# US 2026/0169215 A1 · Perovskite optical fibers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0169215 A1
- Document ID: US20260169215A1
- Status: Published application
- Kind: A1
- Application number: 19/102,207
- Filed: 2023-08-09
- Published: 2026-06-18
- Earliest claimed: 2022-08-10
- Assignees: Queen Mary University of London
- Applicants: Queen Mary University of London
- Inventors: Yongfeng ZHOU; Lei SU
- Web page: https://patentgrep.com/patent/US20260169215A1

## CPC

- C30B 29/12: Halides
- G02B 6/02033: {Core or cladding made from organic material, e.g. polymeric material (G02B1/04 takes precedence)}
- C30B 7/14: the crystallising materials being formed by chemical reactions in the solution
- C30B 29/60: characterised by shape
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

A method for the growth of single-crystal perovskite optical fibres, the fibres having a cladding and a perovskite core, the method comprising: continuously growing the perovskite core along an axial direction of a capillary filled with perovskite precursor solution, wherein the axial directional growth of the perovskite core is realised by capillaries, which limit growth of the perovskite core in the radial direction, wherein the method is controlled by gradually changing heating position and localised contact of a heating block with the capillary, and the capillary forms the cladding of the single-crystal organometallic perovskite optical fibre.

## Claims

### Claim at position 1

1-26. (canceled)

### Claim 27

A method for the growth of single-crystal perovskite optical fibres, the fibres having a cladding and a perovskite core, the method comprising:
continuously growing the perovskite core along an axial direction of a capillary filled with perovskite precursor solution,
wherein the axial directional growth of the perovskite core is realised by capillaries, which limit growth of the perovskite core in the radial direction,
wherein the method is controlled by gradually changing heating position and localised contact of a heating block with the capillary, and
the capillary forms the cladding of the single-crystal organometallic perovskite optical fibre.

### Claim 28 (depends on 27)

The method of claim 27 being a solution-processed, space-confined, inverse temperature crystallisation, localised translational heating method.

### Claim 29 (depends on 27)

The method of claim 27, wherein the length of the fibre is controlled by the heating method.

### Claim 30 (depends on 27)

The method of claim 27 wherein the perovskite is an organometallic perovskite.

### Claim 31 (depends on 27)

The method of claim 27, wherein the cross section of the perovskite fibre core corresponds to an inner diameter of the capillary.

### Claim 32 (depends on 27)

The method of claim 27, wherein the capillary is made from a material which has a refractive index that is lower than the refractive index of the perovskite core.

### Claim 33 (depends on 27)

The method of claim 27 wherein the cladding material is glass or polytetrafluoroethylene.

### Claim 34

A method for the growth of a single-crystal organometallic perovskite optical fibre having a core and cladding, comprising the steps of:
forming a perovskite precursor solution;
filtering the solution;
filling the perovskite precursor solution into capillary tubes;
sealing the capillary tubes at one end;
placing a heat transfer block on a hotplate, such that the heat transfer block has a line contact with the capillary;
heating the solution at a predetermined position on the capillary until a seed perovskite crystal is formed;
reducing the heating temperature such that single-crystal fibre growth of the precursor solution takes place;
translating the predetermined position according to the growth speed of the single-crystal organometallic perovskite optical fibre to ensure heating position is located at the crystal-solution interface, such that a constant temperature gradient is maintained in front of the crystal-solution interface by the changed heating position.

### Claim 35 (depends on 34)

The method of claim 34, further comprising a step of supplying fresh precursor perovskite solution into the capillary tubes at the other end during growth of the single crystal.

### Claim 36 (depends on 34)

The method according to claim 34, wherein the single-crystal organometallic perovskite optical fibre has a CH3NH3PbBr3 core, and the organometallic perovskite precursor solution is formed by dissolving PbBr2 and CH3NH3Br3 (1/1 by molar, 1 M) in DMF by magnetic stirring at room temperature.

### Claim 37 (depends on 35)

The method according to claim 35, wherein the single-crystal organometallic perovskite optical fibre has a CH3NH3PbBr3 core, and the organometallic perovskite precursor solution is formed by dissolving PbBr2 and CH3NH3Br3 (1/1 by molar, 1 M) in DMF by magnetic stirring at room temperature.

### Claim 38 (depends on 34)

The method according to claim 34, wherein the single-crystal organometallic perovskite optical fibres have a CH3NH3PbX3 core, wherein X is chlorine or iodine, and the precursor solution is formed by dissolving PbX2 and CH3NH3X (1/1 by molar, 1 M) in DMF by magnetic stirring at room temperature, and/or wherein the solution is filtered using a PTFE filter with 0.2 μm pore size.

### Claim 39 (depends on 34)

The method according to claim 34, wherein the solution is heated at the sealed end of the capillary tube to 80° C. for a few hours, such that the seed organometallic perovskite crystal is formed.

### Claim 40 (depends on 34)

The method according to claim 34, wherein the hotplate temperature is reduced to 60° C. such that single-crystal fibre growth of the precursor solution takes place.

### Claim 41 (depends on 34)

The method according to claim 34, wherein the precursor solution is refreshed periodically during the crystal growth to produce longer organometallic perovskite optical fibre, wherein optionally, the precursor solution is refreshed when the growth rate of the crystal becomes lower than normal value.

### Claim 42 (depends on 34)

The method according to claim 34, wherein the capillary tubes are made of silica or PTFE.

### Claim 43 (depends on 34)

The method according to claim 34, wherein the diameter of the capillary is equal to or greater than 50 μm and equal to or less than 1000 μm.

### Claim 44 (depends on 27)

An optical fibre manufactured according to the method of claim 27.

### Claim 45 (depends on 34)

An optical fibre manufactured according to the method of claim 34.

### Claim 46

An optical fibre comprising a cladding and a core, wherein the core is a single-crystal organometallic halide perovskite.

### Claim 47 (depends on 46)

The optical fibre according to claim 46, wherein the cladding is silica or PTFE, and optionally, wherein the core is a single crystal CH3NH3PbBr3.

### Claim 48 (depends on 47)

An optical switch comprising the optical fibres of claim 47.