High strength and low corrosion aluminum alloys
AssigneeSecat, Inc.
InventorsNicholas Nanninga, Alex Fryman
Life of this patent
Estimating the term…
Abstract
An aluminum alloy containing silicon, in an amount of 0.1 to 1.5 wt %; magnesium, in an amount of 0.1 to 1.5 wt %; copper, in an amount of 0.1 to 1.05 wt %; nickel, in an amount of 0.1 to 0.75 wt %; iron, in an amount of up to 1.0 wt %; manganese, in an amount of up to 1.0 wt %; chromium, in an amount of up to 0.4 wt %; titanium, in an amount of up to 0.15 wt %; and the balance being aluminum and incidental impurities.
Claims20
An aluminum alloy comprising:
- silicon, in an amount of 0.1 to 1.5 wt %;
- magnesium, in an amount of 0.1 to 1.5 wt %;
- copper, in an amount of 0.10 to 1.05 wt %;
- nickel, in an amount of 0.1 to 0.75 wt %;
- iron, in an amount of up to 1.0 wt %;
- manganese, in an amount of up to 1.0 wt %;
- chromium, in an amount of up to 0.4 wt %;
- titanium, in an amount of up to 0.15 wt %;
- and
- the balance being aluminum and incidental impurities.
7 more elements