# US 2026/0171530 A1 · Aluminium composite material and process of preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0171530 A1
- Document ID: US20260171530A1
- Status: Published application
- Kind: A1
- Application number: 19/122,770
- Filed: 2023-10-31
- Published: 2026-06-18
- Earliest claimed: 2022-11-03
- Assignees: BASF SE
- Applicants: BASF SE
- Inventors: Marc DUCHARDT; Tobias UHLIG; Birgit GERKE; Karl HOELEMANN; Wolfgang ROHDE; Regina VOGELSANG; Wolfram WILK; Kerstin SCHIERLE-ARNDT; Nils-Olof Joachim BORN; Andreas Michael KERN; Sven HILDEBRANDT; Fabian SEELER; Anne-Marie Caroline ZIESCHANG
- Web page: https://patentgrep.com/patent/US20260171530A1

## CPC

- C22B 1/005: {Preliminary treatment of scrap (C22B1/02 - C22B1/26 take precedence)}
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- C22B 1/02: Roasting processes (C22B1/16 takes precedence)
- C22B 1/24: Binding; Briquetting {; Granulating}
- C22B 7/002: {by treating with halogens, sulfur or compounds thereof; by carburising, by treating with hydrogen (hydriding)}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02W 30/84: Recycling of batteries or fuel cells
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Disclosed herein are aluminum composite materials and methods of preparing the same. The aluminum composite materials are useful intermediates in the recycling of lithium ion batteries. For example, some materials may be easily leached to obtain one or more value metals.

## Claims

### Claim 1

An aluminum composite material comprising from 1 wt.-% to 80 wt.-% aluminum, from 1 wt.-% to 20 wt.-% manganese, from 1 wt.-% to 20 wt.-% cobalt, and from 0 wt.-% to 50 wt.-% nickel; wherein each wt.-% is by total weight of the aluminum composite material and the wt.-% aluminum plus the wt.-% manganese plus the wt.-% cobalt plus the wt.-% nickel is less than or equal to 100%, and the aluminum composite material having a mean force at puncture, determined according to European Standard EN 14477:2004, in the range of from 0.1 N to 1.5 N.

### Claim 2 (depends on 1)

The aluminum composite material of claim 1, comprising from 11 to 26 wt.-%, of nickel, based on the total weight of the aluminum composite material.

### Claim 3 (depends on 1)

The aluminum composite material of claim 1, further comprising lithium and oxygen.

### Claim 4 (depends on 1)

The aluminum composite material of claim 1, having an X-ray diffraction pattern, measured by powder X-ray diffraction (P-XRD) using Cu Kα radiation, comprising a reflection at a 2 theta diffraction angle ranging from 21.7 to 22.8 having an intensity normalized to 100, a reflection at a 2 theta diffraction angle ranging from 32.8 to 33.9 having an intensity ranging from 55 to 75, a reflection at a 2 theta diffraction angle ranging from 34.2 to 35.2 having an intensity ranging from 65 to 85, a reflection at a 2 theta diffraction angle ranging from 60.8 to 61.9 having an intensity ranging from 34 to 54, and a reflection at a 2 theta diffraction angle ranging from 27.7 to 28.8 having an intensity ranging from 12 to 32.

### Claim 5 (depends on 1)

The aluminum composite material of claim 1, having a porosity, determined by scanning electron microscopy, ranging from 15 to 80%.

### Claim 6

A process for preparing an aluminum composite material comprising
a) providing an intermediate lithium ion battery recycling material comprising an aluminum foil and a cathode active material (CAM) and having an average particle diameter (D50), determined by laser light scattering, in the range of from 1 μm to 500 μm at a first temperature ranging from −10° C. to 50° C.;
b) heating the intermediate lithium ion battery recycling material at a second temperature ranging from 400° C. to 630° C.;
c) contacting the intermediate lithium ion battery recycling material with a gas comprising less than 1 volume % oxygen and comprising at least one selected from the group consisting of a combustible gas, a reductive gas, carbon dioxide (CO2), and an inert gas to obtain the aluminum composite material; and
d) optionally, subsequently cooling the aluminum composite material to a third temperature ranging from 10° C. to 100° C.

### Claim 7 (depends on 6)

The process of claim 6, wherein the heating step b) comprises ramping up the temperature from the first temperature to the second temperature over a period of from 10 minutes to 2 hours.

### Claim 8 (depends on 7)

The process of claim 7, wherein the temperature ramp has an average rate of temperature increase of at least 1K per minute.

### Claim 9 (depends on 6)

The process of claim 6, further comprising dwelling at the second temperature for a period of time ranging from 0 minutes to 2 hours.

### Claim 10 (depends on 6)

The process of claim 6, wherein the intermediate lithium ion battery recycling material is selected from the group consisting of nickel, cobalt, manganese, copper, aluminum, iron, phosphorus, and combinations thereof.

### Claim 11 (depends on 6)

The process of claim 6, wherein the intermediate lithium ion battery recycling material further comprises at least one organic material selected from the group consisting of polymeric binders, conductive carbon, organic carbonates, and combinations thereof, and the reductive gas is generated in situ by thermal decomposition of the at least one organic material.

### Claim 12 (depends on 6)

The process of claim 6, wherein the intermediate lithium ion battery recycling material shows a particle size distribution, determined by laser light scattering, having a D(10) value in a range of from 2 to 6 μm, a D(50) value in a range of from 10 to 30 μm, and a D(90) value in a range of from 150 to 250 μm.

### Claim 13 (depends on 6)

The process of claim 6, wherein the intermediate lithium ion battery recycling material has been obtained by mechanically comminuting at least one selected from the group consisting of a lithium ion battery, lithium ion battery waste, lithium ion battery production scrap, lithium ion cell production scrap, lithium ion cathode active material, and combinations thereof and subsequent drying of the comminuted material.

### Claim 14 (depends on 6)

The process of claim 6, wherein the intermediate lithium ion battery recycling material comprises from 1 weight % to 5 weight % aluminum in a zero oxidation state as aluminum foil, and from 50 weight % to 95 weight % of cathode active material; wherein each weight % is by total weight of the intermediate lithium ion battery recycling material.

### Claim 15 (depends on 1)

A method of using an aluminum composite material according to claim 1, the method comprising using the aluminum composite material recovering valuable materials from lithium ion batteries.