# US 2026/0168106 A1 · Nanocomposite coating material having adhesion resistance, manufacturing system and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0168106 A1
- Document ID: US20260168106A1
- Status: Published application
- Kind: A1
- Application number: 19/529,573
- Filed: 2026-02-04
- Published: 2026-06-18
- Earliest claimed: 2023-11-28
- Assignees: INNOTION TECH Co., Ltd.
- Applicants: INNOTION TECH Co., Ltd.
- Inventors: JEONG KI HONG; IN KI HONG; MYOUNG KI HONG
- Web page: https://patentgrep.com/patent/US20260168106A1

## CPC

- C23C 16/26: Deposition of carbon only
- C23C 28/042: {including a refractory ceramic layer, e.g. refractory metal oxides, ZrO2, rare earth oxides}
- C23C 14/0036: {Reactive sputtering}
- C23C 14/024: {Deposition of sublayers, e.g. to promote adhesion of the coating (C23C14/027 takes precedence)}
- C23C 14/027: {Graded interfaces}
- C23C 14/06: characterised by the coating material ({C23C14/0021} , C23C14/04 take precedence)
- C23C 14/0605: {Carbon}
- C23C 14/0641: {Nitrides (C23C14/0617 takes precedence)}
- C23C 14/221: {Ion beam deposition (C23C14/46, C23C14/48 take precedence)}
- C23C 14/345: {using substrate bias}
- C23C 16/50: using electric discharges {(generation and control of plasma in discharge tubes for surface treatment H01J37/32, H01J37/34)}
- H01M 4/0409: {by a doctor blade method, slip-casting or roller coating}
- Y02E 60/10: Energy storage using batteries
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

It is an object to provide a coating material having heat resistance, adhesion resistance, durability, chemical resistance, low friction, and releaseability applied to a base material, and to provide a manufacturing method and manufacturing system for such a coating material. A ternary nanocoposite coating material comprising C—F—H or C—F—Si applied to a base material is disclosed.

## Claims

### Claim 1

A coating material having adhesion resistance (non-stick properties), comprising:
a buffer layer sequentially including a Cr layer, a CrN layer, a CrN2 layer, and a CrCH layer; and
a ternary nanocomposite coating layer of C—F—H formed on the buffer layer,
wherein the ternary nanocomposite coating layer is formed by supplying reducing hydrogen in addition to C and F components during the formation process, wherein the coating layer is a gradient coating layer comprising a higher concentration of the F component toward the surface, wherein the coating material has a contact angle of 90° or more, and has a high hardness characteristic of 17 to 27 GPa.

### Claim 2

A coating material having adhesion resistance (non-stick properties), comprising:
a buffer layer sequentially including a Cr layer, a CrN layer, a CrN2 layer, and a CrCH layer; and
a ternary nanocomposite coating layer of C—F—Si formed on the buffer layer,
wherein the ternary nanocomposite coating layer is formed by supplying reducible hydrogen in addition to C, F, and Si components during the formation process, wherein the coating layer is a gradient coating layer comprising a higher concentration of the F component toward the surface, wherein the coating material has a contact angle of 90° or more, and has a high hardness characteristic of 17 to 27 GPa.

### Claim 3 (depends on 1)

The coating material having adhesion resistance (non-stick properties) to claim 1, wherein the coating material exhibiting the adhesion resistance has a low friction coefficient of 0.12 or less and a bonding force of the coating material of 20 N or more.

### Claim 4 (depends on 2)

The coating material having adhesion resistance (non-stick properties) according to claim 2, wherein the coating material exhibiting the adhesion resistance has a low friction coefficient of 0.12 or less and a bonding force of the coating material of 20 N or more.

### Claim 5 (depends on 1)

The coating material having adhesion resistance (non-stick properties) according to claim 1, wherein the coating material exhibiting the adhesion resistance has an electrical resistance of 1×106 to 9.9×108Ω.

### Claim 6 (depends on 2)

The coating material having adhesion resistance (non-stick properties) according to claim 2, wherein the coating material exhibiting the adhesion resistance has an electrical resistance of 1×106 to 9.9×108Ω.

### Claim 7

A manufacturing system for a ternary nanocomposite coating material comprising C—F—H, or C—F—Si, comprising:
a chamber for loading a base material;
an ion source applied to the chamber;
a cylinder sputter source including a Cr target to form a Cr-based buffer layer prior to coating the ternary nanocomposite coating on the surface of the base material;
a raw material supply unit for feeding said ion source with C, F, and H, or C, F, and Si, respectively, as raw materials; and
a power supply unit;
wherein the power supply unit applies a bias voltage of 50 to 500 volts to the base material to attract the generated plasma and electrons toward the base material, wherein the ion source includes permanent magnets or electromagnets arranged to generate high-density plasma,
wherein the cylindrical sputter source is utilized to form a buffer layer on the base material, comprising, in order, a Cr layer, a CrN layer, a CrN2 layer, and a CrCH layer, wherein a ternary nanocomposite coating layer of C—F—H is formed on the buffer layer by supplying hydrocarbon gas, CF4, and reducing hydrogen (H2) to the ion source as raw materials,
or a ternary nanocomposite coating layer of C—F—Si is formed on the buffer layer by supplying hydrocarbon gas, CF4, reducing hydrogen (H4), and at least one of TMS(Tetramethylsilane), SiH4, Si2H6, or SiH2Cl2 as Si sources to the ion source, and the nanocomposite coating layer is formed as a gradient coating layer comprising more of the F component toward the surface.

### Claim 8 (depends on 7)

The nanocomposite coating material manufacturing system according to claim 7, wherein, in order to uniformly coat a large-area surface of the base material inside a large chamber, permanent magnets or electromagnets are arranged in the ion source to generate a magnetic field, thereby concentrating plasma in a predetermined space and forming high-density plasma.

### Claim 9 (depends on 8)

The nanocomposite coating manufacturing system according to claim 8, wherein the permanent magnet and the electromagnet are arranged together to form a magnetic field by the permanent magnet, and selectively drive the electromagnet at a predetermined position to complement the magnetic field formed by the permanent magnet with the electromagnet.

### Claim 10 (depends on 7)

A method of forming a ternary nanocomposite coating material comprising C—F—H using the nanocomposite coating material manufacturing system according to claim 7, comprising the steps of:
prior to forming the ternary nanocomposite coating material, applying a voltage of 300 to 1000 V to a sputtering source including a Cr cylinder target,
applying a bias voltage of 80 to 500 V to the base material,
flowing at least one of an inert gas and nitrogen (N2) to perform a sputtering process to form a Cr-based buffer layer,
wherein, in the buffer layer forming process:
initially, only the inert gas is supplied to form a Cr layer,
subsequently, the inert gas, nitrogen, and reducing hydrogen are supplied to form a CrN layer,
the nitrogen supply ratio is increased to enhance the nitrogen content and form a N-enhanced nitride hardening layer,
in the final stage of buffer layer formation, the inert gas, nitrogen, reducing hydrogen, and hydrocarbon gas are supplied to form a carbonitrided hardening layer of CrCH as a gradient layer,
supplying hydrocarbon gas, CF4 gas, and reducing hydrogen (H2) to the raw material supply unit of the ion source,
applying a voltage of 500 to 2000 V to the ion source and a bias voltage of 50 to 500 V to the base material to form a ternary nanocomposite coating material containing C—F—H,
wherein the composition ratio of CF4 gas supplied to the raw material supply unit of the ion source is gradually increased to form a gradient layer in which the fluorine (F) content increases toward the surface of the ternary nanocomposite coating material,
wherein, in the formation of the ternary nanocomposite coating material, initially, hydrocarbon and reducing hydrogen are supplied to form a first top coating layer comprising a CH-based high-density, high-hardness, and wear-resistant nanomatrix coating,
subsequently, hydrocarbon, CF4 gas, and reducing hydrogen are supplied to form a second top coating layer as an interfacial transition layer comprising CFH-based nanocomposite carbon with anti-sticking functionality,
then, hydrocarbon, CF4, and reducing hydrogen are supplied with an increased CF4 supply ratio to form a FCH coating layer as a third top coating layer, thereby enhancing the anti-sticking property of the base material surface.

### Claim 11 (depends on 7)

A method for forming a ternary nanocomposite coating material comprising C—F—Si using the nanocomposite coating material manufacturing system according to claim 7, comprising the steps of;
prior to forming the ternary nanocomposite coating material, applying a voltage of 300 to 1000 V to a sputtering source including a Cr cylinder target,
applying a bias voltage of 80 to 500 V to the base material,
flowing at least one of an inert gas and nitrogen (N2) to perform a sputtering process to form a Cr-based buffer layer,
wherein, in the buffer layer forming process:
initially, only the inert gas is supplied to form a Cr layer,
subsequently, the inert gas, nitrogen, and reducing hydrogen are supplied to form a CrN layer,
the nitrogen supply ratio is increased to enhance the nitrogen content and form a N-enhanced nitride hardening layer,
in the final stage of buffer layer formation, the inert gas, nitrogen, reducing hydrogen, and hydrocarbon gas are supplied to form a carbonitrided hardening layer of CrCH as a gradient layer,
supplying hydrocarbon gas, CF4 gas, and at least one of TMS (tetramethylsilane), SiH4, Si2H6, or SiH2Cl2 to the raw material supply unit of the ion source, and additionally supplying reducing hydrogen (H2),
applying a voltage of 500 to 2000 V to the ion source and applying a bias voltage of 50 to 500 V to the base material to form the ternary nanocomposite coating material comprising C—F—Si,
wherein the composition ratio of CF4 gas supplied to the raw material supply unit of the ion source is gradually increased to form a gradient layer in which the fluorine (F) content increases toward the surface of the ternary nanocomposite coating material, wherein, in the formation of the ternary nanocomposite coating material,
initially, hydrocarbon, at least one of TMS, SiH4, Si2H6, or SiH2Cl2, and reducing hydrogen are supplied to form a first top coating layer comprising a high-density, high-hardness, and wear-resistant nanomatrix coating,
subsequently, hydrocarbon, CF4 gas, at least one of TMS, SiH4, Si2H6, or SiH2Cl2, and reducing hydrogen are supplied to form a second top coating layer as an interfacial transition layer comprising nanocomposite carbon with anti-sticking functionality,
then, hydrocarbon, CF4 gas, at least one of TMS, SiH4, Si2H6, or SiH2Cl2, and reducing hydrogen are supplied with an increased CF4 supply ratio to form a third top coating layer, thereby enhancing the anti-sticking property of the base material surface.

### Claim 12 (depends on 10)

The method of forming the ternary nanocomposite coating according to claim 10, wherein prior to forming the buffer layer, plasma cleaning is performed on the base material, wherein the voltage applied to the ion source is 500 to 2000 V, the current is 0.3 to 1.8 A, and the bias voltage applied to the base material is 50 to 150 khz, 50 to 500 V.

### Claim 13 (depends on 11)

The method of forming the ternary nanocomposite coating according to claim 11, wherein prior to forming the buffer layer, plasma cleaning is performed on the base material, wherein the voltage applied to the ion source is 500 to 2000 V, the current is 0.3 to 1.8 A, and the bias voltage applied to the base material is 50 to 150 khz, 50 to 500 V.