Method for rapid synthesis of metal sulfides
AssigneeSolid Power Operating, Inc.
InventorsBenjamin A. CARLSON, Samuel M. OBERWETTER, Clara MAUSER, Brian E. FRANCISCO
Life of this patent
Estimating the term…
Abstract
Methods for producing metal sulfides generally include combining an alkali metal sulfide and a metal halide in an aprotic solvent to produce a mixture that includes an alkali metal halide and a metal sulfide. Additional methods include combining a first alkali metal sulfide, a second alkali metal sulfide, and a metal halide in an aprotic solvent to produce a mixture that includes a first alkali metal halide, a second alkali metal halide, and a metal sulfide. The methods may include adding a second solvent to cause an alkali metal halide to precipitate out of the mixture and improve the purity of the metal sulfide.
Claims25
A method of producing a metal sulfide comprising:
- combining a first alkali metal sulfide, a second alkali metal sulfide, and a metal halide in an aprotic solvent to produce a solution comprising a metal sulfide and an alkali metal salt.
A method of producing a metal sulfide comprising:
- (a) combining a first alkali metal salt and a first alkali metal sulfide in an aprotic solvent to produce a mixture comprising a second sulfide and a precipitated second alkali metal salt;
- (b) adding a metal halide to the mixture to produce a supernatant comprising the first alkali metal salt and a metal sulfide and the aprotic solvent;
- (c) removing the precipitated second alkali metal salt from the supernatant;
- (d) adding a second solvent to precipitate the metal sulfide;
- and
- (e) recovering the precipitated metal sulfide.
A method of producing a metal sulfide comprising:
- combining a first alkali metal sulfide, a second alkali metal sulfide, and a metal halide in an aprotic solvent to form a mixture comprising a first alkali metal halide, a precipitated second alkali metal halide, and a metal sulfide;
- removing the precipitated second alkali metal halide from the mixture;
- adding a second solvent to the mixture to precipitate the metal sulfide;
- and
- removing the precipitated metal sulfide from the mixture.
A method of producing a composite comprising a metal sulfide comprising:
- combining a first alkali metal sulfide, a second alkali metal sulfide, and a metal halide in an aprotic solvent to form a mixture comprising a first alkali metal halide, a precipitated second alkali metal halide, and a metal sulfide;
- removing the precipitated second alkali metal halide from the mixture;
- and
- heating the mixture to remove the aprotic solvent, thereby forming a composite comprising a metal sulfide.
A method of producing a metal sulfide comprising:
- combining an alkali metal sulfide and a metal halide in an aprotic solvent to form a mixture;
- adding a second solvent to the mixture to precipitate the metal sulfide;
- and
- removing the precipitated metal sulfide from the mixture.
A method of producing a composite comprising a metal sulfide comprising:
- combining an alkali metal sulfide and a metal halide in an aprotic solvent to form a mixture;
- and
- heating the mixture to remove the aprotic solvent, thereby forming a composite comprising a metal sulfide.