub semiconductor characteristic material layers and material of the absorption layer is −0.2 eV/Å2 or less.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first sub masks are partially contacted one another while the first sub masks have triangular shape, the spaces formed by the first sub masks have triangular shape, the second sub masks are partially contacted one another while the second sub masks have triangular shape, and the spaces formed by the second sub masks have triangular shape,
and wherein the first sub masks, the spaces and the second sub masks be equilateral triangles, and one side of the equilateral triangle has a length of 100 nm to 1 μm.

### Claim 5 (depends on 1)

The method of claim 1, wherein only one precursor is grown in each of the spaces formed by the first sub masks and the spaces formed by the second sub masks.

### Claim 6 (depends on 5)

The method of claim 5, wherein the forming the first sub semiconductor characteristic material layers includes:
forming the first sub masks disposed sequentially with triangular shape on the absorption layer;
depositing a semiconductor characteristic material precursor on a structure where the first sub masks are formed;
forming the first sub semiconductor characteristic material layers by growing the semiconductor characteristic material precursor in the spaces formed by the first sub masks; and
removing the first sub masks.

### Claim 7 (depends on 5)

The method of claim 5, wherein the forming the second sub semiconductor characteristic material layers includes:
depositing a semiconductor characteristic material precursor on a structure where the second sub masks are formed;
forming the second sub semiconductor characteristic material layers by growing the semiconductor characteristic material precursor in the spaces formed by the second sub masks; and
removing the second sub masks.

### Claim 8

A semiconductor device comprising:
a substrate;
an absorption layer formed on the substrate; and
a semiconductor characteristic material layer formed on the absorption layer,
wherein bond energy between material of the absorption layer and semiconductor characteristic material of the semiconductor characteristic material layer is −0.2 eV/Å2 or less.

### Claim 9 (depends on 8)

The semiconductor device of claim 8, wherein the substrate is a silicon substrate, the absorption layer is formed of single crystal aluminum oxide Al2O3 or amorphous Hafnium Dioxide HfO2, and the semiconductor characteristic material layer is formed of Molybdenum disulfide MoS2 or Tungsten Diselenide WSe2.

### Claim 10 (depends on 8)

The semiconductor device of claim 8, wherein the bond energy between the material of the absorption layer and the semiconductor characteristic material of the semiconductor characteristic material layer is −0.2 eV/Å2 to −0.5 eV/Å2.

### Claim 11

A semiconductor device comprising:
a substrate;
an absorption layer formed on the substrate; and
a semiconductor characteristic material layer formed on the absorption layer,
wherein the semiconductor characteristic material layer is formed by disposing sequentially sub semiconductor characteristic material layers on the absorption layer, and
each of the sub semiconductor characteristic material layers has triangular shape.

### Claim 12 (depends on 11)

The semiconductor device of claim 11, wherein the triangular shape is an equilateral triangle, and one side of the equilateral triangle has a length of 100 nm to 1 μm.

### Claim 13 (depends on 11)

The semiconductor device of claim 11, wherein the substrate is a silicon substrate, the absorption layer is formed of single crystal aluminum oxide Al2O3 or amorphous Hafnium Dioxide HfO2, and the semiconductor characteristic material layer is formed of Molybdenum disulfide MoS2 or Tungsten Diselenide WSe2.

### Claim 14 (depends on 11)

The semiconductor device of claim 11, wherein each of the sub semiconductor characteristic material layers is triangles, and
a part of the sub semiconductor characteristic material layers is disposed in a reverse direction.

### Claim 15

A semiconductor device comprising:
a substrate;
an absorption layer formed on the substrate; and
a semiconductor characteristic material layer formed on the absorption layer,
wherein the semiconductor characteristic material layer is formed by disposing sequentially sub semiconductor characteristic material layers on the absorption layer, and each of the sub semiconductor characteristic material layers is formed by growing one precursor.

### Claim 16 (depends on 15)

The semiconductor device of claim 15, wherein the absorption layer is formed of single crystal aluminum oxide Al2O3 or amorphous Hafnium Dioxide HfO2, and the semiconductor characteristic material layer is formed of Molybdenum disulfide MoS2 or Tungsten Diselenide WSe2.