# US 2026/0168173 A1 · Method of manufacturing a film comprising highly refined cellulose fibers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0168173 A1
- Document ID: US20260168173A1
- Status: Published application
- Kind: A1
- Application number: 19/128,840
- Filed: 2023-10-30
- Published: 2026-06-18
- Earliest claimed: 2022-11-11
- Assignees: Stora Enso OYJ
- Applicants: Stora Enso OYJ
- Inventors: Pekka Kylliäinen; Isto Heiskanen
- Web page: https://patentgrep.com/patent/US20260168173A1

## CPC

- D21F 11/14: Making cellulose wadding, filter or blotting paper
- D21H 11/18: Highly hydrated, swollen or fibrillatable fibres
- C08J 5/18: Manufacture of films or sheets
- D21F 1/50: Suction boxes with rolls
- D21F 3/0218: {Shoe presses}
- D21F 9/00: Complete machines for making continuous webs of paper
- D21F 11/00: Processes for making continuous lengths of paper, or of cardboard, or of wet web for fibre board production, on paper-making machines
- D21F 11/04: paper or board consisting on two or more layers
- D21G 1/00: Calenders (if restricted to the treatment of particular materials see the relevant class, e.g. B29C43/24, D06); Smoothing apparatus
- D21H 19/34: comprising cellulose or derivatives thereof
- D21H 19/52: Cellulose; Derivatives thereof
- D21H 21/16: Sizing or water-repelling agents
- D21H 27/10: Packing paper (packaging materials of special type or form B65D65/38)
- C08J 2301/02: Cellulose; Modified cellulose
- D21F: PAPER-MAKING MACHINES; METHODS OF PRODUCING PAPER THEREON
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- D21G: CALENDERS; ACCESSORIES FOR PAPER-MAKING MACHINES (winders or rewinders for finished products, means for adjustment of wrinkles or lateral extensions B65H)

## Abstract

The present invention relates to a method for manufacturing a film comprising highly refined cellulose fibers in a paper-making machine, the method comprising the steps of: a) forming a wet web by applying a pulp suspension comprising at least 50% b dry weight of highly refined cellulose fibers having a Schopper-Riegler (SR) value in the range of 80-100 from a headbox onto a moving wire and partially dewater the web on the wire; and b) feeding the partially dewatered web from the wire into a dewatering nip formed between a suction roll and a lump breaker roll to further dewater the wet web, c) optionally further dewatering the web from the dewatering nip in a press section and drying the web in a drying section to obtain a film comprising the highly refined cellulose fibers.

## Claims

### Claim 1

A method for manufacturing a film comprising highly refined cellulose fibers in a paper-making machine, the method comprising the steps of:
a) forming a wet web by applying a pulp suspension comprising at least 50% by dry weight of highly refined cellulose fibers having a Schopper-Riegler (SR) value in a range of 80-100 from a headbox onto a moving wire and partially dewatering the wet web on the wire to form a partially dewatered web;
b) feeding the partially dewatered web from the wire into a dewatering nip formed between a suction roll and a lump breaker roll to further dewater the partially dewatered web;
c) optionally further dewatering the partially dewatered web from the dewatering nip in a press section; and
d) drying the partially dewatered web in a drying section to obtain a film comprising the highly refined cellulose fibers.

### Claim 2 (depends on 1)

The method according to claim 1, wherein a dry solids content of the pulp suspension applied onto the wire is in a range of 0.1-0.7 wt %.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the highly refined cellulose fibers have an SR value in a range of 80-98.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the highly refined cellulose fibers have a water retention value (WRV) of at least 2.0 g/g.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the highly refined cellulose fibers comprises microfibrillated cellulose (MFC).

### Claim 6 (depends on 1)

The method according to claim 1, wherein a wire speed of the moving wire is >200 m/min.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the wet web formed in step a) is combined with one or more additional webs to form a multiply web.

### Claim 8 (depends on 1)

The method according to claim 1, further comprising:
combining the wet web of step a) wherein the pulp suspension comprises 80-100% by dry weight of highly refined cellulose fibers with a second web comprising 30-70% by dry weight of highly refined cellulose fibers to form a multiply web.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the dewatering nip is arranged such that a surface of the partially dewatered web facing the moving wire in step a) also faces the lump breaker roll in the dewatering nip in step b).

### Claim 10 (depends on 1)

The method according to claim 1, wherein the lump breaker roll is provided with a press felt wrapped around the lump breaker roll.

### Claim 11 (depends on 1)

The method according to claim 1, wherein a press load in the dewatering nip is 10 kN/m or less.

### Claim 12 (depends on 1)

The method according to claim 1, wherein a vacuum in the suction roll is in a range of −400 to −700 mmHg.

### Claim 13 (depends on 1)

The method according to claim 1, wherein a solid content of the partially dewatered web entering the dewatering nip is in a range of 7-13 wt %.

### Claim 14 (depends on 1)

The method according to claim 1, wherein a solid content of the partially dewatered web leaving the dewatering nip is in a range of 14-20 wt %.

### Claim 15 (depends on 1)

The method according to claim 1, wherein press section comprises at least one press nip.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the press section comprises three press nips arranged sequentially in a running direction of the web, and
wherein the press load in a first press nip is in a range of 8-12 kN/m, a press load in a second press nip is in a range of 18-22 kN/m, and a press load in a third press nip is in a range of 28-32 kN/m.

### Claim 17 (depends on 15)

The method according to claim 15, wherein the press section comprises at least one shoe press nip.

### Claim 18 (depends on 17)

The method according to claim 17, wherein press load in the at least one shoe press nip is in a range of 300-900 kN/m.

### Claim 19 (depends on 1)

The method according to claim 1, wherein the dry solids content of the partially dewatered web after the further dewatering in the press section is in a range of 25-45 wt %.

### Claim 20 (depends on 1)

The method according to claim 1, wherein a dry solids content of the film after the drying in the drying section is in a range of 85-99 wt %.

### Claim 21 (depends on 1)

The method according to claim 1, wherein the film has a dry basis weight in a range of 10-60 g/m2.

### Claim 22 (depends on 1)

The method according to claim 1, wherein the film has a density of at least 800 kg/m3, as measured according to standard ISO 534.

### Claim 23 (depends on 1)

The method according to claim 1, wherein the film comprises less than 10 pinholes/m2, as measured according to standard EN 13676:2001.

### Claim 24 (depends on 1)

The method according to claim 1, wherein the film has a KIT value of at least 8, as measured according to standard ISO 16532-2.

### Claim 25 (depends on 1)

The method according to claim 1, wherein the film fibers has a Gurley Hill value of at least 10,000 s/100 ml, as measured according to standard ISO 5636/6.

### Claim 26 (depends on 1)

The method according to claim 1, wherein the film has an oxygen transfer rate (OTR), measured according to standard ASTM F1927-98 at 50% relative humidity and 23° C., of less than 100 cc/m2/24 h/atm.