# US 2026/0176727 A1 · Ultra-high strength sheet having excellent hole expansion ratio, and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0176727 A1
- Document ID: US20260176727A1
- Status: Published application
- Kind: A1
- Application number: 19/127,686
- Filed: 2023-11-28
- Published: 2026-06-25
- Earliest claimed: 2022-11-29
- Assignees: Posco
- Applicants: Posco Co., Ltd.
- Inventors: Sang-Ho Han; Jong-Pan Kong; Eun-Young Kim; Chan-Woo Bang
- Web page: https://patentgrep.com/patent/US20260176727A1

## CPC

- C22C 38/02: containing silicon
- C22C 38/26: with niobium or tantalum
- B32B 15/013: {one layer being formed of an iron alloy or steel, another layer being formed of a metal other than iron or aluminium}
- C21D 1/19: by interrupted quenching
- C21D 1/26: Methods of annealing
- C21D 1/76: Adjusting the composition of the atmosphere
- C21D 8/0426: {Hot rolling}
- C21D 8/0436: {Cold rolling}
- C21D 8/0463: {following hot rolling}
- C21D 8/0473: {Final recrystallisation annealing}
- C21D 9/46: for sheet metals
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/04: containing manganese
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/32: with boron
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/44: with molybdenum or tungsten
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C21D 2211/002: Bainite
- C21D 2211/003: Cementite
- C21D 2211/005: Ferrite
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

The present invention pertains to a steel sheet used in automobiles etc. and, more specifically, to an ultra-high strength steel sheet having an excellent hole expansion ratio, and a method for manufacturing same.

## Claims

### Claim 1

A steel sheet including by weight %:
0.1 to 0.3% of carbon (C), 0.5% or less (excluding 0%) of silicon (Si), 1.0 to 3.0% of manganese (Mn), 0.0005 to 0.003% of boron (B), 0.01% or less (excluding 0%) of phosphorus (P), 0.01% or less (excluding 0%) of sulfur(S), 0.01% or less (excluding 0%) of nitrogen (N), 0.01 to 0.1% of aluminum (Al), with a remainder of Fe and other inevitable impurities,
wherein an average area fraction of cementite precipitates present in at least one grain boundary selected from the group consisting of ferrite and bainite within 10 μm from a surface thereof is 60% or less (excluding 0%), compared to an area of cementite precipitates present in the grain boundary of martensite at a point ¼t from the surface, where t is a total thickness of the steel sheet.

### Claim 2 (depends on 1)

The steel sheet of claim 1, further comprising by weight %: at least one selected from the group consisting of 0.2% or less (excluding 0%) of chromium (Cr), 0.01 to 0.1% of molybdenum (Mo), 0.01 to 0.05% of niobium (Nb), 0.01 to 0.05% of titanium (Ti), and 0.001 to 0.1% of antimony (Sb).

### Claim 3 (depends on 1)

The steel sheet of claim 1, wherein an average area fraction of at least one selected from the group consisting of ferrite and bainite within 30 μm from the surface is 15 to 60%.

### Claim 4 (depends on 1)

The steel sheet of claim 1, wherein an average area fraction of at least one selected from the group consisting of ferrite and bainite within 10 μm from the surface is 50 to 80%.

### Claim 5 (depends on 1)

The steel sheet of claim 1, further comprising:
a zinc-based plating layer on the surface of the steel sheet.

### Claim 6

A method for manufacturing a steel sheet comprising:
reheating a steel slab including by weight %, 0.1 to 0.3% of carbon (C), 0.5% or less (excluding 0%) of silicon (Si), 1.0 to 3.0% of manganese (Mn), 0.0005 to 0.003% of boron (B), 0.01% or less (excluding 0%) of phosphorus (P), 0.01% or less (excluding 0%) of sulfur(S), 0.01% or less (excluding 0%) of nitrogen (N), 0.01 to 0.1% of aluminum (Al), with a remainder of Fe and other inevitable impurities, at a temperature within a range of 1100 to 1300° C.;
hot rolling the reheated slab to manufacture a hot-rolled steel sheet;
coiling the hot-rolled steel sheet at a temperature within a range of 400 to 600° C.;
cold rolling the coiled hot-rolled steel sheet at a reduction ratio of 30 to 80%;
annealing the cold-rolled steel sheet by heat treatment at a temperature within a range of Ac3+10° C. to Ac3+80° C.,
wherein in the annealing operation, a dew point temperature is controlled to be −40° C. or lower at a temperature of Ac3+10° C. or lower, and a dew point temperature is controlled to be from −30° C. to +30° C. at a temperature within a range of Ac3+10° C. to Ac3+80° C.

### Claim 7 (depends on 6)

The method for manufacturing a steel sheet of claim 6, wherein in the annealing operation, a heat treatment is performed at a temperature within a range of Ac3+10° C. to Ac3+80° C. for 30 seconds or longer.

### Claim 8 (depends on 6)

The method for manufacturing a steel sheet of claim 6, further comprising:
primarily cooling the annealed steel sheet to a temperature within a range of 680 to 750° C., which is a primary cooling end temperature range, at an average cooling rate of 10° C./s or less.

### Claim 9 (depends on 8)

The method for manufacturing a steel sheet of claim 8, further comprising:
secondarily cooling the primarily-cooled steel sheet to a temperature within a range of 100° C. to Mf at an average cooling rate of 60 to 160° C./s.

### Claim 10 (depends on 9)

The method for manufacturing a steel sheet of claim 9, further comprising:
reheating and over-aging the secondarily-cooled steel sheet by heat treatment to a temperature within a range of 150 to 240° C.

### Claim 11 (depends on 10)

The method for manufacturing a steel sheet of claim 10, wherein the over-aging heat treatment operation is performed for 200 to 1000 seconds.

### Claim 12 (depends on 6)

The method for manufacturing a steel sheet of claim 6, wherein the steel slab further includes by weight %: at least one selected from the group consisting of 0.2% or less (excluding 0%) of chromium (Cr), 0.01 to 0.1% of molybdenum (Mo), 0.01 to 0.05% of niobium (Nb), 0.01 to 0.05% of titanium (Ti), and 0.001 to 0.1% of antimony (Sb).