# US 2026/0175468 A1 · Manufacturing a wood composite panel comprising soy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0175468 A1
- Document ID: US20260175468A1
- Status: Published application
- Kind: A1
- Application number: 19/128,756
- Filed: 2022-11-11
- Published: 2026-06-25
- Earliest claimed: 2022-11-11
- Assignees: Lignum Technologies AG
- Applicants: Lignum Technologies AG
- Inventors: Christian Felipe SCHWEITZER; Justin Russell HEIM
- Web page: https://patentgrep.com/patent/US20260175468A1

## CPC

- B27N 1/0209: {Methods, e.g. characterised by the composition of the agent}
- B01F 25/52: with a rotary stirrer in the recirculation tube
- B27N 1/00: Pretreatment of moulding material
- B27N 1/02: Mixing the material with binding agent (mixing in general B01F)
- B27N 1/029: {Feeding; Proportioning; Controlling}
- B27N 3/002: {characterised by the type of binder (compositions of macromolecular compounds C08L)}
- B27N 3/04: from fibres
- B27N 3/12: from fibres
- B27N 3/18: Auxiliary operations, e.g. preheating, humidifying, cutting-off
- B27N 3/203: {with heating or cooling means}
- B27N 3/08: Moulding or pressing (presses in general B30B)
- B27N 3/24: characterised by using continuously acting presses having endless belts or chains moved within the compression zone
- B27N: MANUFACTURE BY DRY PROCESSES OF ARTICLES, WITH OR WITHOUT ORGANIC BINDING AGENTS, MADE FROM PARTICLES OR FIBRES CONSISTING OF WOOD OR OTHER LIGNOCELLULOSIC OR LIKE ORGANIC MATERIAL (containing cementitious material B28B; shaping of substances in a plastic state B29C; fibreboards made from fibrous suspensions D21J; drying F26B17/00)
- B01F: MIXING, e.g. DISSOLVING, EMULSIFYING OR DISPERSING (mixing paints B44D3/06)

## Abstract

A method for manufacturing a wood composite panel, in particular an MDF-panel, comprises the following steps: a. providing and mixing soy flour and water in a weight ratio of about 10 to 45% to form a soy solution; b. introducing the soy solution to a high-pressure blow line containing wood fibers; c. introducing resin to the high-pressure blow line to form a soy solution wood fiber resin mixture; d. pre-drying the soy solution wood fiber resin mixture to form a pre-dried soy flour wood fiber resin mixture; and e. hot-pressing the pre-dried soy flour wood fiber resin mixture into the wood composite panel.

## Claims

### Claim 1

A method for manufacturing a wood composite panel, in particular an MDF-panel, comprising the following steps:
a. providing and mixing soy flour and water in a weight ratio of about 10 to 45% to form a soy solution;
b. introducing the soy solution to a high-pressure blow line containing wood fibers;
c. introducing resin to the high-pressure blow line to form a soy solution wood fiber resin mixture;
d. pre-drying the soy solution wood fiber resin mixture to form a pre-dried soy flour wood fiber resin mixture; and
e. hot-pressing the pre-dried soy flour wood fiber resin mixture into the wood composite panel.

### Claim 2 (depends on 1)

The method according to claim 1, wherein soy flour and water are mixed in step a. in a weight ratio of about 12.5 to 35% and preferably in a weight ratio of about 15 to 30% to form a soy solution.

### Claim 3 (depends on 1)

The method according to claim 1, wherein between steps d. and e., an additional step of forming the pre-dried soy flour wood fiber resin mixture into mats is provided, wherein the mats are then hot-pressed in the next step.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the mixing in step a. comprises a recirculation step, wherein the soy solution is recirculated for about 2 to 180 minutes, preferably about 5 to 120 minutes and most preferably about 10 to 60 minutes to obtain a consistent soy solution.

### Claim 5 (depends on 1)

The method according to claim 1, the high-pressure blow line provides a pressure of about 0.2 to 0.8 MPa, preferably about 0.3 to 0.7 MPa and most preferably about 0.4 to 0.6 MPa.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the high-pressure blow line provides a temperature of about 100° C. to 200° C., preferably about 130° C. to 180° C. and most preferably about 150° C. to 165° C.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the resin is a synthetic resin, preferably a PMDI resin.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the soy solution wood resin mixture obtained in step c. has a moisture content of about 40 to 90%, preferably about 50 to 80% and most preferably about 70%.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the pre-dried soy flour wood fiber resin mixture obtained in step d. has a moisture content of about 5 to 30%, preferably about 7 to 20% and most preferably about 10%.

### Claim 10 (depends on 4)

The method according to claim 4, wherein the recirculation step and the soy solution injection step are performed simultaneously.

### Claim 11 (depends on 1)

A wood composite panel obtainable by the method according to claim 1, wherein the panel comprises at least about 0.1 to 3.0% by weight of soy, preferably about 0.2 to 1.2% by weight of soy and most preferably about 0.4 to 0.8% by weight of soy.

### Claim 12

A system for manufacturing a wood composite panel, in particular an MDF-panel, wherein the system comprises:
a mixing means for mixing water with soy flour powder to form a soy solution,
a high-pressure blow line connected to the mixing means, comprising:
a wood fiber port for introducing wood fibers to the high-pressure blow line,
a soy solution port for introducing the soy solution to the high-pressure blow line, and
a resin port for introducing resin to the high-pressure blow line to form a soy solution wood fiber resin mixture,
wherein the system further comprises a dryer arranged downstream of the high-pressure blow line for pre-drying the soy solution wood resin mixture to obtain a pre-dried soy flour wood fiber resin mixture, and
a press for hot-pressing the pre-dried soy flour wood fiber resin mixture to form the wood composite panel.

### Claim 13 (depends on 1)

The system according to claim 1, wherein the system further comprises a mat forming means for forming the pre-dried soy solution wood resin mixture into mats before pressing.

### Claim 14 (depends on 1)

The system according to claim 1, wherein the mixing means comprises:
a soy solution preparation tank having an inlet and an outlet, and
a mixer, preferably a high shear mixer, comprising an inlet and an outlet,
wherein the mixer inlet is connected to the soy solution preparation tank outlet to receive water or soy solution from the soy solution preparation tank, and
wherein the mixer outlet is connected to the soy solution preparation tank inlet via a recirculation path to allow a recirculation of the water or soy solution.

### Claim 15 (depends on 1)

The system according claim 1, wherein the system further comprises a soy solution feed tank, which is adapted to receive the soy solution from the soy solution preparation tank, and which is further adapted to transmit the soy solution to the high-pressure blow line, preferably via a pump arranged between the soy solution feed tank and the high-pressure blow line.