# US 2026/0159440 A1 · Glass fiber and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0159440 A1
- Document ID: US20260159440A1
- Status: Published application
- Kind: A1
- Application number: 19/059,271
- Filed: 2025-02-21
- Published: 2026-06-11
- Earliest claimed: 2024-12-11
- Assignees: Nan Ya Plastics Corporation
- Applicants: Nan Ya Plastics Corporation
- Inventors: CHING-YAO YUAN; WEI-SHENG CHENG; CHIA-CHEN SU
- Web page: https://patentgrep.com/patent/US20260159440A1

## CPC

- C03C 3/091: containing aluminium
- C03C 14/004: {the non-glass component being in the form of particles or flakes}
- C03C 13/00: Fibre or filament compositions (manufacture of fibres or filaments C03B37/00)
- C03B 37/022: from molten glass in which the resultant product consists of different sorts of glass or is characterised by shape, e.g. hollow fibres {, undulated fibres, fibres presenting a rough surface (C03B37/025 takes precedence)}
- C03C 2213/00: Glass fibres or filaments
- C03C 2214/05: surface treated, e.g. coated
- C03C 2214/30: Methods of making the composites
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A glass fiber and method for producing the same are provided. The method for producing the glass fiber includes a covering process, a mixing process, and a drawing process. The covering process is implemented by covering a plurality of silicon nitride powders onto a plurality of surfaces of a plurality of inorganic particles to form a plurality of modified inorganic particles. Based on a total weight of each of the modified inorganic particles being 100 wt %, a content of the silicon nitride powders is between 0.01 wt % and 5 wt %, and a content of the inorganic particles is between 95 wt % and 99.99 wt %. The mixing process is implemented by mixing the modified inorganic particles into a glass raw material. The drawing process is implemented by drawing the glass raw material having the modified inorganic particles mixed therein to form a glass fiber.

## Claims

### Claim 1

A method for producing a glass fiber, comprising:
a covering process implemented by covering a plurality of silicon nitride powders onto a plurality of surfaces of a plurality of inorganic particles to form a plurality of modified inorganic particles; wherein, based on a total weight of each of the modified inorganic particles being 100 wt %, a content of the silicon nitride powders is between 0.01 wt % and 5 wt %, and a content of the inorganic particle is between 95 wt % and 99.99 wt %;
a mixing process implemented by mixing the modified inorganic particles into a glass raw material that is in a molten state; and
a drawing process implemented by drawing the glass raw material having the modified inorganic particles mixed therein to form a glass fiber;
wherein, based on a total weight of the glass fiber being 100 wt %, a content of the modified inorganic particles is between 0.01 wt % and 5 wt %, and a content of the glass raw material is between 95 wt % and 99.99 wt %.

### Claim 2 (depends on 1)

The method according to claim 1, wherein an average particle size of the modified inorganic particles is between 0.01 μm and 50 μm.

### Claim 3 (depends on 1)

The method according to claim 1, wherein, based on a total weight of the glass raw material being 100 wt %, the glass raw material includes 52 wt % to 58 wt % of silicon dioxide, 10 wt % to 18 wt % of aluminum oxide, 0.1 wt % to 5 wt % of calcium oxide, 0.1 wt % to 5 wt % of magnesium oxide, 20 wt % to 30 wt % of boron trioxide, 0.1 wt % to 0.3 wt % of ferric oxide, 0.1 wt % to 4 wt % of strontium oxide, and 0.1 wt % to 2 wt % of titanium dioxide.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the inorganic particles are selected from the group consisting of silicon dioxide, titanium dioxide, aluminum hydroxide, magnesium hydroxide, calcium carbonate, aluminum oxide, magnesium oxide, talc, aluminum nitride, boron nitride, silicon carbide, zinc oxide, zirconium oxide, quartz, diamond powder, diamond-like powder, graphite, calcined kaolin, and fumed silica.

### Claim 5 (depends on 1)

The method according to claim 1, wherein, in the covering process, a first nitrogen compound is dissolved in first solvent, a first silicon source is added into the first solvent, the first nitrogen compound, the first solvent, and the first silicon source is heated at first heating temperature of between 1200° C. and 1400° C., such that the first nitrogen compound and the first silicon source reacts to form the silicon nitride powders, and then the inorganic particles are added into the silicon nitride powders, such that the silicon nitride powders cover onto the surfaces of the inorganic particles to form the modified inorganic particles.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the first nitrogen compound is urea, the first solvent is water, ethanol, or isopropyl alcohol, and the first silicon source is silicon powders.

### Claim 7 (depends on 1)

The method according to claim 1, wherein, in the covering process, a second nitrogen compound is dissolved in a second solvent, a second silicon source is added into the second solvent, the second solvent is stirred to form a gel, the gel is sprayed onto the surfaces of the inorganic particles, and the inorganic particles having the gel formed on the surfaces thereof are heated at a second heating temperature of between 1200° C. and 1400° C., such that the second nitrogen compound and the second silicon source react to form the silicon nitride powders that cover onto the surfaces of the inorganic particles to form the modified inorganic particles.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the second nitrogen source is urea, the second solvent is water, ethanol, or isopropyl alcohol, and the second silicon source is selected from the group consisting of tetraethoxysilane, tetramethoxysilane, and methyltriethoxysilane.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the glass fiber has a dielectric constant (Dk) of between 4.24 and 4.36 measured at a frequency of 10 GHz, and the glass fiber has a dielectric loss rate (Df) of between 0.0017 and 0.0019 measured at a frequency of 10 GHz.

### Claim 10

A glass fiber, comprising:
a glass raw material; and
a plurality of modified inorganic particles dispersed in the glass raw material; wherein each of the modified inorganic particles includes an inorganic particle and a plurality of silicon nitride powders covering on the inorganic particle; wherein, based on a total weight of each of the modified inorganic particles being 100 wt %, a content of the silicon nitride powders is between 0.01 wt % and 5 wt %, and a content of the inorganic particle is between 95 wt % and 99.99 wt %;
wherein, the inorganic particles are selected from the group consisting of silicon dioxide, titanium dioxide, aluminum hydroxide, magnesium hydroxide, calcium carbonate, aluminum oxide, magnesium oxide, talc, aluminum nitride, boron nitride, silicon carbide, zinc oxide, zirconium oxide, quartz, diamond powder, diamond-like powder, graphite, calcined kaolin, and fumed silica; and
wherein, based on a total weight of the glass fiber being 100 wt %, a content of the modified inorganic particles is between 0.01 wt % and 5 wt %, and a content of the glass raw material is between 95 wt % and 99.99 wt %.

### Claim 11 (depends on 10)

The glass fiber according to claim 10, wherein an average particle size of the modified inorganic particles is between 0.01 μm and 50 um.

### Claim 12 (depends on 10)

The method according to claim 10, wherein, based on a total weight of the glass raw material being 100 wt %, the glass raw material includes 52 wt % to 58 wt % of silicon dioxide, 10 wt % to 18 wt % of aluminum oxide, 0.1 wt % to 5 wt % of calcium oxide, 0.1 wt % to 5 wt % of magnesium oxide, 20 wt % to 30 wt % of Boron trioxide, 0.1 wt % to 0.3 wt % of ferric oxide, 0.1 wt % to 4 wt % of strontium oxide, and 0.1 wt % to 2 wt % of titanium dioxide.

### Claim 13 (depends on 10)

The method according to claim 10, wherein the glass fiber has a dielectric constant (Dk) of between 4.24 and 4.36 measured at a frequency of 10 GHz, and the glass fiber has a dielectric loss rate (Df) of between 0.0017 and 0.0019 measured at a frequency of 10 GHz.