# US 2026/0176193 A1 · Break-resistant electrochemical sensor containing break-resistant membrane glass, method for manufacturing a break-resistant membrane glass for a glass component of a measuring half-cell, and method for manufacturing the break-resistant glass assembly of an ion-sensitive single-rod measuring chain

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0176193 A1
- Document ID: US20260176193A1
- Status: Published application
- Kind: A1
- Application number: 19/426,678
- Filed: 2025-12-19
- Published: 2026-06-25
- Earliest claimed: 2024-12-19
- Assignees: Endress+Hauser Conducta GmbH+Co. KG
- Applicants: Endress+Hauser Conducta GmbH+Co. KG
- Inventors: Matthäus Speck-Dechant
- Web page: https://patentgrep.com/patent/US20260176193A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03B 32/00: Thermal after-treatment of glass products not provided for in groups {C03B19/00} , C03B25/00 - C03B31/00 {or C03B37/00}, e.g. crystallisation, eliminating gas inclusions or other impurities; {Hot-pressing vitrified, non-porous, shaped glass products}
- C03C 4/18: for ion-sensitive glass
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- G01N 27/36: Glass electrodes
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A method for manufacturing a break-resistant membrane glass of a glass component of a measuring half-cell of an analyte-sensitive sensor includes providing at least one membrane glass of a sensor which is blown onto a shaft and which consists of a sodium-and lithium-containing glass, such as sodium and lithium silicate glass, or of a lithium-containing glass, such as lithium silicate glass, or which comprises one of these materials. The method further includes bringing the at least one membrane glass blown onto a shaft into contact with a pickling solution containing sodium ions, such as a sodium acetate or sodium nitrate solution or a melt containing sodium ions, and heating the membrane glass at a temperature of 200° C.-500° C. for 10-20 minutes, wherein the membrane glass is ion-sensitive.

## Claims

### Claim 1

A method for manufacturing a break-resistant membrane glass of a glass component of a measuring half-cell of an analyte-sensitive sensor, comprising:
providing at least one membrane glass of a sensor which is blown onto a shaft and which consists of a sodium-and lithium-containing glass;
bringing the at least one membrane glass blown onto a shaft into contact with a pickling solution containing sodium ions; and
heating the membrane glass at a temperature of 200° C.-500° C. for 10-20 minutes, wherein the membrane glass is ion-sensitive.

### Claim 2 (depends on 1)

The method of claim 1, wherein the pickling solution containing sodium ions further contains potassium ions.

### Claim 3 (depends on 1)

The method of claim 1, wherein the bringing into contact with a pickling solution step comprises immersing in the pickling solution or spraying with the pickling solution.

### Claim 4 (depends on 3)

The method of claim 3, wherein after immersion in the pickling solution or spraying with the pickling solution, the glass is heated with a laser.

### Claim 5 (depends on 1)

The method of claim 1, wherein at least the membrane glass is immersed in the melt.

### Claim 6 (depends on 5)

The method of claim 5, wherein the membrane glass is subsequently brought into contact with a pickling solution.

### Claim 7 (depends on 1)

The method of claim 1, wherein the ion-sensitive sensor is a cation-sensitive sensor.

### Claim 8 (depends on 7)

The method of claim 7, wherein the cation-sensitive sensor is a Na+, K+ sensor or a pH-sensitive or hydronium-ion-sensitive sensor.

### Claim 9 (depends on 1)

The method of claim 1, wherein the shaft consists of a sodium silicate glass hardened with potassium ions or contains a sodium silicate glass hardened with potassium ions.

### Claim 10 (depends on 1)

The method of claim 1, followed by the steps:
cooling the glass component containing a shaft and break-resistant membrane glass blown onto the shaft and integrally bonded to the glass component to room temperature; and
cleaning the glass component.

### Claim 11

A method for manufacturing a break-resistant glass assembly of an ion-sensitive single-rod measuring chain comprising hardened ion-sensitive membrane glass, comprising:
providing a glass body containing an inner shaft tube having a cylindrical cavity and an outer shaft tube surrounding the inner shaft tube and integrally bonded to the inner shaft tube and closed at the bottom;
inserting a cylindrical diaphragm into a receptacle of the inner shaft tube, the diaphragm containing an O-ring on the outer surface for sealing with the inner shaft tube;
manufacturing a break-resistant membrane glass of a glass component of a measuring half-cell manufacturing a break-resistant membrane glass of a glass component of a measuring half-cell of an analyte-sensitive sensor, by:
providing at least one membrane glass of a sensor which is blown onto a shaft and which consists of a sodium-and lithium-containing glass;
bringing the at least one membrane glass blown onto a shaft into contact with a pickling solution containing sodium ions; and
heating the membrane glass at a temperature of 200° C.-500° C. for 10-20 minutes, wherein the membrane glass is ion-sensitive; and
inserting the glass component of a measuring half-cell, containing a shaft tube and a pH-sensitive glass membrane integrally bonded to the shaft tube, into the cylindrical cavity.

### Claim 12

A glass assembly of a single-rod measuring chain for an analyte-sensitive sensor, comprising:
an inner shaft tube having a cylindrical cavity;
an outer shaft tube surrounding the inner shaft tube and integrally bonded to the inner shaft tube and closed at the bottom; and
a break-resistant ion-sensitive membrane glass blown onto the shaft tube, wherein the break-resistant ion-sensitive membrane glass comprises or consists of lithium ion silicate glass, wherein at least a portion of the lithium ions are replaced with sodium ions.

### Claim 13 (depends on 12)

The glass assembly of claim 12, wherein the break-resistant ion-sensitive membrane glass is obtained by:
providing at least one membrane glass of a sensor which is blown onto a shaft and which consists of a sodium-and lithium-containing glass;
bringing the at least one membrane glass blown onto a shaft into contact with a pickling solution containing sodium ions; and
heating the membrane glass at a temperature of 200° C.-500° C. for 10-20 minutes, wherein the membrane glass is ion-sensitive.

### Claim 14

A break-resistant electrochemical sensor comprising:
a glass assembly including:
an inner shaft tube having a cylindrical cavity;
an outer shaft tube surrounding the inner shaft tube and integrally bonded to the inner shaft tube and closed at the bottom; and
a break-resistant ion-sensitive membrane glass blown onto the shaft tube, wherein the break-resistant ion-sensitive membrane glass comprises or consists of lithium ion silicate glass, wherein at least a portion of the lithium ions are replaced with sodium ions;
a measuring half-cell and a reference half-cell, in each case comprising a lead and an electrolyte; and
an electronics unit, which is electrically connected to the lead of the measuring half-cell and the lead of the reference half-cell.