# US 2026/0163066 A1 · Solid-state battery and method of manufacturing solid-state battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0163066 A1
- Document ID: US20260163066A1
- Status: Published application
- Kind: A1
- Application number: 19/411,805
- Filed: 2025-12-08
- Published: 2026-06-11
- Earliest claimed: 2024-12-10
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Takuya MATSUYAMA
- Web page: https://patentgrep.com/patent/US20260163066A1

## CPC

- H01M 10/0562: Solid materials
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 50/533: characterised by the shape of the leads or tabs
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0097: with adhesive layers
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A solid-state battery includes: a positive electrode current collector; a positive electrode layer disposed on at least one main face of the positive electrode current collector; an insulating layer that is disposed on the one main face of the positive electrode current collector, is contiguous with the end portion of the positive electrode layer, and is flush with the positive electrode layer; and a solid electrolyte layer disposed on the positive electrode layer and the insulating layer with its end portion in a position overlying the insulating layer.

## Claims

### Claim 1

A solid-state battery, comprising:
a positive electrode current collector;
a positive electrode layer disposed on at least one main face of the positive electrode current collector;
an insulating layer that is disposed on the at least one main face of the positive electrode current collector, that is contiguous with an end portion of the positive electrode layer, and that is flush with the positive electrode layer; and
a solid electrolyte layer disposed on the positive electrode layer and the insulating layer and having an end portion in a position overlying the insulating layer.

### Claim 2 (depends on 1)

The solid-state battery of claim 1, wherein the positive electrode current collector comprises a positive electrode current collector tab-side end portion connected to a positive electrode current collector tab, and wherein the insulating layer and the positive electrode layer are disposed in this order from the positive electrode current collector tab-side end portion.

### Claim 3 (depends on 1)

The solid-state battery of claim 1, comprising an adhesive layer between the positive electrode current collector, and the positive electrode layer and the insulating layer.

### Claim 4 (depends on 3)

The solid-state battery of claim 3, wherein the adhesive layer is conductive.

### Claim 5 (depends on 3)

The solid-state battery of claim 3, wherein the adhesive layer has a thickness of 0.5 μm to 1.5 μm.

### Claim 6 (depends on 1)

The solid-state battery of claim 1, further comprising a negative electrode layer disposed on the solid electrolyte layer, wherein an end portion of the negative electrode layer is in a position overlying the solid electrolyte layer and the insulating layer in a cross-sectional view along a layering direction of the positive electrode current collector, the positive electrode layer and the insulating layer, and the solid electrolyte layer.

### Claim 7 (depends on 1)

The solid-state battery of claim 1, wherein an angle of inclination of an end face of the positive electrode layer that is contiguous with the insulating layer, and an angle of inclination of an end face of the insulating layer at an opposite side from an end face that is contiguous with the positive electrode layer, in a cross-sectional view along a layering direction of the positive electrode current collector, the positive electrode layer and the insulating layer, and the solid electrolyte layer, are in a range of ±10° relative to the layering direction.

### Claim 8 (depends on 1)

The solid-state battery of claim 1, wherein an angle of inclination of an end face of the insulating layer at an opposite side from an end face that is contiguous with the positive electrode layer is closer to 90° than an angle of inclination of an end face of the positive electrode layer that is contiguous with the insulating layer in a cross-sectional view along a layering direction of the positive electrode current collector, the positive electrode layer and the insulating layer, and the solid electrolyte layer.

### Claim 9

A method of manufacturing a solid-state battery, the method comprising:
forming, on at least one main face of a positive electrode current collector, a positive electrode layer and an insulating layer that is contiguous with an end portion of the positive electrode layer and flush with the positive electrode layer; and
forming a solid electrolyte layer on the positive electrode layer and the insulating layer such that an end portion of the solid electrolyte layer overlies the insulating layer.

### Claim 10 (depends on 9)

The method of manufacturing a solid-state battery of claim 9, further comprising forming a negative electrode layer such that an end portion of the negative electrode layer overlies the solid electrolyte layer and the insulating layer in a cross-sectional view along a layering direction of the positive electrode current collector, the positive electrode layer and the insulating layer, and the solid electrolyte layer.

### Claim 11 (depends on 9)

The method of manufacturing a solid-state battery of claim 9, wherein, in the forming the positive electrode layer and the insulating layer, an adhesive layer is formed on the at least one main face of the positive electrode current collector, and the positive electrode layer and the insulating layer, which have been formed on a transfer member, are transferred to the adhesive layer.

### Claim 12 (depends on 11)

The method of manufacturing a solid-state battery of claim 11, wherein the adhesive layer is conductive.

### Claim 13 (depends on 11)

The method of manufacturing a solid-state battery of claim 11, wherein the adhesive layer has a thickness of 0.5 μm to 1.5 μm.

### Claim 14 (depends on 11)

The method of manufacturing a solid-state battery of claim 11, wherein a positive electrode slurry comprising a positive electrode active material is coated on the transfer member, thereafter, an inclined face of a peripheral edge portion of the coated positive electrode slurry is cut off and an insulating slurry comprising an insulating material is coated so as to be contiguous with the peripheral edge portion of the positive electrode slurry, and thereafter, an inclined face of a peripheral edge portion of the coated insulating slurry is cut off.

### Claim 15 (depends on 14)

The method of manufacturing a solid-state battery of claim 14, wherein an angle of inclination of an end face of the positive electrode layer contiguous with the insulating layer, and an angle of inclination of an end face of the insulating layer at an opposite side from an end face that is contiguous with the positive electrode layer, in a cross-sectional view along a layering direction of the positive electrode current collector, the positive electrode layer and the insulating layer, and the solid electrolyte layer, are in a range of ±10° relative to the layering direction.

### Claim 16 (depends on 11)

The method of manufacturing a solid-state battery of claim 11, wherein a positive electrode slurry comprising a positive electrode active material is coated on the transfer member, thereafter, an insulating slurry comprising an insulating material is coated so as to cover an inclined face of a peripheral edge portion of the coated positive electrode slurry, and thereafter, an inclined face of a peripheral edge portion of the coated insulating slurry is cut off.

### Claim 17 (depends on 16)

The method of manufacturing a solid-state battery of claim 16, wherein an angle of inclination of an end face of the insulating layer at an opposite side from an end face that is contiguous with the positive electrode layer is closer to 90° than an angle of inclination of an end face of the positive electrode layer that is contiguous with the insulating layer in a cross-sectional view along a layering direction of the positive electrode current collector, the positive electrode layer and the insulating layer, and the solid electrolyte layer.