# US 2026/0159447 A1 · Method of producing a synthetic carbonated mineral component in a cement manufacturing plant

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0159447 A1
- Document ID: US20260159447A1
- Status: Published application
- Kind: A1
- Application number: 18/708,944
- Filed: 2022-11-09
- Published: 2026-06-11
- Earliest claimed: 2021-11-10
- Applicants: Amrize Technology Switzerland LLC
- Inventors: Gerold SCHNEDL; Stefan DARMANN; Danijela TOMIC-HAZIVAR
- Web page: https://patentgrep.com/patent/US20260159447A1

## CPC

- C04B 20/0232: {with carbon dioxide}
- C04B 18/167: Recycled materials, i.e. waste materials reused in the production of the same materials
- C04B 20/026: {Comminuting, e.g. by grinding or breaking; Defibrillating fibres other than asbestos}
- C04B 20/04: Heat treatment
- C04B 28/04: Portland cements
- C04B 2111/00019: {Carbon dioxide sequestration}
- C04B 2290/20: Integrated combined plants or devices, e.g. combined foundry and concrete plant
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A method of producing a synthetic carbonated mineral component in a cement manufacturing plant, includes crushing concrete demolition waste, introducing the crushed concrete demolition waste into a raw meal mill without any prior screening procedure, grinding and simultaneously carbonating the crushed concrete demolition waste in the raw meal mill by reacting the crushed concrete demolition waste with CO2 contained in a CO2 enriched exhaust gas, thereby obtaining the synthetic carbonated mineral component, and removing the synthetic carbonated mineral component from the raw meal mill.

## Claims

### Claim 1

A method of producing a synthetic carbonated mineral component from concrete demolition waste in a cement manufacturing plant, wherein the cement manufacturing plant comprises a calcination device for producing Portland clinker by decarbonating cement raw meal while releasing a CO2 enriched exhaust gas and further comprising a raw meal mill for grinding the cement raw meal before being introduced into the calcination device, wherein the CO2 enriched exhaust gas is fed into the raw meal mill,
wherein the method comprises the steps of:
a) crushing the concrete demolition waste to obtain crushed concrete demolition waste,
b) during a period, in which the raw meal mill is not operating for grinding the cement raw meal, introducing the crushed concrete demolition waste into the raw meal mill without any prior screening step,
c) grinding and simultaneously carbonating the crushed concrete demolition waste in the raw meal mill, said carbonating being carried out by reacting the crushed concrete demolition waste with CO2 contained in the CO2 enriched exhaust gas, thereby obtaining the synthetic carbonated mineral component,
d) removing the synthetic carbonated mineral component from the raw meal mill.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the crushing step a) is carried out to obtain crushed demolition waste having a particle size of 0-15 mm.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the grinding step is carried out to obtain a synthetic carbonated mineral component, wherein less than 20 wt.-% of the synthetic carbonated mineral component have a diameter larger than 90 micrometers, measured by weighing the residue on a 90 micrometer mesh sieve.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the crushed concrete demolition waste is dried in a dryer before being introduced into the raw meal mill, wherein the CO2 enriched exhaust gas is used as a drying gas and the crushed demolition waste is carbonated in the dryer by reacting it with CO2 contained in the CO2 enriched exhaust gas.

### Claim 5 (depends on 1)

The method according to claim 1, wherein water vapor is added to the CO2 enriched exhaust gas before the CO2 enriched exhaust gas enters the dryer and/or the raw meal mill.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the temperature in the raw meal mill during said carbonation and grinding step is adjusted to 110-140° C.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the CO2 enriched exhaust gas released from the calcination device is used for preheating ground cement raw meal in a preheater, and wherein the CO2 enriched exhaust gas exiting from the preheater is fed into the raw meal mill.

### Claim 8 (depends on 7)

The method according to claim 7, wherein water vapor is added to the CO2 enriched exhaust gas exiting from the preheater.

### Claim 9 (depends on 1)

The method according to claim 1, wherein carbonation in the raw meal mill is conducted until the CaCO3 content of crushed concrete demolition waste has increased by at least 5 wt.-%

### Claim 10 (depends on 1)

The method according to claim 1, wherein a carbonation rate is controlled by adjusting the feed rate of the crushed concrete demolition waste into the raw meal mill and/or by adjusting the grain size obtained by the crushing step.

### Claim 11 (depends on 1)

A method comprising providing a synthetic carbonated mineral component manufactured according to claim 1, wherein the synthetic carbonated mineral component is mixed with Portland clinker so as to produce a composite Portland cement.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the synthetic carbonated mineral component coming from the raw meal mill is added to the mixing step without any prior separating or screening step.

### Claim 13 (depends on 11)

The method according to claim 11, wherein the ratio of synthetic carbonated mineral component to Portland cement is 5-30%.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the synthetic carbonated mineral component and the Portland clinker are co-ground in a cement mill of the cement manufacturing plant.

### Claim 15 (depends on 3)

The method according to claim 3, wherein less than 10 wt.-% of the synthetic carbonated mineral component have a diameter larger than 90 micrometers, measured by weighing the residue on a 90 micrometer mesh sieve.

### Claim 16 (depends on 6)

The method according to claim 6, wherein the temperature in the raw meal mill during said carbonation and grinding step is adjusted to 120-130° C.

### Claim 17 (depends on 11)

The method according to claim 11, wherein the synthetic carbonated mineral component is mixed with Portland clinker coming from the calcination device so as to produce the composite Portland cement.

### Claim 18 (depends on 13)

The method according to claim 13, wherein the ratio of synthetic carbonated mineral component to Portland cement is 20%.