# US 2026/0176456 A1 · Compositon for automotive exterior parts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0176456 A1
- Document ID: US20260176456A1
- Status: Published application
- Kind: A1
- Application number: 19/126,078
- Filed: 2023-10-31
- Published: 2026-06-25
- Earliest claimed: 2022-10-31
- Assignees: Borealis AG
- Applicants: Borealis AG
- Inventors: Claudia KNIESEL; Angelica Maëlle Delphine LEGRAS; Jingbo WANG; Pauli LESKINEN; Markus GAHLEITNER; Klaus BERNREITNER
- Web page: https://patentgrep.com/patent/US20260176456A1

## CPC

- C08L 23/16: Ethylene-propylene or ethylene-propylene-diene copolymers
- B29B 7/007: {for continuous mixing}
- B29B 7/726: {Measuring properties of mixture, e.g. temperature or density (B29B7/724 takes precedence)}
- B29B 7/90: Fillers or reinforcements {, e.g. fibres}
- C08F 2/001: {Multistage polymerisation processes characterised by a change in reactor conditions without deactivating the intermediate polymer (C08F295/00, C08F297/00 take precedence)}
- C08F 4/6465: {containing silicium}
- C08F 210/06: Propene
- C08L 23/06: Polyethylene
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08L 23/12: Polypropene
- C08L 23/14: Copolymers of propene (C08L23/16 takes precedence)
- B29B 7/48: with intermeshing devices, e.g. screws
- C08F 4/65912: {in combination with an organoaluminium compound}
- C08F 4/65916: {supported on a carrier, e.g. silica, MgCl2, polymer}
- C08F 2420/07: Heteroatom-substituted Cp, i.e. Cp or analog where at least one of the substituent of the Cp or analog ring is or contains a heteroatom
- C08F 2500/12: Melt flow index or melt flow ratio
- C08L 2207/02: Heterophasic composition
- C08L 2207/06: Properties of polyethylene
- C08L 2308/00: Chemical blending or stepwise polymerisation process with the same catalyst
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Composition for automotive exterior components, the composition comprising a) 30 to 45 wt.-%, based on the total weight of the composition, of a first heterophasic propylene copolymer (HECO1) having a melt flow rate MFR2 of 50 to 250 g/10 min determined according to ISO 1133 at 230° C. and 2.16 kg load, a soluble fraction (SF) content of 6 to 22 wt.-% based on the total weight of the first heterophasic propylene copolymer (HECO1) as determined according to the CRYSTEX method, and an ethylene content C2(SF) of 15 to 30 wt.-% based on the total weight of the soluble fraction (SF) of the heterophasic propylene copolymer (HECO1) as determined by Fourier transform infrared spectroscopy (FTIR) calibrated with 13C-NMR spectroscopy, b) 15 to 30 wt.-%, based on the total weight of the composition, of a second heterophasic propylene copolymer (HECO2) having an MFR2 of 5 to 15 g/10 min determined according to ISO 1133 at 230° C. and 2.16 kg load, a soluble fraction (SF) content of 25 to 45 wt.-% based on the second heterophasic propylene copolymer (HECO2) as determined according to the CRYSTEX method, and an ethylene content C2(SF) of more than 30 to 50 wt.-% based on the total weight of the soluble fraction (SF) of the heterophasic propylene copolymer (HECO2) as determined by Fourier transform infrared spectroscopy (FTIR) calibrated with 13C-NMR spectroscopy, c) 8 to 18 wt.-%, based on the total weight of the composition, of an ethylene copolymer having a density of 860 to 880 kg/m3 determined according to ISO 1183, and an MFR2 of 0.1 to 3.0 g/10 min determined according to ISO 1133 at 190° C. and 2.16 kg load, and d) 15 to 30 wt.-%, based on the total weight of the composition, of an inorganic filler.

## Claims

### Claim 1

Composition for automotive exterior components, the composition comprising
a) 30 to 45 wt.-%, based on the total weight of the composition, of a first heterophasic propylene copolymer (HECO1) having a melt flow rate MFR2 of 70 to 250 g/10 min determined according to ISO 1133 at 230° C. and 2.16 kg load,
a soluble fraction (SF) content of 6 to 22 wt.-% based on the total weight of the first heterophasic propylene copolymer (HECO1) as determined according to the CRYSTEX method, and
an ethylene content C2(SF) of 15 to 30 wt.-% based on the total weight of the soluble fraction (SF) of the heterophasic propylene copolymer (HECO1) as determined by Fourier transform infrared spectroscopy (FTIR) calibrated with 13C-NMR spectroscopy,
b) 15 to 30 wt.-%, based on the total weight of the composition, of a second heterophasic propylene copolymer (HECO2) having an MFR2 of 5 to 15 g/10 min determined according to ISO 1133 at 230° C. and 2.16 kg load,
a soluble fraction (SF) content of 25 to 45 wt.-% based on the second heterophasic propylene copolymer (HECO2) as determined according to the CRYSTEX method, and
an ethylene content C2(SF) of more than 30 to 50 wt.-% based on the total weight of the soluble fraction (SF) of the heterophasic propylene copolymer (HECO2) as determined by Fourier transform infrared spectroscopy (FTIR) calibrated with 13C-NMR spectroscopy,
c) 8 to 18 wt.-%, based on the total weight of the composition, of an ethylene copolymer having a density of 860 to 880 kg/m3 determined according to ISO 1183, and
an MFR2 of 0.1 to 3.0 g/10 min determined according to ISO 1133 at 190° C. and 2.16 kg load,
d) 15 to 30 wt.-%, based on the total weight of the composition, of an inorganic filler, wherein the composition has an MFR2 of 15 to 30 g/10 min determined according to ISO 1133 at 230° C. and 2.16 kg load.

### Claim 2 (depends on 1)

Composition according to claim 1, wherein the first heterophasic propylene copolymer (HECO1) has a melting temperature Tm in the range of 145 to 160° C. determined by differential scanning calorimetry (DSC) according to ISO 11357, and/or an intrinsic viscosity of the soluble fraction (IV(SF)) of 2.0 to 3.5 dl/g as determined in decalin according to ISO 1628-3.

### Claim 3 (depends on 1)

Composition according claim 1,
wherein the second heterophasic propylene copolymer (HECO2) has an intrinsic viscosity of the soluble fraction (IV(SF)) of 3.0 to 7.0 dl/g as determined in decalin according to ISO 1628-3 and/or
a melting temperature Tm in the range of 162 to 170° C. determined by differential scanning calorimetry (DSC) according to ISO 11357.

### Claim 4 (depends on 1)

Composition according claim 1,
wherein the ethylene copolymer is a copolymer of ethylene and an alpha-olefin having 3 to 10 carbon atoms, preferably 8 carbon atoms.

### Claim 5 (depends on 1)

Composition according claim 1, further comprising
e) 0.5 to 5.0 wt.-%, based on the total weight of the composition, of an additive.

### Claim 6 (depends on 5)

Composition according to claim 5, wherein the additive comprises one or more antioxidant(s), a UV stabilizer, an antistatic agent, an acid scavenger, a nucleating agent, carbon black or a mixture thereof.

### Claim 7 (depends on 1)

Composition according claim 1,
wherein the inorganic filler is selected from talc, wollastonite, kaolin, mica, clay or a mixture thereof, preferably the inorganic filler is talc.

### Claim 8 (depends on 1)

Composition according claim 1,
wherein the inorganic filler has a median particle size D50 of 5 to 20 μm.

### Claim 9 (depends on 1)

Composition according claim 1, further comprising
f) up to 3 wt.-%, based on the total weight of the composition, of a propylene homopolymer (PP-H).

### Claim 10 (depends on 9)

Composition according to claim 9, wherein the propylene homopolymer (PP-H) has an MFR2 of 1 to 100 g/10 min determined accordingto ISO 1133 at 230° C. and 2.16 kg load.

### Claim 11 (depends on 1)

Composition according claim 1,
wherein the first heterophasic propylene copolymer (HECO1) comprises a fraction soluble in cold xylene at 25° C. (XCS fraction) in an amount in the range of 6 to 22 wt.-%, based on the total weight of the first heterophasic propylene copolymer (HECO1), and/or wherein the first heterophasic propylene copolymer (HECO1) has a total ethylene content (C2 total) in the range of 1.8 to 6.5 wt.-% based on the total weight of the first heterophasic propylene copolymer (HECO1) as determined by Fourier transform infrared spectroscopy (FTIR) calibrated with 13C-NMR spectroscopy.

### Claim 12 (depends on 1)

Composition according claim 1,
wherein the composition has a flexural modulus in the range of 1750 to 2750 MPa determined according to ISO 178 on injection molded specimens.

### Claim 13 (depends on 1)

Composition according claim 1,
wherein the composition has a Charpy notched impact strength at 23° C. in the range of more than 30 to 75 kJ/m2 determined according to ISO 179/eA on injection molded specimens.

### Claim 14 (depends on 1)

Article comprising the composition according to claim 1, the article preferably being an automotive exterior component.

### Claim 15 (depends on 1)

A method for improving the adhesion of paint, the method comprising adding to the paint the composition of claim 1.