# US 2026/0159744 A1 · Downstream uses for briquettes and other forms of powder from asphalt shingle waste

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0159744 A1
- Document ID: US20260159744A1
- Status: Published application
- Kind: A1
- Application number: 19/183,338
- Filed: 2025-04-18
- Published: 2026-06-11
- Earliest claimed: 2022-12-12
- Applicants: Bmic LLC
- Inventors: Parminder Agarwal; Zhengang Zong; Ashlee Agens; Wenxiao Chan
- Web page: https://patentgrep.com/patent/US20260159744A1

## CPC

- C09K 8/12: containing synthetic organic macromolecular compounds or their precursors
- C08L 95/00: Compositions of bituminous materials, e.g. asphalt, tar, pitch
- C08L 2555/34: Recycled or waste materials, e.g. reclaimed bitumen, asphalt, roads or pathways, recycled roof coverings or shingles, recycled aggregate, recycled tires, crumb rubber, glass or cullet, fly or fuel ash, or slag
- C08L 2555/52: Aggregate, e.g. crushed stone, sand, gravel or cement
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Downstream uses for briquettes and other forms of asphalt shingle waste are provided. An asphaltic emulsion is provided. The asphaltic emulsion comprises an asphalt, wherein the asphalt comprises a waste asphalt; a filler, wherein the filler comprises a waste filler; and at least 0.1% to 50% by weight of an additive based on a total weight of the asphaltic emulsion, wherein the additive comprises at least one of a surfactant, a stabilizer, or any combination thereof. Related coatings and related methods are also provided, among other things.

## Claims

### Claim 1

A coating comprising:
an asphalt,
wherein the asphalt comprises a waste asphalt;
a filler,
wherein the filler comprises a waste filler;
at least 0.1% to 65% by weight of an additive based on a total weight of the coating,
wherein the additive comprises at least one of a surfactant, a stabilizer, or any combination thereof;
wherein the coating has at least one of:
A) a hardness of 35 or greater as measured according to ASTM D2240;
B) a water vapor permeance of 2 grams or less as measured according to ASTM E398/E96;
C) an adhesive wet peel strength of 10 lb/ft or greater as measured according to ASTM C794;
D) an average structural damping ratio of 1×10−3 or greater as measured according to ASTM E756-05; or
E) an overall transmission loss of 55 dB or greater as measured according to ASTM E2611.

### Claim 2 (depends on 1)

The coating of claim 1, wherein the coating has a hardness of 35 or greater as measured according to ASTM D2240.

### Claim 3 (depends on 1)

The coating of claim 1, wherein the coating has a water vapor permeance of 2 grams or less as measured according to ASTM E398/E96.

### Claim 4 (depends on 1)

The coating of claim 1, wherein the coating has an adhesive wet peel strength of 10 lb/ft or greater as measured according to ASTM C794.

### Claim 5 (depends on 1)

The coating of claim 1, wherein the coating has an average structural damping ratio of 1×10−3 or greater as measured according to ASTM E756-05.

### Claim 6 (depends on 1)

The coating of claim 1, wherein the coating has an overall transmission loss of 55 dB or greater as measured according to ASTM E2611.

### Claim 7 (depends on 1)

The coating of claim 1, wherein the coating comprises 1% to 75% by weight of a polymer based on the total weight of the coating.

### Claim 8 (depends on 7)

The coating of claim 7, wherein the polymer comprises a styrenic block copolymer.

### Claim 9 (depends on 1)

The coating of claim 1, wherein the coating has a coefficient of thermal expansion of less than 1×10−4 in/in/F as measured according to ASTM 831.

### Claim 10

An asphaltic emulsion comprising:
an asphalt,
wherein the asphalt comprises a waste asphalt;
a filler,
wherein the filler comprises a waste filler;
at least 0.1% to 50% by weight of an additive based on a total weight of the asphaltic emulsion,
wherein the additive comprises at least one of a surfactant, a stabilizer, or any combination thereof;
wherein, when applied to a substrate to form a coating, the coating has at least one of:
A) a hardness of 35 or greater as measured according to ASTM D2240;
B) a water vapor permeance of 2 grams or less as measured according to ASTM E398/E96;
C) an adhesive wet peel strength of 10 lb/ft or greater as measured according to ASTM C794;
D) an average structural damping ratio of 1×10−3 or greater as measured according to ASTM E756-05; or
E) an overall transmission loss of 55 dB or greater as measured according to ASTM E2611.

### Claim 11 (depends on 10)

The asphaltic emulsion of claim 10, wherein, when applied to a substrate to form a coating, the coating has a hardness of 35 or greater as measured by ASTM D2240.

### Claim 12 (depends on 10)

The asphaltic emulsion of claim 10, wherein, when applied to a substrate to form a coating, the coating has a water vapor permeance of 2 grams or less as measured by ASTM E398/E96.

### Claim 13 (depends on 10)

The asphaltic emulsion of claim 10, wherein, when applied to a substrate to form a coating, the coating has an adhesive wet peel strength of 10 lb/ft or greater as measured by ASTM C794.

### Claim 14 (depends on 10)

The asphaltic emulsion of claim 10, wherein, when applied to a substrate to form a coating, the coating has an average structural damping ratio of 1×10−3 or greater as measured according to ASTM E756-05.

### Claim 15 (depends on 10)

The asphaltic emulsion of claim 10, wherein, when applied to a substrate to form a coating, the coating has an overall transmission loss of 55 dB or greater as measured according to ASTM E2611.

### Claim 16 (depends on 10)

The asphaltic emulsion of claim 10, wherein the asphaltic emulsion comprises 1% to 60% by weight of a polymer based on a total weight of the asphaltic emulsion.

### Claim 17 (depends on 10)

The asphaltic emulsion of claim 10, wherein the asphaltic emulsion comprises 5% to 65% by weight of the asphalt based on the total weight of the asphaltic emulsion.

### Claim 18 (depends on 10)

The asphaltic emulsion of claim 10, wherein the asphaltic emulsion comprises 1% to 40% by weight of the filler based on the total weight of the asphaltic emulsion.

### Claim 19

A method comprising:
obtaining an asphalt shingle waste,
wherein the asphalt shingle waste comprises a waste asphalt and a waste filler;
obtaining an additive,
wherein the additive comprises at least one of a surfactant, a stabilizer, or any combination thereof;
emulsifying the asphalt shingle waste and the additive to form an emulsion,
wherein the emulsion comprises:
5% to 65% by weight of an asphalt based on a total weight of the emulsion;
1% to 40% by weight of a filler based on the total weight of the emulsion.

### Claim 20 (depends on 19)

The method of claim 19, wherein the emulsion comprises 1% to 60% by weight of a polymer based on the total weight of the emulsion.