# US 2026/0175467 A1 · Modified wood and transparent wood composites, and systems and methods for forming and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0175467 A1
- Document ID: US20260175467A1
- Status: Published application
- Kind: A1
- Application number: 19/538,941
- Filed: 2026-02-12
- Published: 2026-06-25
- Earliest claimed: 2020-07-10
- Assignees: University of Maryland, College Park
- Applicants: University of Maryland, College Park
- Inventors: Liangbing HU; Ruiyu MI; Qinqin XIA; Chaoji CHEN; Tian LI
- Web page: https://patentgrep.com/patent/US20260175467A1

## CPC

- B27K 3/15: Impregnating involving polymerisation {including use of polymer-containing impregnating agents (macromolecular compounds derived from lignocellulosic materials C08H; compositions of lignin-containing materials C08L97/02)}
- B27K 3/0221: {Pore opening (B27K3/0214 takes precedence)}
- B27K 3/16: Inorganic impregnating agents
- B27K 2240/10: Extraction of components naturally occurring in wood, cork, straw, cane or reed
- B27K: PROCESSES, APPARATUS OR SELECTION OF SUBSTANCES FOR IMPREGNATING, STAINING, DYEING, BLEACHING OF WOOD OR SIMILAR MATERIALS, OR TREATING OF WOOD OR SIMILAR MATERIALS WITH PERMEANT LIQUIDS, NOT OTHERWISE PROVIDED FOR (applying liquids or other fluent materials to surfaces in general B05; coating wood or similar material B44D); CHEMICAL OR PHYSICAL TREATMENT OF CORK, CANE, REED, STRAW OR SIMILAR MATERIALS

## Abstract

A material can comprise a contiguous block of chemically-modified wood infiltrated with an index-matching polymer. The contiguous block has a first section that is substantially transparent to light and a second section that is translucent or opaque. The first section can have a lower lignin content than the second section. Alternatively, the first section can have a chromophore state altered from that of the wood in its natural state, and the lignin in the second section can retain a chromophore state of the wood in its natural state. In some embodiments, a material comprises a section of wood chemically-modified such that chromophores of lignin within the wood in its natural state are altered or removed, and the section retains at least 70% of the lignin of the wood in its natural state. Methods for forming such materials are also disclosed.

## Claims

### Claim 1

A material comprising:
a contiguous block of chemically-modified wood infiltrated with polymer, the chemically-modified wood retaining a cellulose-based microstructure of the wood in its natural state, the polymer having a refractive index substantially matching a refractive index of cellulose and filling open spaces within the microstructure,
wherein the contiguous block has a first section and a second section adjacent to the first section,
a lignin content of the first section is less than or equal to 3 wt %, and
a lignin content of the second section is greater than or equal to 7.5 wt %.

### Claim 2 (depends on 1)

The material of claim 1, wherein the lignin content of the first section is less than or equal to 1 wt %, and the lignin content of the second section is greater than or equal to 12.5 wt %.

### Claim 3 (depends on 1)

The material of claim 1, wherein:
the cellulose-based microstructure has lumina defined by cell walls, the lumina extending along a longitudinal growth direction of the wood in its natural state, cellulose nanofibers forming the cell walls also extending along the longitudinal growth direction and substantially perpendicular to a radial direction of the wood it is natural state; and
a tensile strength of the contiguous block substantially along the radial direction is at least 20 MPa.

### Claim 4 (depends on 1)

The material of claim 1, wherein the polymer comprises epoxy resin.

### Claim 5

A material comprising:
a section of wood chemically-modified such that chromophores of lignin within the wood in its natural state are altered or removed while otherwise retaining a cellulose-based microstructure of the wood in its natural state; and
a polymer infiltrating the cellulose-based microstructure of the chemically-modified section of wood,
wherein the polymer has a refractive index substantially matching a refractive index of cellulose and fills open spaces within the microstructure, and
the section is substantially transparent to light having a wavelength of 600 nm.

### Claim 6 (depends on 5)

The material of claim 5, wherein a lignin content of the section is at least 15 wt %.

### Claim 7 (depends on 5)

The material of claim 5, wherein said section comprises an entirety of a contiguous block of wood.

### Claim 8 (depends on 5)

The material of claim 5, wherein:
said section comprises a first section of a contiguous block of wood;
the material comprises a second section of the contiguous block of wood adjacent to the first section; and
the lignin in the second section retains a chromophore state of the wood in its natural state.

### Claim 9 (depends on 8)

The material of claim 8, wherein the first section has a transmittance of at least 80% for the light at the wavelength of 600 nm, and the second section has a transmittance of less than 36% for the light at the wavelength of 600 nm.

### Claim 10 (depends on 5)

The material of claim 5, wherein the section has a transmittance of at least 80% and a haze of at least 50% for the light at the wavelength of 600 nm.

### Claim 11

A method comprising:
applying a first volume of a liquid oxidation agent to an external surface of a section of a contiguous block of wood; and
during or after the applying, exposing the section of the contiguous block of wood to ultra-violet (UV) radiation,
wherein chromophores of lignin within said section are chemically oxidized and removed in situ by the UV exposure in the presence of the liquid oxidation agent, and
after the exposing, a cellulose-based microstructure of the wood and at least 70% of the lignin in said section prior to the applying are retained.

### Claim 12 (depends on 11)

The method of claim 11, wherein the liquid oxidation agent comprises a solution of hydrogen peroxide (H2O2).

### Claim 13 (depends on 11)

The method of claim 11, wherein, after the exposing, a lignin content of the section is at least 15 wt %.

### Claim 14 (depends on 11)

The method of claim 11, prior to or concurrent with the applying, applying a second volume of an alkali to the external surface of the section of contiguous block of wood.

### Claim 15 (depends on 11)

The method of claim 11, wherein the applying comprises direct application to the external surface without immersing the contiguous block, and the direct application comprises brushing, spraying, rolling, or any combination thereof.

### Claim 16 (depends on 11)

The method of claim 11, wherein:
the applying comprises applying the first volume to the external surface in a predetermined pattern without applying any liquid oxidation agent to a second section of the contiguous wood block adjacent to said section; and
after the exposing, the second section has a lignin content greater than a lignin content of the section.

### Claim 17 (depends on 16)

The method of claim 16, further comprising, prior to the applying, defining a boundary of the predetermined pattern by disposing a hydrophobic material on the external surface.

### Claim 18 (depends on 11)

The method of claim 11, wherein the exposing comprises using a mask with predetermined pattern to illuminate the section without illuminating a second section of the contiguous wood block adjacent to said section.

### Claim 19 (depends on 11)

The method of claim 11, further comprising:
after the exposing, infiltrating the contiguous block with a polymer so as to fill open spaces within the retained cellulose-based microstructure of the section, the polymer having a refractive index substantially matching a refractive index of cellulose,
wherein, after the infiltrating, the section is substantially transparent to light having a wavelength of 600 nm.

### Claim 20 (depends on 19)

The method of claim 19, wherein the infiltrating comprises:
immersing the contiguous block within a liquid polymer or polymer precursor;
applying a vacuum to cause the liquid polymer or polymer precursor to flow into the cellulose-based microstructure; and
drying the liquid polymer or polymerizing the precursor to form a solid polymer in situ within the microstructure of the contiguous block.