# US 2026/0159456 A1 · Gel-like energetic material and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0159456 A1
- Document ID: US20260159456A1
- Status: Published application
- Kind: A1
- Application number: 19/178,791
- Filed: 2025-04-14
- Published: 2026-06-11
- Earliest claimed: 2022-10-18
- Assignees: Xi'an Jiaotong University
- Applicants: Xi'an Jiaotong University
- Inventors: Huantong SHI; Yujia HU; Lun CHENG; Meng ZHANG; Xingwen LI; Jian WU
- Web page: https://patentgrep.com/patent/US20260159456A1

## CPC

- C06B 33/08: with a nitrated organic compound
- C06B 21/0008: {Compounding the ingredient}
- C06B: EXPLOSIVES OR THERMIC COMPOSITIONS (blasting F42D); MANUFACTURE THEREOF; USE OF SINGLE SUBSTANCES AS EXPLOSIVES (compounds in general C01, C07 or C08; {demolition agents based on cementitious or like materials C04B41/0009})

## Abstract

The present disclosure discloses a gel-like energetic material, a preparation method, and a related system and device. The gel-like energetic material can be stably filled in a water gap for a long time without a housing and enables positive and negative electrodes of the gap to communicate with each other. A common formula is a mixture containing nitromethane, aluminum powder, and metal oxides. After initiating explosive device testing, friction sensitivity and impact sensitivity are both zero, and safety is extremely high. Formula compositions are insoluble or extremely difficult to dissolve in water, will not fail or decompose after soaked in water for a long time, and can still detonate normally under an action of a pulse current. After being filled in the water gap, the gel-like energetic material can generate a shock wave with a fixed amplitude, impulse and energy under drive of a pulse source with specific parameters.

## Claims

### Claim 1

A gel-like energetic material, comprising, in parts by mass, 30-65 parts of nitromethane, 10-30 parts of metal oxide powder, 15-40 parts of aluminum powder and 1-3 parts of hydrophobic fumed silica for gelation.

### Claim 2 (depends on 1)

The gel-like energetic material according to claim 1, wherein purity of the nitromethane is greater than 99%; a particle size of both the metal oxide powder and the aluminum powder is in a range from 1 μm to 100 μm; and a metal oxide is selected from copper oxide, manganese dioxide, ferric oxide or ferroferric oxide.

### Claim 3 (depends on 1)

A method for preparing the gel-like energetic material according to claim 1, comprising the following steps:
step 1: mixing metal oxide powder and aluminum powder uniformly to obtain aluminum powder/metal oxide powder;
step 2: adding the aluminum powder/metal oxide powder into nitromethane, and stirring at a room temperature to uniformly mix the nitromethane with the aluminum powder/metal oxide powder, so as to obtain aluminum powder/metal oxide/nitromethane powder; and
step 3: adding hydrophobic fumed silica into the aluminum powder/metal oxide/nitromethane powder, and stirring at a room temperature to make a mixture be gelated, so as to obtain the gel-like energetic material; wherein
in step 2 and step 3, a revolution speed for stirring is in a range from 50 r/min to 500 r/min.

### Claim 4 (depends on 1)

A method for preparing the gel-like energetic material according to claim 1, wherein the method is based on a device for preparing the gel-like energetic material, and the device comprises a cavity (104), a cavity sealing cover (103), a spiral stirring rod (102) and a stirring extension rod (107);
the cavity (104) is provided with the cavity sealing cover (103), the spiral stirring rod (102) is arranged in the cavity, and a stirring rod installation hole (105) is formed at a bottom of the cavity;
the cavity sealing cover (103) is provided with a pressurization valve (101);
an installation seat is arranged at a bottom of the spiral stirring rod (102), the installation seat is arranged in the stirring rod installation hole (105), a filling port (106) communicating with the cavity (104) is formed in the installation seat, and an outlet of the filling port (106) is provided with a counter bore for connecting the stirring extension rod (107); and
a tail end of the stirring extension rod (107) is connected to a stirring motor for driving the spiral stirring rod (102) to rotate;
wherein the method comprises the following steps:
step 1: mixing metal oxide powder and aluminum powder uniformly to obtain aluminum powder/metal oxide powder;
step 2: adding nitromethane into the cavity (104), then adding the aluminum powder/metal oxide powder to the cavity (104), covering the cavity sealing cover (103), starting the stirring motor to drive the spiral stirring rod (102) to perform rotary stirring at a room temperature so as to uniformly mix the nitromethane and the aluminum powder/metal oxide powder, and turning off the stirring motor; and
step 3: opening the cavity sealing cover (103), adding hydrophobic fumed silica into the cavity (104), covering the cavity sealing cover (103), starting the stirring motor to drive the spiral stirring rod (102) to perform rotary stirring at a room temperature so as to make a mixture be gelated, and obtaining the gel-like energetic material.

### Claim 5 (depends on 4)

The method for preparing the gel-like energetic material according to claim 4, wherein after obtaining the gel-like energetic material, the stirring extension rod (107) is removed, the pressurization valve (101) on the cavity sealing cover (103) is opened, and the cavity (104) is pressurized through the pressurization valve (101), so that the gel-like energetic material is discharged from the filling port (106).