# US 2026/0160496 A1 · Plasma assisted metal oxide reduction during die-to-wafer anneal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0160496 A1
- Document ID: US20260160496A1
- Status: Published application
- Kind: A1
- Application number: 18/970,088
- Filed: 2024-12-05
- Published: 2026-06-11
- Earliest claimed: 2024-12-05
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Angelique Raley; Arkalgud Sitaram
- Web page: https://patentgrep.com/patent/US20260160496A1

## CPC

- F27B 17/0025: {specially adapted for treating semiconductor wafers}
- H01J 37/32449: {Gas control, e.g. control of the gas flow}
- H01J 37/32816: {Pressure}
- H10W 72/019: {of bond pads}
- H10W 72/01971: {Cleaning, e.g. oxide removal}
- H10W 72/90: Bond pads, in general
- H10W 72/941: {Dispositions of bond pads}
- H10W 80/00: Direct bonding of chips, wafers or substrates
- H10W 80/016: {Cleaning}
- H10W 80/102: {Controlling the environment during the bonding, e.g. the temperature or pressure}
- H10W 80/301: {Bonding techniques, e.g. hybrid bonding}
- H10W 80/312: {characterised by the direct bonding of electrically conductive pads}
- H10W 80/334: {Thermocompression bonding}
- H10W 80/743: {having disposition changed during the connecting}
- H10W 80/314: {characterized by direct bonding of pads or other interconnections}
- H10W 80/327: {characterised by the direct bonding of insulating parts, e.g. of silicon oxide layers}
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for making a semiconductor device can include picking and placing a top die onto a bottom die on a wafer such that a first set of operational contacts of the bottom die are aligned with and physically contacting a second set of operational contacts of the top die, and such that a first set of test contacts are exposed and not fully covered by the top die, and annealing the wafer to induce bonding of the second set of operational contacts of the top die with the first set of operational contacts of the bottom die in a plasma-equipped furnace chamber while exciting a plasma along with flowing gas including nitrogen and hydrogen to hinder oxidation of metal, such as copper, in the first set of test contacts during the annealing.

## Claims

### Claim 1

A method of manufacturing semiconductor devices, the method comprising:
providing a first wafer comprising a bottom die, wherein the bottom die comprises a first integrated circuit formed therein, wherein the bottom die comprises a first set of operational contacts and a first set of test contacts, wherein the first set of operational contacts and the first set of test contacts are exposed on a top surface of the bottom die, and wherein the first set of test contacts include a metal;
providing a top die from a second wafer, wherein the second wafer is different than the first wafer, wherein the top die comprises a second integrated circuit formed therein, wherein the top die comprises a second set of operational contacts, and wherein the second set of operational contacts are exposed on a bottom surface of the top die;
picking and placing the top die onto the bottom die such that the second set of operational contacts of the top die are aligned with and physically contacting the first set of operational contacts of the bottom die, and such that the first set of test contacts are exposed and not fully covered by the top die; and
annealing the first wafer to induce bonding of the second set of operational contacts of the top die with the first set of operational contacts of the bottom die in a plasma-equipped furnace chamber while exciting a plasma in the plasma-equipped furnace chamber along with flowing of a chamber gas including nitrogen and hydrogen to hinder oxidation of the metal of the first set of test contacts during the annealing.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
prior to the annealing, placing the first wafer into the plasma-equipped furnace chamber while the top die is in place on the bottom die;
placing a third wafer and a fourth wafer into the plasma-equipped furnace chamber along with the first wafer; and
annealing the third wafer and the fourth wafer along with the first wafer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the bottom die is not singulated from the first wafer prior to the annealing, and wherein the top die is singulated from the second wafer prior to the annealing.

### Claim 4 (depends on 1)

The method of claim 1, wherein the metal contains copper, and wherein the annealing is performed at temperature in a range of 200° C. to 400° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the flowing of the chamber gas is at a pressure less than 5 mTorr.

### Claim 6 (depends on 1)

The method of claim 1, wherein the flowing of the chamber gas is at a pressure in a range of 1 mTorr to 9 mTorr.

### Claim 7 (depends on 1)

The method of claim 1, wherein the flowing of the chamber gas is at a volumetric flow rate less than 500 sccm.

### Claim 8

A method of manufacturing semiconductor devices, the method comprising:
providing a first wafer comprising a plurality of bottom dies, wherein each of the plurality of bottom dies comprises a first integrated circuit formed therein, wherein each of the plurality of bottom dies comprises a first set of operational contacts and a first set of test contacts, wherein the first set of operational contacts and the first set of test contacts are exposed on a top surface of each of the plurality of bottom dies, and wherein the first set of test contacts of each of the plurality of bottom dies include a metal;
providing a plurality of top dies from a second one or more wafers, wherein the second one or more wafers is different than the first wafer, wherein each of the plurality of top dies comprises a second integrated circuit formed therein, wherein each of the plurality of top dies comprises a second set of operational contacts, and wherein the second set of operational contacts are exposed on a bottom surface of each of the plurality of top dies;
picking and placing the plurality of top dies onto the plurality of bottom dies, respectively, such that the second set of operational contacts of each of the plurality of top dies are aligned with and physically contacting the first set of operational contacts of each of the plurality of bottom dies, respectively, and such that the first set of test contacts of each of the plurality of bottom dies are exposed and not fully covered by the plurality of top dies; and
annealing the first wafer to induce bonding of the second set of operational contacts of each of the plurality of top dies with the first set of operational contacts of each of the plurality of bottom dies, respectively, in a plasma-equipped furnace chamber while exciting a plasma in the plasma-equipped furnace chamber along with flowing of a chamber gas including nitrogen and hydrogen to hinder oxidation of the metal of the first set of test contacts of the plurality of bottom dies during the annealing.

### Claim 9 (depends on 8)

The method of claim 8, further comprising:
prior to the annealing, placing the first wafer into the plasma-equipped furnace chamber while the plurality of top dies are in place on the plurality of bottom dies;
placing a third wafer and a fourth wafer into the plasma-equipped furnace chamber along with the first wafer; and
annealing the third wafer and the fourth wafer along with the first wafer.

### Claim 10 (depends on 8)

The method of claim 8, wherein the plurality of bottom dies are not singulated from the first wafer prior to the annealing, and wherein the plurality of top dies are singulated from the second one or more wafers prior to the annealing.

### Claim 11

A method of manufacturing semiconductor devices, the method comprising:
providing a first wafer comprising a bottom die, wherein the bottom die comprises a first integrated circuit formed therein, wherein the bottom die comprises a first set of operational contacts and a first set of test contacts, wherein the first set of operational contacts and the first set of test contacts are exposed on a top surface of the bottom die, and wherein the first set of test contacts include a metal;
providing a top die from a second wafer, wherein the second wafer is different than the first wafer, wherein the top die comprises a second integrated circuit formed therein, wherein the top die comprises a second set of operational contacts, and wherein the second set of operational contacts are exposed on a bottom surface of the top die;
performing a first annealing of the first wafer in a plasma-equipped furnace chamber while exciting a first plasma in the plasma-equipped furnace chamber along with flowing of a first chamber gas including nitrogen and hydrogen to remove surface oxidation from the first set of operational contacts and the first set of test contacts;
picking and placing the top die onto the bottom die such that the second set of operational contacts of the top die are aligned with and physically contacting the first set of operational contacts of the bottom die, and such that the first set of test contacts are exposed and not fully covered by the top die; and
performing a second annealing of the first wafer to induce bonding of the second set of operational contacts of the top die with the first set of operational contacts of the bottom die in the plasma-equipped furnace chamber while exciting a second plasma in the plasma-equipped furnace chamber along with flowing of a second chamber gas including nitrogen and hydrogen to hinder oxidation of the metal of the first set of test contacts during the second annealing.

### Claim 12 (depends on 11)

The method of claim 11, further comprising:
prior to the first annealing, placing the first wafer into the plasma-equipped furnace chamber;
after the first annealing, removing the first wafer from the plasma-equipped furnace chamber; and
prior to the second annealing, placing the first wafer into the plasma-equipped furnace chamber while the top die is in place on the bottom die.

### Claim 13 (depends on 11)

The method of claim 11, further comprising:
prior to the second annealing, placing the first wafer into the plasma-equipped furnace chamber while the top die is in place on the bottom die;
placing a third wafer and a fourth wafer into the plasma-equipped furnace chamber along with the first wafer; and
performing the second annealing for the third wafer and the fourth wafer along with the first wafer.

### Claim 14 (depends on 11)

The method of claim 11, wherein the metal contains copper, and wherein the second annealing is performed at temperature in a range of 200° C. to 400° C., and wherein the first annealing is performed at temperature in a range of 100° C. to 450° C.

### Claim 15 (depends on 11)

The method of claim 11, wherein the flowing of the first chamber gas is at a pressure in a range of 1 mTorr to 9 mTorr, and at a volumetric flow in a range of 100 sccm to 1000 sccm.

### Claim 16 (depends on 11)

The method of claim 11, wherein the flowing of the second chamber gas is at a pressure less than 5 mTorr.

### Claim 17 (depends on 11)

The method of claim 11, wherein the flowing of the second chamber gas is at a pressure in a range of 1 mTorr to 9 mTorr.

### Claim 18 (depends on 11)

The method of claim 11, wherein the flowing of the second chamber gas is at a volumetric flow rate less than 500 sccm.

### Claim 19 (depends on 11)

The method of claim 11, wherein the flowing of the second chamber gas is at a volumetric flow in a range of 100 sccm to 1000 sccm.

### Claim 20 (depends on 11)

The method of claim 11, wherein the first chamber gas includes of ammonia, and wherein the second chamber gas includes N2 and H2.