- Number: US 2026/0166528 A1
- Document ID: US20260166528A1
- Status: Published application
- Kind: A1
- Application number: 19/257,602
- Filed: 2025-07-02
- Published: 2026-06-18
- Earliest claimed: 2024-12-12
- Assignees: Industrial Technology Research Institute
- Applicants: Industrial Technology Research Institute
- Inventors: Kuo-Ching WU; Pao-Tsern LIN; Hsi-Yen HSU; Chao-Huang CHEN; Cheng-Hsun LI; Yen-Chih CHEN; Ying-Chieh LEE
- Web page: https://patentgrep.com/patent/US20260166528A1

## CPC

- B01J 23/8892: {Manganese}
- B01J 23/745: Iron
- B01J 23/78: with alkali- or alkaline earth metals
- B01J 23/83: with rare earths or actinides
- C07C 2/862: {the non-hydrocarbon contains only oxygen as hetero-atoms}
- C07C 2523/34: Manganese
- C07C 2523/745: Iron
- C07C 2523/83: with rare earths or actinides
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

Disclosed is a catalyst mixture that includes a mixture of a metal oxide catalyst and an iron-based catalyst. The metal oxide catalyst has a chemical formula of Fe1MnaMbOx, wherein M is Ce or La, a is 0.1 to 0.5, b is 0.1 to 0.3, and x is chemical stoichiometry. The iron-based catalyst includes 70 mol % to 97 mol % of porous FeO(OH)c, wherein 1<c<2, and 3 mol % to 30 mol % of an alkaline metal compound loaded onto the porous FeO(OH)c.

## Claims

### Claim 1

A catalyst mixture comprising:
a mixture of a metal oxide catalyst and an iron-based catalyst,
wherein the metal oxide catalyst has a chemical formula of Fe1MnaMbOx, wherein M is Ce or La, a is 0.1 to 0.5, b is 0.1 to 0.3, and x is chemical stoichiometry,
wherein the iron-based catalyst comprises 70 mol % to 97 mol % of porous FeO(OH)c, wherein 1<c<2, and 3 mol % to 30 mol % of an alkaline metal compound loaded onto the porous FeO(OH)c.

### Claim 2 (depends on 1)

The catalyst mixture as claimed in claim 1, wherein a is 0.1 to 0.43.

### Claim 3 (depends on 1)

The catalyst mixture as claimed in claim 1, wherein b is 0.14 to 0.3.

### Claim 4 (depends on 1)

The catalyst mixture as claimed in claim 1, wherein c satisfies 1<c≤1.52.

### Claim 5 (depends on 1)

The catalyst mixture as claimed in claim 1, wherein the metal oxide catalyst and the iron-based catalyst have a volume ratio of 1:4 to 1:1.

### Claim 6 (depends on 1)

The catalyst mixture as claimed in claim 1, wherein the porous FeO(OH)c has a specific surface area of at least 100 m2/g.

### Claim 7 (depends on 1)

The catalyst mixture as claimed in claim 1, wherein the porous FeO(OH)c has a pore volume in a range of 0.2 cm3/g to 0.5 cm3/g.

### Claim 8 (depends on 1)

The catalyst mixture as claimed in claim 1, wherein the porous FeO(OH)c has an average pore size in a range of 40 Å to 70 Å.

### Claim 9 (depends on 1)

A method of synthesizing alkanes and olefins, the method comprising:
bringing a gaseous mixture of carbon dioxide, methane, and hydrogen into contact with the catalyst mixture as claimed in claim 1 to form a product comprising water and at least one of alkanes having a carbon number of 2 or more and olefins having a carbon number of 2 or more.

### Claim 10 (depends on 9)

The method as claimed in claim 9, wherein the product further comprises carbon monoxide and methane.

### Claim 11 (depends on 9)

The method as claimed in claim 9, wherein the gaseous mixture has a gas hourly space velocity in a range of 200 h−1 to 3000 h−1.

### Claim 12 (depends on 9)

The method as claimed in claim 9, wherein the carbon dioxide and the methane in the gaseous mixture have a molar ratio in a range of 1:0.2 to 1:4, and the carbon dioxide and the hydrogen in the gaseous mixture have a molar ratio in a range of 1:0.5 to 1:4.

### Claim 13 (depends on 9)